Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Electrical | 60.0 °C @Thickness 1.50 mm |
140 °F @Thickness 0.0591 in |
UL 746 |
Polymer Resources ABS-GP1-[color]-EP General Purpose ABS, Electroplating Grade General Purpose Acrylonitrile Butadiene Styrene, Electroplating GradeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sam.. |
|||
UL RTI, Electrical | 60.0 °C @Thickness 3.00 mm |
140 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources ABS-GP1-[color]-EP General Purpose ABS, Electroplating Grade General Purpose Acrylonitrile Butadiene Styrene, Electroplating GradeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sam.. |
|||
UL RTI, Electrical | 60.0 °C @Thickness 3.00 mm |
140 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources PC/ABS-FR1 Flame Retardant PC/ABS Alloy PC/ABS Alloy, Flame Retardant, Standard FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided.. |
|||
UL RTI, Electrical | 60.0 °C @Thickness 3.00 mm |
140 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources PC/ABS-FR2 Flame Retardant PC/ABS Alloy, High Flow PC/ABS Alloy, Flame Retardant, Higher FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided b.. |
|||
UL RTI, Electrical | 60.0 °C @Thickness >=1.00 mm |
140 °F @Thickness >=0.0394 in |
UL 746B |
LG Chemical AF312B ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical.. |
|||
UL RTI, Electrical | 60.0 °C @Thickness >=2.50 mm |
140 °F @Thickness >=0.0984 in |
|
LG Chemical AF342F ABS, Flame Retardant, High Flow Feature: Injection Molding, Flame Retardant, High FlowApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provided .. |
|||
UL RTI, Electrical | 60.0 °C @Thickness >=1.50 mm |
140 °F @Thickness >=0.0591 in |
UL 746B |
LG Chemical ER451 ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior & Exterior Housing (garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemica.. |
|||
UL RTI, Electrical | 60.0 °C @Thickness >=1.50 mm |
140 °F @Thickness >=0.0591 in |
UL 746B |
LG Chemical FH380P ABS, High Flow Feature: Injection Molding, High Flow, Good PaintabilityApplication: Electric & Electronic Painting Products)CAS No. 9003-56-9Information provided by LG Chemical |
|||
UL RTI, Electrical | 60.0 °C @Thickness >=1.50 mm |
140 °F @Thickness >=0.0591 in |
UL 746B |
LG Chemical HF380I ABS, High Flow Feature: Injection Molding, High Flow, Good PaintabilityApplication: Painting Products of Motor Cycle)CAS No. 9003-56-9Information provided by LG Chemical |
|||
UL RTI, Electrical | 60.0 °C @Thickness >=1.50 mm |
140 °F @Thickness >=0.0591 in |
UL 746B |
LG Chemical HI153 ABS, High Flow Feature: Injection Molding, High Flow, Good WeatherabilityApplication: Electric & Electronic Products, Miscellaneous GoodsCAS No. 9003-56-9Information provided by LG Chemical |
|||
UL RTI, Electrical | 60.0 °C @Thickness >=1.50 mm |
140 °F @Thickness >=0.0591 in |
|
LG Chemical LUMAX GN5006FC PBT+ABS, Heat Resistance Description: Injection Molding, PBT+ABS, Halogen Free Flame RetardantApplication: E&E (Connector)CAS: 9003-56-9, 9003-54-7 and 24968-12-5Information provided by LG Chemical |
|||
UL RTI, Electrical | 60.0 °C @Thickness >=1.50 mm |
140 °F @Thickness >=0.0591 in |
|
LG Chemical LUMAX GP5106FI PBT+ABS+GF10%, Flame Retardant Description: Injection Molding Grade, PBT+ABS+GF10%, Flame Retardant, Impact Modified, Dimensional StabilityApplication: E&E (Switch)CAS: 9003-56-9, 68928-70-1, 65997-17-3, 24968-12-5, 9003-54-7 an.. |
|||
UL RTI, Electrical | 60.0 °C @Thickness >=3.00 mm |
140 °F @Thickness >=0.118 in |
|
LG Chemical LUMID HI5063A(W) PA6/ABS+MF6%, High Impact Feature: Injection Molding, PA6/ABS+MF6%, High ImpactApplication: Electric/Electronic Components (Shaver Die)CAS No. 25038-54-4, 9003-56-9, 9003-54-7 and 14807-96-6Information provided by LG Chemica.. |
|||
UL RTI, Electrical | 60.0 °C @Thickness >=1.20 mm |
140 °F @Thickness >=0.0472 in |
|
LG Chemical LUPOY GN5001RFH PC/ABS, Halogen Free Flame Retardant, Heat Resistance Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, Heat ResistanceApplication: E&E (TV, Navigation Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Ch.. |
|||
UL RTI, Electrical | 60.0 °C @Thickness >=1.50 mm |
140 °F @Thickness >=0.0591 in |
UL 746B |
LG Chemical MP220 ABS, High Adhesion, Heat Resistance Feature: Injection Molding, High Adhesion, Metal PlatingApplication: Automobiles Radiator Grill, MoldingCAS No. 9003-56-9 and 9003-54-7Information provided by LG Chemical |
|||
UL RTI, Electrical | 60.0 °C @Thickness >=3.00 mm |
140 °F @Thickness >=0.118 in |
UL 746B |
LG Chemical MP220 ABS, High Adhesion, Heat Resistance Feature: Injection Molding, High Adhesion, Metal PlatingApplication: Automobiles Radiator Grill, MoldingCAS No. 9003-56-9 and 9003-54-7Information provided by LG Chemical |
|||
UL RTI, Electrical | 60.0 °C @Thickness >=1.50 mm |
140 °F @Thickness >=0.0591 in |
UL 746B |
LG Chemical PT270 ABS Feature: Injection Molding, Good PaintabilityApplication: Exterior Part of Automobile and Motor cycleCAS No. 9003-56-9Information provided by LG Chemical |
|||
UL RTI, Electrical | 60.0 °C @Thickness >=1.50 mm |
140 °F @Thickness >=0.0591 in |
UL 746B |
LG Chemical XR409E ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior Housing (Switch Panel Housing etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provided by LG Ch.. |
|||
UL RTI, Electrical | 60.0 °C @Thickness >=3.00 mm |
140 °F @Thickness >=0.118 in |
UL 746B |
LG Chemical XR409E ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior Housing (Switch Panel Housing etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provided by LG Ch.. |
|||
UL RTI, Electrical | 60.0 °C @Thickness >=3.00 mm |
140 °F @Thickness >=0.118 in |
UL 746B |
LG Chemical XR409H ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior Housing (Switch Panel Housing etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provided by LG Ch.. |
|||
UL RTI, Electrical | 60.0 °C @Thickness >=2.00 mm |
140 °F @Thickness >=0.0787 in |
|
LG Chemical AF360 ABS, TBBA-free Flame Retardant Feature: Injection Molding, TBBA-free Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 84852-53-9 and 1309-64-4Information provided b.. |
|||
UL RTI, Electrical | 60.0 °C @Thickness >=3.00 mm |
140 °F @Thickness >=0.118 in |
|
LG Chemical AF360 ABS, TBBA-free Flame Retardant Feature: Injection Molding, TBBA-free Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 84852-53-9 and 1309-64-4Information provided b.. |
|||
UL RTI, Electrical | 60.0 °C @Thickness >=1.50 mm |
140 °F @Thickness >=0.0591 in |
|
LG Chemical LUPOY GN5001EF PC/ABS, Br, Cal-free flame retardant Description: Injection Molding, PC/ABS, Halogen Free Flame RetardantApplication: Industrial / IT productCAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical |
|||
UL RTI, Electrical | 60.0 °C @Thickness >=1.20 mm |
140 °F @Thickness >=0.0472 in |
|
LG Chemical LUPOY GN5001RF PC/ABS, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, Good FlowApplication: E&E (TV, Navigation Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical.. |
|||
UL RTI, Electrical | 60.0 °C @Thickness >=1.20 mm |
140 °F @Thickness >=0.0472 in |
|
LG Chemical LUPOY GN5001RFJ PC/ABS, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, High FlowApplication: IT/OA (OA Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical |
|||
UL RTI, Electrical | 60.0 °C @Thickness >=1.50 mm |
140 °F @Thickness >=0.0591 in |
|
LG Chemical LUPOY GN5009F PC/ABS, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, High FlowApplication: IT/OA (Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical |
|||
UL RTI, Electrical | 60.0 °C @Thickness >=2.00 mm |
140 °F @Thickness >=0.0787 in |
|
LG Chemical LUPOY GN5009F PC/ABS, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, High FlowApplication: IT/OA (Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical |
|||
UL RTI, Electrical | 60.0 °C @Thickness >=3.00 mm |
140 °F @Thickness >=0.118 in |
|
LG Chemical LUPOY GN5009F PC/ABS, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, High FlowApplication: IT/OA (Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical |
|||
UL RTI, Electrical | 60.0 °C @Thickness >=3.00 mm |
140 °F @Thickness >=0.118 in |
UL 746B |
LG Chemical XR407E ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (MWO Frame, DVD inner part etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provided by.. |
|||
UL RTI, Electrical | 60.0 °C @Thickness >=3.00 mm |
140 °F @Thickness >=0.118 in |
|
LG Chemical HF350U ABS, High Flow Feature: Injection Molding, High Flow, Good WeatherabilityApplication: E & E Products (Monitor) )CAS No. 9003-56-9Information provided by LG Chemical |