Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical with Impact | 80.0 °C @Thickness 1.50 mm |
176 °F @Thickness 0.0591 in |
UL 746 |
Polymer Resources PC-FR2-TFE Polycarbonate, Flame Retardant, 5% PTFE Polycarbonate, Improved Flame Retardant, 5% PTFE LubricantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
UL RTI, Mechanical with Impact | 80.0 °C @Thickness 3.00 mm |
176 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources PC-FR2-TFE Polycarbonate, Flame Retardant, 5% PTFE Polycarbonate, Improved Flame Retardant, 5% PTFE LubricantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
UL RTI, Mechanical with Impact | 80.0 °C @Thickness 3.00 mm |
176 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources PC-G10 Polycarbonate, 10% Glass Reinforced Polycarbonate, 10% Glass ReinforcedFeatures: • Flame Retardant • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-p.. |
|||
UL RTI, Mechanical with Impact | 80.0 °C @Thickness 1.70 mm |
176 °F @Thickness 0.0669 in |
UL 746 |
Polymer Resources PC-G20 Polycarbonate, 20% Glass Reinforced Polycarbonate, 20% Glass ReinforcedFeatures: • Flame Retardant • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-p.. |
|||
UL RTI, Mechanical with Impact | 80.0 °C @Thickness 0.749 mm |
176 °F @Thickness 0.0295 in |
UL 746 |
Polymer Resources PC-GP1-D-[color]-1 Polycarbonate, General Purpose, Low Flow with Mold Release Polycarbonate, General Purpose, Low Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
UL RTI, Mechanical with Impact | 80.0 °C @Thickness 0.749 mm |
176 °F @Thickness 0.0295 in |
UL 746 |
Polymer Resources PC-GP2-D Polycarbonate, General Purpose, Medium Flow Polycarbonate, General Purpose, Medium FlowFeatures: • Ultra High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on.. |
|||
UL RTI, Mechanical with Impact | 80.0 °C @Thickness 0.749 mm |
176 °F @Thickness 0.0295 in |
UL 746 |
Polymer Resources PC-GP2-D-[color]-1 Polycarbonate, General Purpose, Medium Flow with Mold Release Polycarbonate, General Purpose, Medium Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inf.. |
|||
UL RTI, Mechanical with Impact | 80.0 °C @Thickness 1.50 mm |
176 °F @Thickness 0.0591 in |
UL 746 |
Polymer Resources PC-GP4 Polycarbonate, General Purpose, Easy Flow Polycarbonate, General Purpose, Easy FlowFeatures: • High Impact Resistance • Self Extinguishing • High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conduc.. |
|||
UL RTI, Mechanical with Impact | 80.0 °C @Thickness 3.00 mm |
176 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources PC-GP4-[color]-1 Polycarbonate, General Purpose, Easy Flow with Mold Release Polycarbonate, General Purpose, Easy Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor.. |
|||
UL RTI, Mechanical with Impact | 80.0 °C @Thickness 1.50 mm |
176 °F @Thickness 0.0591 in |
UL 746 |
Polymer Resources PC-HM-FR1 Polycarbonate, 10% Glass Reinforced, Flame Retardant Polycarbonate, 10% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information .. |
|||
UL RTI, Mechanical with Impact | 80.0 °C @Thickness 3.00 mm |
176 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources PC-HM-FR1-[color]-1 Polycarbonate, 10% Glass Reinforced, Flame Retardant with Mold Release Polycarbonate, 10% Glass Reinforced, Flame Retardant with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sa.. |
|||
UL RTI, Mechanical with Impact | 80.0 °C @Thickness 0.749 mm |
176 °F @Thickness 0.0295 in |
UL 746 |
Polymer Resources PC-UV2-D-[color]-1 Polycarbonate, UV-stabilized, Medium Flow with Mold Release Polycarbonate, UV-stabilized, Medium Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor.. |
|||
UL RTI, Mechanical with Impact | 80.0 °C @Thickness 3.00 mm |
176 °F @Thickness 0.118 in |
UL 746B |
DuPont Performance Polymers Delrin® 500CL BK601 Acetal Homopolymer
(Unverified Data**) Delrin® 500CL BK601 is a medium viscosity acetal homopolymer containing a chemical lubricant, designed for low wear and friction against metals.Information provided by DuPont Performance Polymers |
|||
UL RTI, Mechanical with Impact | 80.0 °C @Thickness >=0.500 mm |
176 °F @Thickness >=0.0197 in |
|
LG Chemical Lupoy 1302-05 Polycarbonate Resin Description: LUPOY 1302-5 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main.. |
|||
UL RTI, Mechanical with Impact | 80.0 °C @Thickness >=3.00 mm |
176 °F @Thickness >=0.118 in |
|
LG Chemical LUPOY GN1002FH PC, Halogen Free, Flame Retardant, Heat Resistant Description: Injection Molding, PC, Halogen Free Flame Retardant, Heat Resistant, Chemical Resistance, High ImpactApplication: IT/OA Housing and Components (Adaptor)CAS: 103598-77-2, 25232-40-0 and .. |
|||
UL RTI, Mechanical with Impact | 80.0 °C @Thickness >=2.00 mm |
176 °F @Thickness >=0.0787 in |
|
LG Chemical LUPOY GN5001RFH PC/ABS, Halogen Free Flame Retardant, Heat Resistance Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, Heat ResistanceApplication: E&E (TV, Navigation Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Ch.. |
|||
UL RTI, Mechanical with Impact | 80.0 °C @Thickness >=3.00 mm |
176 °F @Thickness >=0.118 in |
|
LG Chemical LUPOY GN5001RFM PC/ABS, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, General PurposeApplication: E&E (Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 80.0 °C @Thickness >=1.50 mm |
176 °F @Thickness >=0.0591 in |
|
LG Chemical LUPOY HI1002ML PC, High Impact Description: Injection Molding, PC, General Purpose, High Impact, Chemical ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 9046-16-6Information provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 80.0 °C @Thickness >=3.00 mm |
176 °F @Thickness >=0.118 in |
|
LG Chemical LUPOY SC2302 PC+GF30%, High Impact Description: Injection Molding, PC+GF30%, Good Toughness, Good Impact, Chemical ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 65997-17-3Information provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 80.0 °C @Thickness >=1.70 mm |
176 °F @Thickness >=0.0669 in |
|
LG Chemical LUPOY SC3154 PC+GF15% Description: Injection Molding, PC+GF15%, General Purpose, Good Toughness, Dimensional Stability, Good Surface, Chemical ResistanceApplication: Mobile Phone Housing and ComponentsInformation provide.. |
|||
UL RTI, Mechanical with Impact | 80.0 °C @Thickness >=0.500 mm |
176 °F @Thickness >=0.0197 in |
|
LG Chemical Lupoy 1200HP-15 Polycarbonate Resin Description: LUPOY PC 1200HP-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
UL RTI, Mechanical with Impact | 80.0 °C @Thickness >=0.500 mm |
176 °F @Thickness >=0.0197 in |
|
LG Chemical Lupoy 1302HP-10 Polycarbonate Resin Description: LUPOY PC 1302HP-10 resin is designed for extrusion products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Characteristics.. |
|||
UL RTI, Mechanical with Impact | 80.0 °C @Thickness >=0.500 mm |
176 °F @Thickness >=0.0197 in |
|
LG Chemical Lupoy 1302HP-21 Polycarbonate Resin Description: LUPOY PC 1302HP-21 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
UL RTI, Mechanical with Impact | 80.0 °C @Thickness >=0.500 mm |
176 °F @Thickness >=0.0197 in |
|
LG Chemical Lupoy 1302HP-22 Polycarbonate Resin Description: LUPOY PC 1302HP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
UL RTI, Mechanical with Impact | 80.0 °C @Thickness >=1.00 mm |
176 °F @Thickness >=0.0394 in |
|
LG Chemical LUPOY EF1006F PC, Halogen Free, Flame Retardant, High Heat Resistance Description: Injection Molding, PC, Halogen Free Flame Retardant, High Heat ResistanceApplication: IT/OA Housing and Components (Adaptor)CAS: 103598-77-2Information provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 80.0 °C @Thickness >=1.50 mm |
176 °F @Thickness >=0.0591 in |
|
LG Chemical LUPOY GN5001RF PC/ABS, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, Good FlowApplication: E&E (TV, Navigation Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical.. |
|||
UL RTI, Mechanical with Impact | 80.0 °C @Thickness >=1.50 mm |
176 °F @Thickness >=0.0591 in |
|
LG Chemical LUPOY GN5001RFJ PC/ABS, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, High FlowApplication: IT/OA (OA Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 80.0 °C @Thickness >=2.00 mm |
176 °F @Thickness >=0.0787 in |
|
LG Chemical LUPOY GN5001RFJ PC/ABS, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, High FlowApplication: IT/OA (OA Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 80.0 °C @Thickness >=3.00 mm |
176 °F @Thickness >=0.118 in |
|
LG Chemical LUPOY GN5001RFJ PC/ABS, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, High FlowApplication: IT/OA (OA Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 80.0 °C @Thickness >=0.500 mm |
176 °F @Thickness >=0.0197 in |
|
LG Chemical Lupoy 1302HP-07 Polycarbonate Resin Description: LUPOY PC 1302HP-07 resin is designed for extrusion products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Characteristics.. |