Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical without Impact | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® 103FHS BKB009 Nylon 66
(Unverified Data**) Zytel® 103FHS BKB009 is a heat stabilized, internally lubricated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont Perf.. |
|||
UL RTI, Mechanical without Impact | 125 °C @Thickness >=1.60 mm |
257 °F @Thickness >=0.0630 in |
|
LG Chemical LUCON SP9306FL sPS+MF Description Injection Molding Grade, sPS+MF, Low Thermal Conductivity, Chemical Resistance, High Heat ResistanceApplication: Electrical or Electronic Parts CAS No. 9003-53-6, 65997-17-3, 68928-70-1 .. |
|||
UL RTI, Mechanical without Impact | 125 °C @Thickness >=1.50 mm |
257 °F @Thickness >=0.0591 in |
|
LG Chemical Lupoy 1301EP22 Polycarbonate Resin Description: LUPOY PC 1301EP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
UL RTI, Mechanical without Impact | 125 °C @Thickness >=3.00 mm |
257 °F @Thickness >=0.118 in |
|
LG Chemical Lupoy 1301EP-22 Polycarbonate Resin Description: LUPOY PC 1301EP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
UL RTI, Mechanical without Impact | 125 °C @Thickness >=3.00 mm |
257 °F @Thickness >=0.118 in |
|
LG Chemical Lupoy 1301V-7 Polycarbonate Resin Description: LUPOY PC 1301V-07 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.. |
|||
UL RTI, Mechanical without Impact | 125 °C @Thickness 0.750 mm |
257 °F @Thickness 0.0295 in |
UL746B |
Mitsubishi Xantar® 18 SR FD Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical without Impact | 125 °C @Thickness 0.750 mm |
257 °F @Thickness 0.0295 in |
UL746B |
Mitsubishi Xantar® 22 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical without Impact | 125 °C @Thickness 0.750 mm |
257 °F @Thickness 0.0295 in |
UL746B |
Mitsubishi Xantar® 22 UR Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical without Impact | 125 °C @Thickness 0.750 mm |
257 °F @Thickness 0.0295 in |
UL746B |
Mitsubishi Xantar® 24 SR FD Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical without Impact | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
UL746B |
Mitsubishi Xantar® 25 SR FD Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical without Impact | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
UL746B |
Mitsubishi Xantar® 27 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical without Impact | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
UL746B |
Mitsubishi Xantar® 27 SR FD Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical without Impact | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
UL746B |
Mitsubishi Xantar® FC 22 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical without Impact | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
UL746B |
Mitsubishi Xantar® G4F 22 UR Polycarbonate-20% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical without Impact | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
UL746B |
Mitsubishi Xantar® G4F 23 UR Polycarbonate-20% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical without Impact | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
UL746B |
Mitsubishi Xantar® G4F 25 R Polycarbonate-20% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical without Impact | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
UL746B |
Mitsubishi Xantar® G4F 25 UR Polycarbonate-20% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical without Impact | 125 °C @Thickness >=3.00 mm |
257 °F @Thickness >=0.118 in |
|
LG Chemical Lupoy 1200HP-15 Polycarbonate Resin Description: LUPOY PC 1200HP-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
UL RTI, Mechanical without Impact | 125 °C @Thickness >=3.00 mm |
257 °F @Thickness >=0.118 in |
|
LG Chemical Lupoy 1201HP-08 Polycarbonate Resin Description: LUPOY PC 1201HP-08 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
UL RTI, Mechanical without Impact | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
UL746B |
Mitsubishi Xantar® MX 2015 Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
UL RTI, Mechanical without Impact | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
UL746B |
DSM Stanyl® 46HF5050 Nylon 46-50% Glass Reinforced (European and Asian Grade) (Cond) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
UL RTI, Mechanical without Impact | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
UL746B |
DSM Stanyl® TE250F8 Nylon 46-40% Glass Reinforced (European and Asian Grade) (Cond) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
UL RTI, Mechanical without Impact | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
UL746B |
DSM Stanyl® TE250F8 Nylon 46-40% Glass Reinforced (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
UL RTI, Mechanical without Impact | 125 °C @Thickness 3.00 mm |
257 °F @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® 22HSP NT Nylon 66, DAM Availability:Asia PacificEuropeNorth America Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood ToughnessHigh Rigidit.. |
|||
UL RTI, Mechanical without Impact | 125 °C @Thickness 0.750 mm |
257 °F @Thickness 0.0295 in |
UL 746 |
Ascend Performance Materials Vydyne® R525H BK02 Nylon 66, 25% Glass Reinforced, DAM Vydyne® R525H BK02 is high-flow, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose.. |
|||
UL RTI, Mechanical without Impact | 125 °C @Thickness 0.750 mm |
257 °F @Thickness 0.0295 in |
UL 746 |
Ascend Performance Materials Vydyne® R525H BLK Nylon 66, 25% Glass Reinforced, DAM Vydyne® R525H BLK is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties.. |
|||
UL RTI, Mechanical without Impact | 125 °C @Thickness 0.750 mm |
257 °F @Thickness 0.0295 in |
UL 746 |
Ascend Performance Materials Vydyne® R530H BK0201 Nylon 66, 30% Glass Reinforced, DAM Vydyne® R530H BK0201 is general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in black, it is specifically designed to maximize the retention of p.. |
|||
UL RTI, Mechanical without Impact | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
UL746B |
Mitsubishi Xantar® 27 UR Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances wher.. |
|||
UL RTI, Mechanical without Impact | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
UL746B |
Mitsubishi Xantar® G8F 23 R Polycarbonate-40% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances wher.. |
|||
UL RTI, Mechanical without Impact | 125 °C @Thickness 1.50 mm |
257 °F @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® 22HSP NT Nylon 66, DAM Availability:Asia PacificEuropeNorth AmericaAdditive: Lubricant Features:Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood Tou.. |