Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 3.00 mm |
167 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources PC/TP-GP2 PC/Polyester Alloy High Impact, Excellent Chemical ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided b.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 0.749 mm |
167 °F @Thickness 0.0295 in |
UL 746 |
Polymer Resources TP-FR-IM2 Polybutylene Terephthalate, Impact Modified, Flame Retardant, High Flow Polybutylene Terephthalate, Impact Modified, Flame Retardant, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test s.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 3.00 mm |
167 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources TP-G30 Polybutylene Terephthalate, 30% Glass Reinforced Polybutylene Terephthalate, 30% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information prov.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 1.50 mm |
167 °F @Thickness 0.0591 in |
UL 746 |
Polymer Resources TP-IGFR-G30 Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant, Reduced Warpage Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant, Reduced WarpageProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmen.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 3.00 mm |
167 °F @Thickness 0.118 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® 101F BKB009 Nylon 66
(Unverified Data**) Zytel® 101F BKB009 is an internally lubricated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont Performance Polymers |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 6.00 mm |
167 °F @Thickness 0.236 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® 101F BKB009 Nylon 66
(Unverified Data**) Zytel® 101F BKB009 is an internally lubricated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont Performance Polymers |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness >=3.00 mm |
167 °F @Thickness >=0.118 in |
|
LG Chemical AF312 ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness >=2.50 mm |
167 °F @Thickness >=0.0984 in |
|
LG Chemical AF312T ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness >=0.800 mm |
167 °F @Thickness >=0.0315 in |
|
LG Chemical Lupox® NH2306F PBT+GF30% Description: Injection Molding, PBT+GF30%, Halogen Free Flame RetardantApplication: IT/OA, E&E (Connector)CAS No. 65997-17-3 and 24968-12-5Information provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness >=1.60 mm |
167 °F @Thickness >=0.0630 in |
|
LG Chemical Lupox® NH2306F PBT+GF30% Description: Injection Molding, PBT+GF30%, Halogen Free Flame RetardantApplication: IT/OA, E&E (Connector)CAS No. 65997-17-3 and 24968-12-5Information provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 0.810 mm |
167 °F @Thickness 0.0319 in |
UL 746 |
Teknor Apex Chemlon® 223 Nylon 6, Unreinforced Features: Nucleated for fast cyclingProcessing Method: Injection MoldingForms: Pellets Additive: Nucleating AgentInformation Provided by Teknor Apex |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 1.60 mm |
167 °F @Thickness 0.0630 in |
|
Eurostar Starflam R10002E PA66/6, Injection Molded Starflam R10002E is a Unfilled, Halogen Free and Red Phosphorous Free, Flame Retardant, Polyamide 66/Polyamide 6 Injection Molding Resin (also known as R1000Z220EM)Information provided by Polymer Te.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 0.710 mm |
167 °F @Thickness 0.0280 in |
UL 746 |
Ascend Performance Materials Vydyne® 20NSP1 Nylon 66, DAM Availability:Asia PacificEuropeNorth AmericaFiller/Reinforcement:Glass Fiber, 43% Filler by Weight Additive:Nucleating AgentLubricant Features:Fast Molding CycleGeneral PurposeGood Mold Release Good.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 3.00 mm |
167 °F @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® 21SPC Nylon 66, DAM Vydyne® 21SPC is a general-purpose PA66 resin available in natural color. It is designed principally for injection-molding fabrication. This resin offers a well balanced combination of engineering .. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 0.710 mm |
167 °F @Thickness 0.0280 in |
UL 746 |
Ascend Performance Materials Vydyne® 21SPF BLK Nylon 66, Conditioned Vydyne® 21SPF BLK is a, general-purpose PA66 resin used for extrusion-compounding. Available in black, it is designed principally for injection-molding fabrication. This grade offers a well-balance.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 3.00 mm |
167 °F @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® 21SPG1 Nylon 66, DAM Availability:Asia PacificEuropeNorth America Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood ToughnessHigh Rigidit.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 3.00 mm |
167 °F @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® 47H Nylon 66, Impact Modified, DAM Vydyne® 47H is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne 4.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 3.00 mm |
167 °F @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® 47H Nylon 66, Impact Modified, DAM Vydyne® 47H is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne 4.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 3.00 mm |
167 °F @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® 49 Nylon 66, DAM Vydyne® 49 is a general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved imp.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 0.750 mm |
167 °F @Thickness 0.0295 in |
UL 746 |
Ascend Performance Materials Vydyne® 41 Nylon 66, DAM Vydyne® 41 is a general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved imp.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 1.50 mm |
167 °F @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® 41 Nylon 66, DAM Vydyne® 41 is a general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved imp.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 0.750 mm |
167 °F @Thickness 0.0295 in |
UL 746 |
Ascend Performance Materials Vydyne® 41H BK03 Nylon 66, Impact Modified, DAM Vydyne® 41H BK03 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 3.00 mm |
167 °F @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® 41H BK03 Nylon 66, Impact Modified, DAM Vydyne® 41H BK03 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 3.00 mm |
167 °F @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® 47 BK11 Nylon 66, Impact Modified, DAM Vydyne® 47H BK11 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 1.50 mm |
167 °F @Thickness 0.0591 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® ST801 NC010A Nylon 66
(Unverified Data**) Zytel® ST801 is an unreinforced, super tough polyamide 66 for injection molding and extrusion. It offers outstanding break resistance over a wide temperature and humidity range and high productivit.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 0.400 mm |
167 °F @Thickness 0.0157 in |
UL 746 |
Ascend Performance Materials Vydyne® ECO366 Nylon 66, Flame-retardant, DAM Vydyne® ECO366 is a non-halogenated, unfilled, flame-retardant PA66 homopolymer designed with superior flow properties to assist in filling thin-walled, intricate parts. It is lubricated for machin.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 0.710 mm |
167 °F @Thickness 0.0280 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® EFE1068 NC010T Nylon 66
(Unverified Data**) Zytel® EFE1068 NC010T is a lubricated polyamide 66 for injection molding. It has excellent flow characteristics and was developed for fast production cycles and high productivity applications.Info.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 6.00 mm |
167 °F @Thickness 0.236 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® EFE1068 NC010T Nylon 66
(Unverified Data**) Zytel® EFE1068 NC010T is a lubricated polyamide 66 for injection molding. It has excellent flow characteristics and was developed for fast production cycles and high productivity applications.Info.. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 0.710 mm |
167 °F @Thickness 0.0280 in |
UL 746 |
Ascend Performance Materials Vydyne® 21SPF1 Nylon 66, DAM Vydyne® 21SPF1 is a general-purpose PA66 resin available in natural color. It is designed principally for injection-molding applications with the added benefits of improved flow during the molding .. |
|||
UL RTI, Mechanical with Impact | 75.0 °C @Thickness 1.50 mm |
167 °F @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® 21SPF1 Nylon 66, DAM Vydyne® 21SPF1 is a general-purpose PA66 resin available in natural color. It is designed principally for injection-molding applications with the added benefits of improved flow during the molding .. |