Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical with Impact | 105 °C @Thickness 3.00 mm |
221 °F @Thickness 0.118 in |
UL 746 |
PolyOne Maxxam™ FR PP FR 7A11 Polypropylene, Unspecified (PP, Unspecified) Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V.. |
|||
UL RTI, Mechanical with Impact | 105 °C @Thickness 1.50 mm |
221 °F @Thickness 0.0591 in |
UL 746 |
PolyOne Maxxam™ FR PP FR 7B31 Polypropylene, Unspecified (PP, Unspecified) Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V.. |
|||
UL RTI, Mechanical with Impact | 105 °C @Thickness 3.00 mm |
221 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources PEI-G20 Polyetherimide, 20% Glass Reinforced Polyetherimide, 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Poly.. |
|||
UL RTI, Mechanical with Impact | 105 °C @Thickness 1.50 mm |
221 °F @Thickness 0.0591 in |
UL 746 |
Polymer Resources PEI-G40 Polyetherimide, 40% Glass Reinforced Polyetherimide, 40% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Poly.. |
|||
UL RTI, Mechanical with Impact | 105 °C @Thickness 3.00 mm |
221 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources TPSF-G10 Polybutylene Terephthalate, Structural Foam, 10% Glass Reinforced Polybutylene Terephthalate, Structural Foam, 10% Glass ReinforcedProcess: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Info.. |
|||
UL RTI, Mechanical with Impact | 105 °C @Thickness 1.50 mm |
221 °F @Thickness 0.0591 in |
UL 746 |
Solvay Specialty Polymers Ixef® 1022 Polyarylamide (PARA)
(Unverified Data**) Ixef 1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance. Ixef 1022.. |
|||
UL RTI, Mechanical with Impact | 105 °C @Thickness 1.50 mm |
221 °F @Thickness 0.0591 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® FR70M30V0 BK010 Nylon 66
(Unverified Data**) Zytel® FR70M30V0 BK010 is a 30% mineral reinforced, flame retardant, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
UL RTI, Mechanical with Impact | 105 °C @Thickness >=1.50 mm |
221 °F @Thickness >=0.0591 in |
|
LG Chemical LUMID GP3400A(W) PA6+MF40%, General Purpose Feature: Injection Molding, PA6+MF40%, General PurposeApplication: E&E (Rice Cooker Housing)CAS No. 25038-54-4 and 14807-96-6Information provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 105 °C @Thickness >=1.60 mm |
221 °F @Thickness >=0.0630 in |
|
LG Chemical Lupoy 1302-05 Polycarbonate Resin Description: LUPOY 1302-5 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main.. |
|||
UL RTI, Mechanical with Impact | 105 °C @Thickness >=2.50 mm |
221 °F @Thickness >=0.0984 in |
|
LG Chemical Lupoy 1302-05 Polycarbonate Resin Description: LUPOY 1302-5 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main.. |
|||
UL RTI, Mechanical with Impact | 105 °C @Thickness >=1.60 mm |
221 °F @Thickness >=0.0630 in |
|
LG Chemical Lupoy 1302-10 Polycarbonate Resin Description: LUPOY PC 1302-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
UL RTI, Mechanical with Impact | 105 °C @Thickness >=1.60 mm |
221 °F @Thickness >=0.0630 in |
|
LG Chemical Lupoy 1302HP-09 Polycarbonate Resin Description: LUPOY PC 1302HP-09 resin is designed for extrusion products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Characteristics.. |
|||
UL RTI, Mechanical with Impact | 105 °C @Thickness >=1.60 mm |
221 °F @Thickness >=0.0630 in |
|
LG Chemical Lupoy 1302HP-10 Polycarbonate Resin Description: LUPOY PC 1302HP-10 resin is designed for extrusion products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Characteristics.. |
|||
UL RTI, Mechanical with Impact | 105 °C @Thickness >=1.60 mm |
221 °F @Thickness >=0.0630 in |
|
LG Chemical Lupoy 1302UV-08 Polycarbonate Resin Description: LUPOY PC 1302UV-08 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
UL RTI, Mechanical with Impact | 105 °C @Thickness >=1.50 mm |
221 °F @Thickness >=0.0591 in |
|
LG Chemical Lupoy 1303-10 Polycarbonate Resin Description: LUPOY PC 1303-07 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
UL RTI, Mechanical with Impact | 105 °C @Thickness >=1.50 mm |
221 °F @Thickness >=0.0591 in |
|
LG Chemical Lupoy 1303-15 Polycarbonate Resin Description: LUPOY PC 1303-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
UL RTI, Mechanical with Impact | 105 °C @Thickness >=1.50 mm |
221 °F @Thickness >=0.0591 in |
|
LG Chemical Lupoy 1303EP-30 Polycarbonate Resin Description: LUPOY PC 1303EP-30 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
UL RTI, Mechanical with Impact | 105 °C @Thickness 1.50 mm |
221 °F @Thickness 0.0590 in |
UL 746 |
Teknor Apex Chemlon® 182 Nylon 66, Non-Halogenated Notes: General Purpose; U.L. 94 V-O at 0.57 mm; Colorable; Flame Retardant Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor Apex |
|||
UL RTI, Mechanical with Impact | 105 °C @Thickness 3.00 mm |
221 °F @Thickness 0.118 in |
UL 746 |
Teknor Apex Chemlon® 182 Nylon 66, Non-Halogenated Notes: General Purpose; U.L. 94 V-O at 0.57 mm; Colorable; Flame Retardant Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor Apex |
|||
UL RTI, Mechanical with Impact | 105 °C @Thickness 1.50 mm |
221 °F @Thickness 0.0590 in |
UL 746 |
Teknor Apex Chemlon® 233 GH Nylon, 6, 30% Short Glass Fiber Reinforced Features: Good Dimensional Stability; Good Impact Resistance; Good Processability; Good Toughness; Heat Stabilized; High Strength; Lubricated Processing Method: Injection Molding Forms: Pellets Addi.. |
|||
UL RTI, Mechanical with Impact | 105 °C @Thickness 1.70 mm |
221 °F @Thickness 0.0669 in |
|
Eurostar Starflam RF0023E PA66/6, 10% Glass Filled, Injection Molded Starflam RF0023E is a Mineral Flame Retardant, Halogen Free and Phosphorous Free, Glass Fiber Reinforced, Polyamide 66/6 Injection Molding (also known as RF1002Z230EM)Information provided by Polymer.. |
|||
UL RTI, Mechanical with Impact | 105 °C @Thickness 1.60 mm |
221 °F @Thickness 0.0630 in |
|
Eurostar Starflam RF0057P PA66/6, 25% Glass Filled, Injection Molded Starflam RF0057P is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 66/6 Injection Molding Resin (also known as RF1005Z270EM)Information provided by Polym.. |
|||
UL RTI, Mechanical with Impact | 105 °C @Thickness 0.800 mm |
221 °F @Thickness 0.0315 in |
|
Eurostar Starflam PF0057E PA6, 25% Glass Filled, Injection Molded Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 6 Injection Molding Resin (also known as PF-1005 Z270)Information provided by Polymer Technology & Services,.. |
|||
UL RTI, Mechanical with Impact | 105 °C @Thickness 1.60 mm |
221 °F @Thickness 0.0630 in |
|
Eurostar Starflam PF0057E PA6, 25% Glass Filled, Injection Molded Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 6 Injection Molding Resin (also known as PF-1005 Z270)Information provided by Polymer Technology & Services,.. |
|||
UL RTI, Mechanical with Impact | 105 °C @Thickness 1.60 mm |
221 °F @Thickness 0.0630 in |
|
Eurostar Starflam PF0057E PA6, 25% Glass Filled, Injection Molded Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 6 Injection Molding Resin (also known as PF-1005 Z270)Information provided by Polymer Technology & Services,.. |
|||
UL RTI, Mechanical with Impact | 105 °C @Thickness 3.00 mm |
221 °F @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® R525 Nylon 66, 25% Glass Reinforced, DAM Vydyne® R525 is hydrolysis-resistant, 25% glass-fiber reinforced PA66 resin. Available in natural it is lubricated for improved machine feed and flow. Glass-reinforced Vydyne resins provide higher .. |
|||
UL RTI, Mechanical with Impact | 105 °C @Thickness 3.00 mm |
221 °F @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® R535 Nylon 66, 35% Glass Reinforced, DAM Vydyne® R535 is general-purpose, hydrolysis-resistant, 35% glass-fiber reinforced PA66 resin. This product is lubricated for improved flow and offers superior surface appearance. Glass-reinforced V.. |
|||
UL RTI, Mechanical with Impact | 105 °C @Thickness 3.00 mm |
221 °F @Thickness 0.118 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® 80G33HS1L BK104 Nylon 66
(Unverified Data**) Zytel® 80G33HS1L BK104 is a 33% glass fiber reinforced, heat stabilized black polyamide 66 resin with outstanding impact resistance developed using DuPont Super Tough technology.Information provide.. |
|||
UL RTI, Mechanical with Impact | 105 °C @Thickness 1.50 mm |
221 °F @Thickness 0.0591 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® 80G33HS1L BK104 Nylon 66
(Unverified Data**) Zytel® 80G33HS1L BK104 is a 33% glass fiber reinforced, heat stabilized black polyamide 66 resin with outstanding impact resistance developed using DuPont Super Tough technology.Information provide.. |
|||
UL RTI, Mechanical with Impact | 105 °C @Thickness 3.00 mm |
221 °F @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® R530 NAT Nylon 66, 30% Glass Reinforced, DAM Vydyne® R530 NAT is general-purpose, injection-molding grade, 30% glass-fiber reinforced PA66 resin. Available in natural, it is lubricated for good machine feed, flow and mold releaseAvailability:.. |