Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical without Impact | 120 °C @Thickness 3.00 mm |
248 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources TP-GP2 Polybutylene Terephthalate, General Purpose Polybutylene Terephthalate, General Purpose Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provid.. |
|||
UL RTI, Mechanical without Impact | 120 °C @Thickness 1.50 mm |
248 °F @Thickness 0.0591 in |
UL 746B |
DuPont Performance Polymers Crastin® S600F20 NC010 PBT
(Unverified Data**) Crastin® S600F20 NC010 is an unreinforced, lubricated, medium viscosity polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
UL RTI, Mechanical without Impact | 120 °C @Thickness 1.50 mm |
248 °F @Thickness 0.0591 in |
UL 746B |
DuPont Performance Polymers Crastin® S620F20 BK851 PBT
(Unverified Data**) Crastin® S620F20 BK851 is an unreinforced, nucleated, lubricated, medium viscosity, black polybutylene terephthalate resin for fast injection molding.Information provided by DuPont Performance Poly.. |
|||
UL RTI, Mechanical without Impact | 120 °C @Thickness 3.00 mm |
248 °F @Thickness 0.118 in |
UL 746B |
DuPont Performance Polymers Crastin® S620F20 BK851 PBT
(Unverified Data**) Crastin® S620F20 BK851 is an unreinforced, nucleated, lubricated, medium viscosity, black polybutylene terephthalate resin for fast injection molding.Information provided by DuPont Performance Poly.. |
|||
UL RTI, Mechanical without Impact | 120 °C @Thickness 3.00 mm |
248 °F @Thickness 0.118 in |
UL 746B |
DuPont Performance Polymers Crastin® SK602 BK851 PBT
(Unverified Data**) Crastin® SK602 BK851 is a 15% glass fiber reinforced, lubricated, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
UL RTI, Mechanical without Impact | 120 °C @Thickness >=3.00 mm |
248 °F @Thickness >=0.118 in |
|
LG Chemical LUMID GP2330B(W) PA66+GF33%, General Purpose Feature: Injection Molding, PA6+GF33%, General PurposeApplication: Automotive (Air Intake Manifold, Cylinder Head Cover)CAS No. 32131-17-2 and 65997-17-3Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 120 °C @Thickness >=3.00 mm |
248 °F @Thickness >=0.118 in |
|
LG Chemical LUMID GP2430B(W) PA66+GF43%, General Purpose Feature: Injection Molding, PA66+GF43%, General PurposeApplication: Automotive (Air Intake Manifold)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 120 °C @Thickness >=3.00 mm |
248 °F @Thickness >=0.118 in |
|
LG Chemical LUPOL GP1007FE Flame Retardant PP Description: Injection Molding, FR PP, General Purpose, Flame RetardantApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 1309-64-4Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 120 °C @Thickness >=3.00 mm |
248 °F @Thickness >=0.118 in |
|
LG Chemical LUPOL HG3200SK2 PP+MF20%, High Gloss Description: Injection Molding, PP+MF20%, High GlossApplication: Electrical & Electronic PartsCAS: 9003-07-0 and 7727-43-7Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 120 °C @Thickness >=1.60 mm |
248 °F @Thickness >=0.0630 in |
|
LG Chemical Lupox® TE5006F PET+PC Description: Injection Molding, PET+PC, Flame Retardant, GWIT, CTIApplication: IT/OA, E&E (Connector)CAS No. 68928-70-1, 103598-77-2, 25038-59-9 and 1309-64-4Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 120 °C @Thickness >=1.60 mm |
248 °F @Thickness >=0.0630 in |
|
LG Chemical Lupoy 1302-05 Polycarbonate Resin Description: LUPOY 1302-5 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main.. |
|||
UL RTI, Mechanical without Impact | 120 °C @Thickness >=3.00 mm |
248 °F @Thickness >=0.118 in |
|
LG Chemical Lupoy 1302-07 Polycarbonate Resin Description: LUPOY PC 1302-07 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
UL RTI, Mechanical without Impact | 120 °C @Thickness >=1.50 mm |
248 °F @Thickness >=0.0591 in |
|
LG Chemical LUPOY GN1006FL PC, Halogen Free, Flame Retardant, Transparency Description: Injection Molding, PC, Halogen Free Flame Retardant, TransparencyApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 120 °C @Thickness >=1.50 mm |
248 °F @Thickness >=0.0591 in |
|
LG Chemical LUPOL GP3156F Flame Retardant PP Description: Injection Molding, FR PP, General Purpose, Flame RetardantApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0, 84852-53-9, 14807-96-6 and 1309-64-4Information provided .. |
|||
UL RTI, Mechanical without Impact | 120 °C @Thickness >=1.60 mm |
248 °F @Thickness >=0.0630 in |
|
LG Chemical Lupoy 1302HP-10 Polycarbonate Resin Description: LUPOY PC 1302HP-10 resin is designed for extrusion products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Characteristics.. |
|||
UL RTI, Mechanical without Impact | 120 °C @Thickness >=3.00 mm |
248 °F @Thickness >=0.118 in |
|
LG Chemical Lupoy 1303-15 Polycarbonate Resin Description: LUPOY PC 1303-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
UL RTI, Mechanical without Impact | 120 °C @Thickness >=1.70 mm |
248 °F @Thickness >=0.0669 in |
|
LG Chemical LUPOY EF1006F PC, Halogen Free, Flame Retardant, High Heat Resistance Description: Injection Molding, PC, Halogen Free Flame Retardant, High Heat ResistanceApplication: IT/OA Housing and Components (Adaptor)CAS: 103598-77-2Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 120 °C @Thickness 0.810 mm |
248 °F @Thickness 0.0319 in |
UL 746 |
Teknor Apex Chemlon® 182 Nylon 66, Non-Halogenated Notes: General Purpose; U.L. 94 V-O at 0.57 mm; Colorable; Flame Retardant Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor Apex |
|||
UL RTI, Mechanical without Impact | 120 °C @Thickness 1.50 mm |
248 °F @Thickness 0.0590 in |
UL 746 |
Teknor Apex Chemlon® 282 Nylon 6, Non-halogenated Features: Flame Retardant; General Purpose; Halogen-free; U.L. 94 V-O at 0.63 mm; ColorableProcessing Method: Injection Molding Forms: Pellets Additive: Flame RetardantInformation Provided by Teknor.. |
|||
UL RTI, Mechanical without Impact | 120 °C @Thickness 3.00 mm |
248 °F @Thickness 0.118 in |
UL 746 |
Teknor Apex Chemlon® 282 Nylon 6, Non-halogenated Features: Flame Retardant; General Purpose; Halogen-free; U.L. 94 V-O at 0.63 mm; ColorableProcessing Method: Injection Molding Forms: Pellets Additive: Flame RetardantInformation Provided by Teknor.. |
|||
UL RTI, Mechanical without Impact | 120 °C @Thickness 0.750 mm |
248 °F @Thickness 0.0295 in |
UL746B |
DSM Stanyl® 46HF5040 Nylon 46-40% Glass Reinforced (European and Asian Grade) (Cond) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
UL RTI, Mechanical without Impact | 120 °C @Thickness 0.750 mm |
248 °F @Thickness 0.0295 in |
UL746B |
DSM Stanyl® 46HF5041LW Nylon 46-40% Glass Reinforced (European and Asian Grade) (Cond) Stanyl is a high performance polyamide providing unmatched performance and value across an amazingly broad range of automotive and electronic applications. Stanyl offers:Highest mechanical propertie.. |
|||
UL RTI, Mechanical without Impact | 120 °C @Thickness 3.00 mm |
248 °F @Thickness 0.118 in |
|
Eurostar Starflam AFR450X2 PA66, 25% Glass Filled, Injection Molded AFR450X2 is a Red Phosphorous, Flame Retardant, 25% Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive su.. |
|||
UL RTI, Mechanical without Impact | 120 °C @Thickness 0.860 mm |
248 °F @Thickness 0.0339 in |
|
Eurostar Starflam RF0023E PA66/6, 10% Glass Filled, Injection Molded Starflam RF0023E is a Mineral Flame Retardant, Halogen Free and Phosphorous Free, Glass Fiber Reinforced, Polyamide 66/6 Injection Molding (also known as RF1002Z230EM)Information provided by Polymer.. |
|||
UL RTI, Mechanical without Impact | 120 °C @Thickness 1.50 mm |
248 °F @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® R525 Nylon 66, 25% Glass Reinforced, DAM Vydyne® R525 is hydrolysis-resistant, 25% glass-fiber reinforced PA66 resin. Available in natural it is lubricated for improved machine feed and flow. Glass-reinforced Vydyne resins provide higher .. |
|||
UL RTI, Mechanical without Impact | 120 °C @Thickness 1.50 mm |
248 °F @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® 41H NT Nylon 66, Impact Modified, DAM Vydyne® 41H NT is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyn.. |
|||
UL RTI, Mechanical without Impact | 120 °C @Thickness 3.00 mm |
248 °F @Thickness 0.118 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® 79G13HSL NC010 Nylon 66
(Unverified Data**) Zytel® 79G13HSL is a 13% glass fiber reinforced, heat stabilized, lubricated slightly toughened polyamide 66 for injection molding. It has improved impact resistance.Information provided by DuPont .. |
|||
UL RTI, Mechanical without Impact | 120 °C @Thickness 3.00 mm |
248 °F @Thickness 0.118 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® HTN FR52G30BL BK337 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTNFR52G30BL BK337 is a 30% glass reinforced, flame retardant, lubricated high performance polyamide resin that has been developed for connector applications.Information provided by DuPont P.. |
|||
UL RTI, Mechanical without Impact | 120 °C @Thickness 1.50 mm |
248 °F @Thickness 0.0591 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® HTN FR52G45BL BK337 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTNFR52G45BL BK337 is a 45% glass reinforced, flame retardant, lubricated high performance polyamide resin that has been developed for connector applications.Information provided by DuPont .. |
|||
UL RTI, Mechanical without Impact | 120 °C @Thickness 0.750 mm |
248 °F @Thickness 0.0295 in |
UL746B |
DSM Stanyl® 46HF5050 Nylon 46-50% Glass Reinforced (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |