Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical with Impact | 60.0 °C @Thickness 3.00 mm |
140 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources ABS-FR Flame Retardant ABS Flame Retardant Acrylonitrile Butadiene StyreneFeatures: • Flame Retardant • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch.. |
|||
UL RTI, Mechanical with Impact | 60.0 °C @Thickness 1.50 mm |
140 °F @Thickness 0.0591 in |
UL 746 |
Polymer Resources ABS-GP1 General Purpose ABS General Purpose Acrylonitrile Butadiene StyreneFeatures: • Medium Impact ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pig.. |
|||
UL RTI, Mechanical with Impact | 60.0 °C @Thickness 3.00 mm |
140 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources ABS-GP1 General Purpose ABS General Purpose Acrylonitrile Butadiene StyreneFeatures: • Medium Impact ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pig.. |
|||
UL RTI, Mechanical with Impact | 60.0 °C @Thickness 1.50 mm |
140 °F @Thickness 0.0591 in |
UL 746 |
Polymer Resources ABS-GP1-[color]-UV General Purpose ABS, UV-stabilized General Purpose Acrylonitrile Butadiene Styrene, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.In.. |
|||
UL RTI, Mechanical with Impact | 60.0 °C @Thickness >=1.00 mm |
140 °F @Thickness >=0.0394 in |
UL 746B |
LG Chemical AF312B ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical.. |
|||
UL RTI, Mechanical with Impact | 60.0 °C @Thickness >=3.00 mm |
140 °F @Thickness >=0.118 in |
|
LG Chemical AF345 ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provided by LG Chemi.. |
|||
UL RTI, Mechanical with Impact | 60.0 °C @Thickness >=1.50 mm |
140 °F @Thickness >=0.0591 in |
UL 746B |
LG Chemical ER451 ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior & Exterior Housing (garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemica.. |
|||
UL RTI, Mechanical with Impact | 60.0 °C @Thickness >=1.50 mm |
140 °F @Thickness >=0.0591 in |
UL 746B |
LG Chemical HF380NS ABS, High Flow, General Anti-Static Feature: Injection Molding, High Flow, General Anti-StaticApplication: Electric & Electronic Products, Miscellaneous goods)CAS No. 9003-56-9Information provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 60.0 °C @Thickness >=1.50 mm |
140 °F @Thickness >=0.0591 in |
UL 746B |
LG Chemical HF380XC ABS, High Flow, High Surface Gloss Feature: Injection Molding, High Flow, High Surface GlossApplication: High melt flow index is suitable for injection molding of large and complicated part. High thermal stabilities enables to expres.. |
|||
UL RTI, Mechanical with Impact | 60.0 °C @Thickness >=3.00 mm |
140 °F @Thickness >=0.118 in |
|
LG Chemical HF380XC ABS, High Flow, High Surface Gloss Feature: Injection Molding, High Flow, High Surface GlossApplication: High melt flow index is suitable for injection molding of large and complicated part. High thermal stabilities enables to expres.. |
|||
UL RTI, Mechanical with Impact | 60.0 °C @Thickness >=1.20 mm |
140 °F @Thickness >=0.0472 in |
|
LG Chemical LUMAX GN5006FC PBT+ABS, Heat Resistance Description: Injection Molding, PBT+ABS, Halogen Free Flame RetardantApplication: E&E (Connector)CAS: 9003-56-9, 9003-54-7 and 24968-12-5Information provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 60.0 °C @Thickness >=0.750 mm |
140 °F @Thickness >=0.0295 in |
|
LG Chemical LUMID HI5063A(W) PA6/ABS+MF6%, High Impact Feature: Injection Molding, PA6/ABS+MF6%, High ImpactApplication: Electric/Electronic Components (Shaver Die)CAS No. 25038-54-4, 9003-56-9, 9003-54-7 and 14807-96-6Information provided by LG Chemica.. |
|||
UL RTI, Mechanical with Impact | 60.0 °C @Thickness >=1.50 mm |
140 °F @Thickness >=0.0591 in |
|
LG Chemical LUMID HI5083A(W) PA6/ABS+MF8%, High Impact Feature: Injection Molding, PA6/ABS+MF8%, High ImpactApplication: Electric/Electronic Components (Shaver Die)CAS No. 25038-54-4, 9003-56-9, 9003-54-7 and 14807-96-6Information provided by LG Chemica.. |
|||
UL RTI, Mechanical with Impact | 60.0 °C @Thickness >=1.00 mm |
140 °F @Thickness >=0.0394 in |
|
LG Chemical LUPOY GN5008HF PC/ABS, Halogen Free Flame Retardant, High Impact Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, Heat Resistance, High FlowApplication: E&E (OA, Navigation Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provid.. |
|||
UL RTI, Mechanical with Impact | 60.0 °C @Thickness >=1.50 mm |
140 °F @Thickness >=0.0591 in |
|
LG Chemical LUPOY HG5000B PC/ABS, Heat Resistance Description: Injection Molding, PC/ABS, High Gloss, Heat Resistance, High FlowApplication: E&E (housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 60.0 °C @Thickness >=1.50 mm |
140 °F @Thickness >=0.0591 in |
UL 746B |
LG Chemical MP220 ABS, High Adhesion, Heat Resistance Feature: Injection Molding, High Adhesion, Metal PlatingApplication: Automobiles Radiator Grill, MoldingCAS No. 9003-56-9 and 9003-54-7Information provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 60.0 °C @Thickness >=1.50 mm |
140 °F @Thickness >=0.0591 in |
|
LG Chemical RS650 ABS Feature: Extrusion Molding, General PurposeApplication: MiscellaneousCAS No. 9003-56-9Information provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 60.0 °C @Thickness >=3.00 mm |
140 °F @Thickness >=0.118 in |
UL 746B |
LG Chemical RS657L ABS, Chemical Resistance to Cyclopentane, Low Specific Gravity Feature: Extrusion Molding, Chemical Resistance to Cyclopentane, Thin ThicknessApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 60.0 °C @Thickness >=3.00 mm |
140 °F @Thickness >=0.118 in |
UL 746B |
LG Chemical XR401B ABS, High Flow, Heat Resistance Feature: Injection Molding, High Flow, Heat ResistanceApplication: Automotives Exterior Housing (Side Mirror Housing, Garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information p.. |
|||
UL RTI, Mechanical with Impact | 60.0 °C @Thickness >=3.00 mm |
140 °F @Thickness >=0.118 in |
UL 746B |
LG Chemical XR409H ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior Housing (Switch Panel Housing etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provided by LG Ch.. |
|||
UL RTI, Mechanical with Impact | 60.0 °C @Thickness >=2.00 mm |
140 °F @Thickness >=0.0787 in |
|
LG Chemical AF360 ABS, TBBA-free Flame Retardant Feature: Injection Molding, TBBA-free Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 84852-53-9 and 1309-64-4Information provided b.. |
|||
UL RTI, Mechanical with Impact | 60.0 °C @Thickness >=3.00 mm |
140 °F @Thickness >=0.118 in |
|
LG Chemical AF360 ABS, TBBA-free Flame Retardant Feature: Injection Molding, TBBA-free Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 84852-53-9 and 1309-64-4Information provided b.. |
|||
UL RTI, Mechanical with Impact | 60.0 °C @Thickness >=2.00 mm |
140 °F @Thickness >=0.0787 in |
|
LG Chemical LUPOY GN5009F PC/ABS, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, High FlowApplication: IT/OA (Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 60.0 °C @Thickness >=1.50 mm |
140 °F @Thickness >=0.0591 in |
|
LG Chemical TR552 MABS, Transparency, High Impact, Chemical Resistance Feature: Injection Molding, Transparency, High Impact, Chemical ResistanceApplication: Electric/Electronic Applications, Copier, Printer etcCAS No. 9011-14–7 and 9003-56-9Information provided b.. |
|||
UL RTI, Mechanical with Impact | 60.0 °C @Thickness >=3.00 mm |
140 °F @Thickness >=0.118 in |
|
LG Chemical TR552 MABS, Transparency, High Impact, Chemical Resistance Feature: Injection Molding, Transparency, High Impact, Chemical ResistanceApplication: Electric/Electronic Applications, Copier, Printer etcCAS No. 9011-14–7 and 9003-56-9Information provided b.. |
|||
UL RTI, Mechanical with Impact | 60.0 °C @Thickness >=1.50 mm |
140 °F @Thickness >=0.0591 in |
UL 746B |
LG Chemical XR401 ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (Frame etc) Automotives Interior & Exterior Housing (lamp housing etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 .. |
|||
UL RTI, Mechanical with Impact | 60.0 °C @Thickness >=3.00 mm |
140 °F @Thickness >=0.118 in |
UL 746B |
LG Chemical XR401 ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (Frame etc) Automotives Interior & Exterior Housing (lamp housing etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 .. |
|||
UL RTI, Mechanical with Impact | 60.0 °C @Thickness >=3.00 mm |
140 °F @Thickness >=0.118 in |
|
LG Chemical HF350U ABS, High Flow Feature: Injection Molding, High Flow, Good WeatherabilityApplication: E & E Products (Monitor) )CAS No. 9003-56-9Information provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 60.0 °C @Thickness >=3.00 mm |
140 °F @Thickness >=0.118 in |
|
LG Chemical SG175G ABS, Super Surface Gloss, High Flow Feature: Injection Molding, Super Surface Gloss, High FlowApplication: Electric & Electronic ProductsCAS No. 9003-56-9Information provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 60.0 °C @Thickness >=2.00 mm |
140 °F @Thickness >=0.0787 in |
|
LG Chemical LUPOY GN5201F PC/ABS+GF20%, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS+GF20%, Halogen Free Flame Retardant, High StiffnessApplication: E&E (Housing, OA Frame)CAS: 103598-77-2, 9003-56-9, 181028-79-5 and 65997-17-3Information provi.. |