Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical without Impact | 115 °C @Thickness 3.00 mm |
239 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources PC-GP1-D-[color]-1 Polycarbonate, General Purpose, Low Flow with Mold Release Polycarbonate, General Purpose, Low Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
UL RTI, Mechanical without Impact | 115 °C @Thickness 1.50 mm |
239 °F @Thickness 0.0591 in |
UL 746 |
Polymer Resources PC-GP2-D-[color]-1 Polycarbonate, General Purpose, Medium Flow with Mold Release Polycarbonate, General Purpose, Medium Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inf.. |
|||
UL RTI, Mechanical without Impact | 115 °C @Thickness 1.50 mm |
239 °F @Thickness 0.0591 in |
UL 746 |
Polymer Resources PC-GP3-D Polycarbonate, General Purpose, High Flow Polycarbonate, General Purpose, High FlowFeatures: • High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inc.. |
|||
UL RTI, Mechanical without Impact | 115 °C @Thickness 1.50 mm |
239 °F @Thickness 0.0591 in |
UL 746 |
PolyOne Bergamid™ A700 G15 HW UF Polyamide 66 (Nylon 66) These products contain flame retardants which are activated by longer residence times in the cylinder and then can decompose. At interruption of the moulding cycle (approx. >5 min) it is recommended.. |
|||
UL RTI, Mechanical without Impact | 115 °C @Thickness 1.50 mm |
239 °F @Thickness 0.0591 in |
UL 746 |
PolyOne Bergamid™ A700 G20 HW UF Polyamide 66 (Nylon 66) Information provided by PolyOne |
|||
UL RTI, Mechanical without Impact | 115 °C @Thickness 1.50 mm |
239 °F @Thickness 0.0591 in |
UL 746 |
Polymer Resources PC-GP3-D-[color]-1 Polycarbonate, General Purpose, High Flow with Mold Release Polycarbonate, General Purpose, High Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor.. |
|||
UL RTI, Mechanical without Impact | 115 °C @Thickness 3.00 mm |
239 °F @Thickness 0.118 in |
DAM; UL 746B |
DuPont Performance Polymers Minlon® 10B140 BK061 Nylon 66
(Unverified Data**) Minlon® 10B140 BK061 is a 40% mineral reinforced, black polyamide 66 resin for injection molding. It has very low warpage.Information provided by DuPont Performance Polymers |
|||
UL RTI, Mechanical without Impact | 115 °C @Thickness 0.710 mm |
239 °F @Thickness 0.0280 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® 103FHS BKB009 Nylon 66
(Unverified Data**) Zytel® 103FHS BKB009 is a heat stabilized, internally lubricated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont Perf.. |
|||
UL RTI, Mechanical without Impact | 115 °C @Thickness 0.780 mm |
239 °F @Thickness 0.0307 in |
UL 746 |
A. Schulman POLYFLAM™ FPP 1007 Talc Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1007 is a 40% talc filled homopolymer polypropylene compound.Information provided by A. Schulman. |
|||
UL RTI, Mechanical without Impact | 115 °C @Thickness 1.57 mm |
239 °F @Thickness 0.0618 in |
UL 746 |
A. Schulman POLYFLAM™ FPP 1007 Talc Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1007 is a 40% talc filled homopolymer polypropylene compound.Information provided by A. Schulman. |
|||
UL RTI, Mechanical without Impact | 115 °C @Thickness 0.780 mm |
239 °F @Thickness 0.0307 in |
UL 746 |
A. Schulman POLYFLAM™ FPP 1007 Talc Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1007 is a 40% talc filled homopolymer polypropylene compound.Information provided by A. Schulman. |
|||
UL RTI, Mechanical without Impact | 115 °C @Thickness 0.780 - 1.57 mm |
239 °F @Thickness 0.0307 - 0.0618 in |
UL 746 |
A. Schulman POLYFORT™ FPP 1310 Coupled Mica Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1310 is a Coupled Mica filled homopolymer polypropylene compound for injection molding.Information provided by A. Schulman. |
|||
UL RTI, Mechanical without Impact | 115 °C @Thickness 0.780 mm |
239 °F @Thickness 0.0307 in |
UL 746 |
A. Schulman POLYFLAM™ FPP 1007 Talc Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1007 is a 40% talc filled homopolymer polypropylene compound.Information provided by A. Schulman. |
|||
UL RTI, Mechanical without Impact | 115 °C @Thickness 1.57 mm |
239 °F @Thickness 0.0618 in |
UL 746 |
A. Schulman POLYFLAM™ FPP 1007 Talc Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1007 is a 40% talc filled homopolymer polypropylene compound.Information provided by A. Schulman. |
|||
UL RTI, Mechanical without Impact | 115 °C @Thickness 1.50 mm |
239 °F @Thickness 0.0591 in |
|
Eurostar Starflam AFR450X1 PA66, 25% Glass Filled, Injection Molded AFR450X1 is a Red Phosphorous, Flame Retardant, Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli.. |
|||
UL RTI, Mechanical without Impact | 115 °C @Thickness 1.50 mm |
239 °F @Thickness 0.0591 in |
|
Eurostar Starflam AFR450X2 PA66, 25% Glass Filled, Injection Molded AFR450X2 is a Red Phosphorous, Flame Retardant, 25% Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive su.. |
|||
UL RTI, Mechanical without Impact | 115 °C @Thickness 0.710 mm |
239 °F @Thickness 0.0280 in |
UL 746 |
Ascend Performance Materials Vydyne® 22HSP NT Nylon 66, DAM Availability:Asia PacificEuropeNorth America Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood ToughnessHigh Rigidit.. |
|||
UL RTI, Mechanical without Impact | 115 °C @Thickness 1.50 mm |
239 °F @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® 47H BK0501 Nylon 66, Impact Modified, DAM Vydyne® 47H BK0501 is general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
UL RTI, Mechanical without Impact | 115 °C @Thickness 0.750 mm |
239 °F @Thickness 0.0295 in |
UL 746 |
Ascend Performance Materials Vydyne® 47H BK0668 Nylon 66, Impact Modified, Heat Stabilized, DAM Vydyne® 47H BK0668 is a high-performance, medium-impact-modified, heat-stabilized grade of PA66 resin.Availability:Asia PacificEuropeNorth AmericaAdditive:Impact Modifier Features:Gasoline Resistan.. |
|||
UL RTI, Mechanical without Impact | 115 °C @Thickness 1.50 mm |
239 °F @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® 47H Nylon 66, Impact Modified, DAM Vydyne® 47H is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne 4.. |
|||
UL RTI, Mechanical without Impact | 115 °C @Thickness 0.750 mm |
239 °F @Thickness 0.0295 in |
UL 746 |
Ascend Performance Materials Vydyne® 47H Nylon 66, Impact Modified, DAM Vydyne® 47H is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne 4.. |
|||
UL RTI, Mechanical without Impact | 115 °C @Thickness 0.750 mm |
239 °F @Thickness 0.0295 in |
UL 746 |
Ascend Performance Materials Vydyne® R515 Nylon 66, 15% Glass Reinforced, DAM Vydyne® R515 is general-purpose, 15% glass-fiber reinforced PA66 resin. Availability:Asia PacificEuropeNorth AmericaFiller/Reinforcement:Glass Fiber, 15% Filler by WeightAdditive:Lubricant Features.. |
|||
UL RTI, Mechanical without Impact | 115 °C @Thickness 0.750 mm |
239 °F @Thickness 0.0295 in |
UL 746 |
Ascend Performance Materials Vydyne® R540 Nylon 66, 40% Glass Reinforced, DAM Vydyne® R540 is general-purpose, hydrolysis-resistant, 40% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties when.. |
|||
UL RTI, Mechanical without Impact | 115 °C @Thickness 0.750 mm |
239 °F @Thickness 0.0295 in |
UL 746 |
Ascend Performance Materials Vydyne® 41H NT Nylon 66, Impact Modified, DAM Vydyne® 41H NT is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyn.. |
|||
UL RTI, Mechanical without Impact | 115 °C @Thickness 3.00 mm |
239 °F @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® 47H BK0644 Nylon 66, Impact Modified, DAM Vydyne® 47H BK0644 is a high-performance, medium-impact-modified, heat-stabilized PA66 resin with excellent UV stability and outstanding processing characteristics. This product has an UL746C f1 ra.. |
|||
UL RTI, Mechanical without Impact | 115 °C @Thickness 0.710 mm |
239 °F @Thickness 0.0280 in |
UL 746B |
Ascend Performance Materials Vydyne® 66J Nylon 66, General Purpose, high viscosity, DAM Vydyne® 66J is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66J resin offers high strength, .. |
|||
UL RTI, Mechanical without Impact | 115 °C @Thickness 0.780 mm |
239 °F @Thickness 0.0307 in |
UL 746 |
A. Schulman POLYFLAM™ FPP 1007 Talc Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1007 is a 40% talc filled homopolymer polypropylene compound.Information provided by A. Schulman. |
|||
UL RTI, Mechanical without Impact | 115 °C @Thickness 1.57 mm |
239 °F @Thickness 0.0618 in |
UL 746 |
A. Schulman POLYFLAM™ FPP 1007 Talc Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1007 is a 40% talc filled homopolymer polypropylene compound.Information provided by A. Schulman. |
|||
UL RTI, Mechanical without Impact | 115 °C @Thickness 0.780 mm |
239 °F @Thickness 0.0307 in |
UL 746 |
A. Schulman POLYFLAM™ FPP 1007 Talc Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1007 is a 40% talc filled homopolymer polypropylene compound.Information provided by A. Schulman. |
|||
UL RTI, Mechanical without Impact | 115 °C @Thickness 0.710 mm |
239 °F @Thickness 0.0280 in |
UL 746 |
Ascend Performance Materials Vydyne® 22HSP NT Nylon 66, DAM Availability:Asia PacificEuropeNorth AmericaAdditive: Lubricant Features:Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood Tou.. |