Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical without Impact | 130 °C @Thickness 1.60 mm |
266 °F @Thickness 0.0630 in |
UL 746 |
Polymer Resources TP-FRG30 Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant Polybutylene Terephthalate, 30% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.. |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness 3.00 mm |
266 °F @Thickness 0.118 in |
UL 746B |
DuPont Performance Polymers Crastin® LW9020FR BK851 PBT
(Unverified Data**) Crastin® LW9020FR BK851 is a 20% glass fiber reinforced, flame retardant, black polybutylene terephthalate alloy for injection molding. It has improved surface aesthetics, excellent dimensional sta.. |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness 1.50 mm |
266 °F @Thickness 0.0591 in |
UL 746B |
DuPont Performance Polymers Crastin® LW9030FR BK851 PBT
(Unverified Data**) Crastin® LW9030FR BK851 is a 30% glass fiber reinforced, flame retardant, black polybutylene terephthalate alloy for injection molding. It has improved surface aesthetics, excellent dimensional sta.. |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness 3.00 mm |
266 °F @Thickness 0.118 in |
UL 746B |
DuPont Performance Polymers Crastin® LW9320 BK851 PBT
(Unverified Data**) Crastin® LW9320 BK851 is a 20% glass fiber reinforced, black polybutylene terephthalate alloy for injection molding. It has improved surface aesthetics, excellent dimensional stability and low warp.. |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness 0.750 mm |
266 °F @Thickness 0.0295 in |
UL 746B |
DuPont Performance Polymers Crastin® SK603 BK851 PBT
(Unverified Data**) Crastin® SK603 BK851 is a 20% glass fiber reinforced, lubricated, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness 6.00 mm |
266 °F @Thickness 0.236 in |
UL 746B |
DuPont Performance Polymers Crastin® SK609 BK851 PBT
(Unverified Data**) Crastin® SK609 BK851 is a 50% glass fiber reinforced, lubricated, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness 0.850 mm |
266 °F @Thickness 0.0335 in |
UL 746B |
DuPont Performance Polymers Crastin® ST830FRUV NC010 PBT
(Unverified Data**) Crastin® ST830FRUV NC010 is an unreinforced, Super Tough, flame retardant polybutylene terephthalate resin for injection molding. It contains a UV light stabilizer and is recognized as UL94V-0 at 0.. |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness 3.00 mm |
266 °F @Thickness 0.118 in |
UL 746B |
DuPont Performance Polymers Crastin® ST830FRUV NC010 PBT
(Unverified Data**) Crastin® ST830FRUV NC010 is an unreinforced, Super Tough, flame retardant polybutylene terephthalate resin for injection molding. It contains a UV light stabilizer and is recognized as UL94V-0 at 0.. |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness 0.750 mm |
266 °F @Thickness 0.0295 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® HTN 52G35HSL BK083 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTN52G35HSL BK083 is a 35% glass reinforced, heat stabilized, lubricated high performance polyamide resin that can be molded in water heated molds. It is also a PPA resin.Information provid.. |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness 0.710 mm |
266 °F @Thickness 0.0280 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® 70G30L NC010 Nylon 66
(Unverified Data**) Zytel® 70G30L NC010 is a 30% glass fiber reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness >=1.50 mm |
266 °F @Thickness >=0.0591 in |
|
LG Chemical LUPOY GP1000L PC, Transparent Description: Injection Molding, PC, General Purpose, Transparency, High FlowApplication: IT/OA, E&E Housing and Components Automotive InteriorCAS: 103598-77-2Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness >=0.750 mm |
266 °F @Thickness >=0.0295 in |
|
LG Chemical Lupoy NF1005F 03R Polycarbonate Resin Description: LUPOY NF 1005F03R, eco-friendly UL94 V0/1.5 mm, is designed for extrusion products. It combines an excellent physical property balance of heat resistance, transparency and impact streng.. |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness >=1.50 mm |
266 °F @Thickness >=0.0591 in |
|
LG Chemical Lupoy NF1007F 10R Polycarbonate Resin Description: LUPOY NF 1007F10R, eco-friendly UL94 V0/3.0 mm, is designed for extrusion and injection molding products. It combines an excellent physical property balance of heat resistance, transpar.. |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness >=3.00 mm |
266 °F @Thickness >=0.118 in |
|
LG Chemical Lupoy NF1007F 10R Polycarbonate Resin Description: LUPOY NF 1007F10R, eco-friendly UL94 V0/3.0 mm, is designed for extrusion and injection molding products. It combines an excellent physical property balance of heat resistance, transpar.. |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness >=0.750 mm |
266 °F @Thickness >=0.0295 in |
|
LG Chemical LUSEP GP2400 PPS+GF40%, General Purpose Feature: Injection Molding, PPS+GF40%, General PurposeApplication: Pump Units, Motor Units, etc.CAS No. 25212-74-2 and 65997-17-3Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness 3.00 mm |
266 °F @Thickness 0.118 in |
UL746B |
Mitsubishi Xantar® 18 UR Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness 3.00 mm |
266 °F @Thickness 0.118 in |
UL746B |
Mitsubishi Xantar® 22 SR FD Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness 3.00 mm |
266 °F @Thickness 0.118 in |
UL746B |
Mitsubishi Xantar® FC 25 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness 3.00 mm |
266 °F @Thickness 0.118 in |
UL746B |
Mitsubishi Xantar® FC 25 UR Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness 3.00 mm |
266 °F @Thickness 0.118 in |
UL746B |
Mitsubishi Xantar® G4F 22 UR Polycarbonate-20% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness 3.00 mm |
266 °F @Thickness 0.118 in |
UL746B |
Mitsubishi Xantar® G4F 23 R Polycarbonate-20% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness 3.00 mm |
266 °F @Thickness 0.118 in |
UL746B |
Mitsubishi Xantar® MX 1071 FD Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness 3.00 mm |
266 °F @Thickness 0.118 in |
UL746B |
Mitsubishi Xantar® MX 1082 Polycarbonate-20% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness 0.800 mm |
266 °F @Thickness 0.0315 in |
UL746B |
DSM Akulon® K222-KGV4 Nylon 6-20% Glass Reinforced (European and Asian Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness 1.50 mm |
266 °F @Thickness 0.0591 in |
UL746B |
DSM Arnite® T06 200 PBT (European and Asian Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness 0.750 mm |
266 °F @Thickness 0.0295 in |
UL 746 |
Ascend Performance Materials Vydyne® R550 Nylon 66, 50% Glass Reinforced, DAM Vydyne® R550 is general-purpose, hydrolysis-resistant, 50% glass-fiber reinforced PA66 resin. Available in natural, it is also lubricated for improved flow and offers superior surface appearance. G.. |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness 1.50 mm |
266 °F @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® R550 Nylon 66, 50% Glass Reinforced, DAM Vydyne® R550 is general-purpose, hydrolysis-resistant, 50% glass-fiber reinforced PA66 resin. Available in natural, it is also lubricated for improved flow and offers superior surface appearance. G.. |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness 0.830 mm |
266 °F @Thickness 0.0327 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® FR70G25V0 NC010 Nylon 66
(Unverified Data**) Zytel® FR70G25V0 NC010 is a 25% glass fiber reinforced, heat stabilized, flame retardant polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
UL RTI, Mechanical without Impact | 130 °C @Thickness 1.50 mm |
266 °F @Thickness 0.0591 in |
UL 746B |
DuPont Performance Polymers Crastin® LW9030 BK851 PBT
(Unverified Data**) Crastin® LW9030 BK851 is a 30% glass fiber reinforced, black polybutylene terephthalate alloy for injection molding. It has improved surface aesthetics, excellent dimensional stability and low warp.. |