Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Electrical | 90.0 °C @Thickness >=3.00 mm |
194 °F @Thickness >=0.118 in |
|
LG Chemical LUMID GP2259AFL PA6+GF25%, Flame Retardant Feature: Injection Molding, PA6+GF25%, Flame RetardantApplication: IT/OA (Connector)CAS No. 25038-54-4, 65997-17-3, 1163-19-5, 1309-64-4 and 138265-88-0Information provided by LG Chemical |
|||
UL RTI, Electrical | 90.0 °C @Thickness 1.40 mm |
194 °F @Thickness 0.0551 in |
UL 746 |
Teknor Apex APEX® 1015 Polyvinyl Chloride, Semi-Rigid Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
UL RTI, Electrical | 90.0 °C @Thickness 3.00 mm |
194 °F @Thickness 0.118 in |
UL 746 |
Teknor Apex APEX® 1015 Polyvinyl Chloride, Semi-Rigid Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
UL RTI, Electrical | 90.0 °C @Thickness 0.889 mm |
194 °F @Thickness 0.0350 in |
UL 746 |
Teknor Apex APEX® 1017 Polyvinyl Chloride, Semi-Rigid Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
UL RTI, Electrical | 90.0 °C @Thickness 3.00 mm |
194 °F @Thickness 0.118 in |
UL 746 |
Teknor Apex APEX® 1017 Polyvinyl Chloride, Semi-Rigid Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
UL RTI, Electrical | 90.0 °C @Thickness 0.889 mm |
194 °F @Thickness 0.0350 in |
UL 746 |
Teknor Apex APEX® 1008 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
UL RTI, Electrical | 90.0 °C @Thickness 1.40 mm |
194 °F @Thickness 0.0551 in |
UL 746 |
Teknor Apex APEX® 1008 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
UL RTI, Electrical | 90.0 °C @Thickness 3.00 mm |
194 °F @Thickness 0.118 in |
UL 746 |
Teknor Apex APEX® 1020 Polyvinyl Chloride, Semi-Rigid Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
UL RTI, Electrical | 90.0 °C @Thickness 0.810 mm |
194 °F @Thickness 0.0319 in |
UL 746 |
Teknor Apex APEX® 4101 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
UL RTI, Electrical | 90.0 °C @Thickness 0.810 mm |
194 °F @Thickness 0.0319 in |
UL 746 |
Teknor Apex APEX® 4103 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
UL RTI, Electrical | 90.0 °C @Thickness 3.00 mm |
194 °F @Thickness 0.118 in |
UL 746 |
Teknor Apex APEX® 4103 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
UL RTI, Electrical | 90.0 °C @Thickness 0.810 mm |
194 °F @Thickness 0.0319 in |
UL 746 |
Teknor Apex APEX® 4107 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
UL RTI, Electrical | 90.0 °C @Thickness 3.00 mm |
194 °F @Thickness 0.118 in |
UL 746 |
Teknor Apex APEX® 4107 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
UL RTI, Electrical | 90.0 °C @Thickness 3.00 mm |
194 °F @Thickness 0.118 in |
UL 746 |
Teknor Apex APEX® 4112 Polyvinyl Chloride, Flexible Notes: 75°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Mold.. |
|||
UL RTI, Electrical | 90.0 °C @Thickness 1.00 mm |
194 °F @Thickness 0.0394 in |
UL 746 |
Teknor Apex APEX® 76-5179-B Polyvinyl Chloride, Flexible Notes: 80°C General Purpose; RoHS Compliant Features: Flame Retardant Uses: Wire and Cable ApplicationsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709Addition.. |
|||
UL RTI, Electrical | 90.0 °C @Thickness 3.00 mm |
194 °F @Thickness 0.118 in |
UL 746 |
Teknor Apex APEX® 76-5179-B Polyvinyl Chloride, Flexible Notes: 80°C General Purpose; RoHS Compliant Features: Flame Retardant Uses: Wire and Cable ApplicationsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709Addition.. |
|||
UL RTI, Electrical | 90.0 °C @Thickness 3.00 mm |
194 °F @Thickness 0.118 in |
UL 746 |
Teknor Apex APEX® 1001 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
UL RTI, Electrical | 90.0 °C @Thickness 1.40 mm |
194 °F @Thickness 0.0551 in |
UL 746 |
Teknor Apex APEX® 1002 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
UL RTI, Electrical | 90.0 °C @Thickness 3.00 mm |
194 °F @Thickness 0.118 in |
UL 746 |
Teknor Apex APEX® 1002 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
UL RTI, Electrical | 90.0 °C @Thickness 3.00 mm |
194 °F @Thickness 0.118 in |
UL 746 |
Teknor Apex APEX® 1003 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
UL RTI, Electrical | 90.0 °C @Thickness 0.889 mm |
194 °F @Thickness 0.0350 in |
UL 746 |
Teknor Apex APEX® 1004 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
UL RTI, Electrical | 90.0 °C @Thickness 1.40 mm |
194 °F @Thickness 0.0551 in |
UL 746 |
Teknor Apex APEX® 1004 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
UL RTI, Electrical | 90.0 °C @Thickness 1.40 mm |
194 °F @Thickness 0.0551 in |
UL 746 |
Teknor Apex APEX® 1007 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
UL RTI, Electrical | 90.0 °C @Thickness 0.889 mm |
194 °F @Thickness 0.0350 in |
UL 746 |
Teknor Apex APEX® 1009 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
UL RTI, Electrical | 90.0 °C @Thickness 1.40 mm |
194 °F @Thickness 0.0551 in |
UL 746 |
Teknor Apex APEX® 1009 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
UL RTI, Electrical | 90.0 °C @Thickness 3.00 mm |
194 °F @Thickness 0.118 in |
UL 746 |
Teknor Apex APEX® 1011 Polyvinyl Chloride, Semi-Rigid Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
UL RTI, Electrical | 90.0 °C @Thickness 0.810 mm |
194 °F @Thickness 0.0319 in |
UL 746 |
Teknor Apex APEX® 4011 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
UL RTI, Electrical | 90.0 °C @Thickness 3.00 mm |
194 °F @Thickness 0.118 in |
UL 746 |
Teknor Apex APEX® 4011 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
UL RTI, Electrical | 90.0 °C @Thickness 3.00 mm |
194 °F @Thickness 0.118 in |
UL 746 |
Teknor Apex APEX® 4020 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
UL RTI, Electrical | 90.0 °C @Thickness 3.00 mm |
194 °F @Thickness 0.118 in |
UL 746 |
Teknor Apex APEX® 1013 Polyvinyl Chloride, Semi-Rigid Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molded .. |