Thermal Properties | Metric | English | Comments |
---|---|---|---|
Working Point | 1023 °C | 1873 °F | Viscosity 10<sup>4</sup> dPa s; ISO 7884-2 |
Schott Glass 8625 Biocompatible Glass Biocompatible glass, high IR-absorbing, Transponders (implantable) The heavy metal content of the elements lead, cadmium, mercury, and hexavalent chromium is below 100 ppmInformation provided by S.. |