Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Electrical | 50.0 °C @Thickness 0.750 mm |
122 °F @Thickness 0.0295 in |
UL 746B |
DuPont Performance Polymers Delrin® 500AL NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 500AL is a medium viscosity acetal homopolymer, with an advanced system of lubrication for applications requiring low wear and/or coefficient of friction against steel, itself or other plas.. |
|||
UL RTI, Electrical | 50.0 °C @Thickness 0.750 mm |
122 °F @Thickness 0.0295 in |
UL 746B |
DuPont Performance Polymers Delrin® 500P BK602 Acetal Homopolymer
(Unverified Data**) Delrin® 500P BK602 is a general purpose medium viscosity black acetal homopolymer resin for injection molding. Delrin® 500P has improved processing thermal stability compared to Delrin® 500.Infor.. |
|||
UL RTI, Electrical | 50.0 °C @Thickness 0.800 mm |
122 °F @Thickness 0.0315 in |
UL 746B |
DuPont Performance Polymers Delrin® 988PA NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 988PA NC010 is a low viscosity acetal homopolymer for injection molding with low screw deposit. It is especially formulated for gear applications requiring high precision and dimensional st.. |
|||
UL RTI, Electrical | 50.0 °C @Thickness 3.00 mm |
122 °F @Thickness 0.118 in |
UL 746B |
DuPont Performance Polymers Delrin® 988PA NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 988PA NC010 is a low viscosity acetal homopolymer for injection molding with low screw deposit. It is especially formulated for gear applications requiring high precision and dimensional st.. |
|||
UL RTI, Electrical | 50.0 °C @Thickness >=3.00 mm |
122 °F @Thickness >=0.118 in |
|
LG Chemical ALPHALAC SF510 HIPS Super flow, High gloss and high impact equivalent to ABS, Excellent mechanical properties compare with general HIPS, Meet requirements for cost and quality, Applications include TV cabinets, thin pa.. |
|||
UL RTI, Electrical | 50.0 °C @Thickness >=3.00 mm |
122 °F @Thickness >=0.118 in |
|
LG Chemical ALPHALAC SG960 HIPS Description: Injection Molding, General Purpose, Good ProcessabilityApplication: Washer Cover, Air-conditioner Panel, Refrigerator PartsCAS No. 9003-55-8Information provided by LG Chemical |
|||
UL RTI, Electrical | 50.0 °C @Thickness >=3.00 mm |
122 °F @Thickness >=0.118 in |
|
LG Chemical ALPHALAC SG970 HIPS Description: Injection Molding, General Purpose, Good Processability, High glossApplication: Air Conditioner Panel, Washer CoverCAS No. 9003-55-8Information provided by LG Chemical |
|||
UL RTI, Electrical | 50.0 °C @Thickness >=2.50 mm |
122 °F @Thickness >=0.0984 in |
|
LG Chemical HIPS 406AF PS, Flame Retardant Description: Injection Molding, PS, Flame RetardantApplication: Office Appliances (Parts of Printer or Copier)CAS: 9003-55-8, 25713-60-4 and 1309-64-4Information provided by LG Chemical |
|||
UL RTI, Electrical | 50.0 °C @Thickness >=1.50 mm |
122 °F @Thickness >=0.0591 in |
|
LG Chemical HIPS 410AF PS, Flame Retardant Description: Injection Molding, PS, Flame RetardantApplication: Office Appliances (Parts of Printer or Copier)CAS: 9003-55-8, 25713-60-4 and 1309-64-4Information provided by LG Chemical |
|||
UL RTI, Electrical | 50.0 °C @Thickness >=1.60 mm |
122 °F @Thickness >=0.0630 in |
|
LG Chemical HIPS 460AF PS, Flame Retardant Description: Injection Molding, PS, Flame RetardantApplication: Electric Parts Requiring Flame RetardancyCAS: 9003-55-8, 25713-60-4, 84852-53-9 and 1309-64-4Information provided by LG Chemical |
|||
UL RTI, Electrical | 50.0 °C @Thickness >=3.00 mm |
122 °F @Thickness >=0.118 in |
|
LG Chemical HIPS 60HRI PS, Impact Modified Description: Injection Molding, PS, General Purpose, Impact ModifiedApplication: TV Sets, Tape Recorders, Vacuum Cleaner, Washing Machine, Air ConditionerCAS: 9003-55-8Information provided by LG Che.. |
|||
UL RTI, Electrical | 50.0 °C @Thickness >=1.50 mm |
122 °F @Thickness >=0.0591 in |
|
LG Chemical HIPS 65IHE PS, Impact Modified Description: Injection Molding, PS, General Purpose, Impact ModifiedApplication: Refrigerator Tray, Food Tray, Refrigerator Door LinerCAS: 9003-55-8Information provided by LG Chemical |
|||
UL RTI, Electrical | 50.0 °C @Thickness >=3.00 mm |
122 °F @Thickness >=0.118 in |
|
LG Chemical HIPS MI770 PS, Impact Modified Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica.. |
|||
UL RTI, Electrical | 50.0 °C @Thickness >=1.50 mm |
122 °F @Thickness >=0.0591 in |
|
LG Chemical KEYFLEX BT 10288D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Low ModulusApplication: Automotive Interior, Soft Touch GripsCAS: 37282-12-5Information provided by LG Chemical |
|||
UL RTI, Electrical | 50.0 °C @Thickness >=1.50 mm |
122 °F @Thickness >=0.0591 in |
|
LG Chemical LI911 ASA Description: Good Weatherability, High FlowApplication: Air-conditioner grill, Sawing Machine Cover, Electric/Electronic ApplicationsCAS: 26299-47-8Information provided by LG Chemical |
|||
UL RTI, Electrical | 50.0 °C @Thickness >=3.00 mm |
122 °F @Thickness >=0.118 in |
|
LG Chemical LI911 ASA Description: Good Weatherability, High FlowApplication: Air-conditioner grill, Sawing Machine Cover, Electric/Electronic ApplicationsCAS: 26299-47-8Information provided by LG Chemical |
|||
UL RTI, Electrical | 50.0 °C @Thickness >=1.50 mm |
122 °F @Thickness >=0.0591 in |
|
LG Chemical TR557 MABS, High Transparency, High Impact Feature: Injection Molding, High Transparency, High ImpactApplication: Electric/Electronic Applications, Copier, Printer etc.CAS No. 9011-14–7 and 9003-56-9Information provided by LG Chemical |
|||
UL RTI, Electrical | 50.0 °C @Thickness >=3.00 mm |
122 °F @Thickness >=0.118 in |
|
LG Chemical 80HF SAN, High Transparency, Heat Resistance, Chemical Resistance Feature: Injection Molding, SAN, High Transparency, Heat Resistance, Chemical ResistanceApplication: Refrigerator Sleeves, MiscellaneousCAS No. 9003-54-7Information provided by LG Chemical |
|||
UL RTI, Electrical | 50.0 °C @Thickness >=1.50 mm |
122 °F @Thickness >=0.0591 in |
|
LG Chemical 80HFICELLHK SAN, High Transparency, Heat Resistance, Chemical Resistance Feature: Injection Molding, SAN, High Transparency, Heat Resistance, Chemical ResistanceApplication: Refrigerator Sleeves, MiscellaneousCAS No. 9003-54-7Information provided by LG Chemical |
|||
UL RTI, Electrical | 50.0 °C @Thickness >=1.50 mm |
122 °F @Thickness >=0.0591 in |
|
LG Chemical ALPHALAC SG970NSU HIPS Description: Injection Molding, General Purpose, Good Processability, High gloss, antistatic and UV stabilizedApplication: Air Conditioner Panel, Washer CoverCAS No. 9003-55-8Information provided by.. |
|||
UL RTI, Electrical | 50.0 °C @Thickness >=3.00 mm |
122 °F @Thickness >=0.118 in |
|
LG Chemical ALPHALAC SG970NSU HIPS Description: Injection Molding, General Purpose, Good Processability, High gloss, antistatic and UV stabilizedApplication: Air Conditioner Panel, Washer CoverCAS No. 9003-55-8Information provided by.. |
|||
UL RTI, Electrical | 50.0 °C @Thickness >=3.00 mm |
122 °F @Thickness >=0.118 in |
|
LG Chemical GPPS 25SP(I) PS, High Transparency, Heat Resistance Description: Injection Molding, PS, High Transparency, Heat ResistanceApplication: PSP, Food Tray, Electric/Electrical Component, CoatingCAS: 9003-53-6Information provided by LG Chemical |
|||
UL RTI, Electrical | 50.0 °C @Thickness >=1.50 mm |
122 °F @Thickness >=0.0591 in |
|
LG Chemical TR551 MABS, High Transparency, High Rigidity, High Hardness Feature: Injection Molding, High Transparency, High Rigidity, High HardnessApplication: Electric/Electronic Parts Copier, Compact Cases etc.CAS No. 9011-14–7 and 9003-56-9Information provided b.. |
|||
UL RTI, Electrical | 50.0 °C @Thickness 3.00 mm |
122 °F @Thickness 0.118 in |
UL 746B |
DuPont Performance Polymers VESPEL TP-8311 Polyimide Thermoplastic parts from filled PI (polyimide) for balanced mechanical properties and low wear and friction performance in both dry and lubricated high temperature environmentsInformation provided b.. |
|||
UL RTI, Electrical | 50.0 °C @Thickness 0.750 mm |
122 °F @Thickness 0.0295 in |
UL 746B |
DuPont Performance Polymers VESPEL TP-8311 Polyimide Thermoplastic parts from filled PI (polyimide) for balanced mechanical properties and low wear and friction performance in both dry and lubricated high temperature environmentsInformation provided b.. |
|||
UL RTI, Electrical | 50.0 °C @Thickness 1.50 mm |
122 °F @Thickness 0.0591 in |
UL 746B |
DuPont Performance Polymers Hytrel® G3548L TPC-ET
(Unverified Data**) Hytrel® G3548L is a low modulus grade with nominal hardness of 35D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like injec.. |
|||
UL RTI, Electrical | 50.0 °C @Thickness >=1.50 mm |
122 °F @Thickness >=0.0591 in |
|
LG Chemical HIPS MI750 PS, Impact Modified Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica.. |
|||
UL RTI, Electrical | 50.0 °C @Thickness >=6.00 mm |
122 °F @Thickness >=0.236 in |
|
LG Chemical LI912 ASA Description: Good Weatherability, General PurposeApplication: Mail Box, Sprinkler, Sash Joiner, Toy, Satellite Antenna CoverCAS: 26299-47-8Information provided by LG Chemical |
|||
UL RTI, Electrical | 50.0 °C @Thickness >=1.50 mm |
122 °F @Thickness >=0.0591 in |
|
LG Chemical LI923 Extrusion ASA Description: Good Weatherability, High RigidityApplication: Communication Instrument Cover, Cable Connecting Cover, Door PanelCAS: 26299-47-8Information provided by LG Chemical |
|||
UL RTI, Electrical | 50.0 °C @Thickness >=6.00 mm |
122 °F @Thickness >=0.236 in |
|
LG Chemical LI923 Extrusion ASA Description: Good Weatherability, High RigidityApplication: Communication Instrument Cover, Cable Connecting Cover, Door PanelCAS: 26299-47-8Information provided by LG Chemical |