Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glow Wire Test | 650 °C @Thickness 3.00 mm |
1200 °F @Thickness 0.118 in |
STN EN 60695-2-12 |
Plastcom PLASTAMID® 66 GF 30 TS 002 PA66 reinforced with glass fiber, heat stabilized PA66 for injection molding, reinforced with 30 % glass fiber, heat stabilized, used in automotive, engineering and electrical industry, eg. intake pipes, cylinder heads, induction coils, carrying pa.. |
|||
Glow Wire Test | 650 °C | 1200 °F | |
Plastcom SLOVAMID 6 GF 20 PA6, 20% glass beads FeaturesNearly ideal anisotropy of shrinkage in the vertical and in the horizontal direction is established. Manufacturing of exact mouldings. Disadvantage are the relatively low mechanical properti.. |
|||
Glow Wire Test | 650 °C | 1200 °F | STN IEC 60695-2-10 |
Plastcom SLOVAMID 6 GF 60 Polyamide 6, 60% Glass Fiber FeaturesPA 6 for injection moulding, chemically strengthened with 60% of glass fiber, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good.. |
|||
Glow Wire Test | 650 °C | 1200 °F | STN IEC 60695-2-10 |
Plastcom SLOVAMID 6 T 15 Polyamide 6, 15% Micronized Talc FeaturesDecreased shrinkage against the BT types, increased heat application up to 170°C. Increased tensile modulus - strength of the material. PA matrix reduction. Application for tools, fillin.. |
|||
Glow Wire Test | 650 °C | 1200 °F | |
Plastcom SLOVAMID 66 GF 33 PA66, 33% glass fibre FeaturesChemically reinforced with 33% glass fibre, suitable for mouldings with high strength and toughness also at minus temperatures. Used in the automotive, engineering and electrical industry. A.. |
|||
Glow Wire Test | 650 °C @Thickness 3.00 mm |
1200 °F @Thickness 0.118 in |
IEC 60695-2-1 |
Polimeri Europa Sinkral® PD D 232/M4 ABS Resin Special very low gloss extrusion / co-extrusion grade, with good flow.Applications: Sinkral PD D 232/M4 is widely used in extrusion / co-extrusion of foils, when a very high matte appearance is req.. |
|||
Glow Wire Test | 650 °C @Thickness 2.00 mm |
1200 °F @Thickness 0.0787 in |
IEC 695-2-1 |
Polykemi AB POLYblend 6005 PC/ABS-Blend Information provided by Polykemi AB |
|||
Glow Wire Test | 650 °C @Thickness 2.20 mm |
1200 °F @Thickness 0.0866 in |
IEC 695-2-1 |
Polykemi AB POLYfill PP CQX15015 R3 UV Polypropylene, Mineral Reinforced, Scratch Resistant Information provided by Polykemi AB |
|||
Glow Wire Test | 650 °C @Thickness 3.20 mm |
1200 °F @Thickness 0.126 in |
Glow Wire Flammability Index; IEC 60695-2-12 |
SABIC Innovative Plastics Cycoloy® CX1440 PC+ABS (Europe-Africa-Middle East) CYCOLOY CX1440 is a general purpose PC+ABS blend specially developped for thin wall applications requiring weld line strength and high flow with a good balance of propertiesThis data was supplied by.. |
|||
Glow Wire Test | 650 °C @Thickness 3.20 mm |
1200 °F @Thickness 0.126 in |
Glow Wire Flammability Index; IEC 60695-2-12 |
SABIC Innovative Plastics Cycoloy® LG9000 PC+ABS (Europe-Africa-Middle East) CYCOLOY LG9000 is a low gloss PC+ABS injection moulding grade. LG9000 combines good impact / heat and UV resistance with a low gloss surface appearence. It is suitable for automotive interior applic.. |
|||
Glow Wire Test | 650 °C @Thickness 2.00 mm |
1200 °F @Thickness 0.0787 in |
IEC 695-2-1 |
Polykemi AB SCANAMID 66 A13^ F30 Nylon 66, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Glow Wire Test | 650 °C @Thickness 2.00 mm |
1200 °F @Thickness 0.0787 in |
IEC 695-2-1 |
Polykemi AB SCANMID 6 B12^ F50 Nylon 6, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Glow Wire Test | 650 °C @Thickness 3.20 mm |
1200 °F @Thickness 0.126 in |
Glow Wire Flammability Index; IEC 60695-2-12 |
SABIC Innovative Plastics Cycoloy® C1000HF PC+ABS (Europe-Africa-Middle East) CYCOLOY C1000HF is a general purpose PC+ABS blend specially developed for thin wall applications requiring a high flow with a good balance of properties. It is suitable for applications in the autom.. |
|||
Glow Wire Test | 650 °C @Thickness 2.00 mm |
1200 °F @Thickness 0.0787 in |
IEC 695-2-1 |
Polykemi AB SCANMID 6 B22^ E F20 Nylon 6, Glass Fiber Reinforced, Modified Information provided by Polykemi AB |
|||
Glow Wire Test | 650 - 960 °C | 1200 - 1760 °F | Average value: 865 °C Grade Count:7 |
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are incl.. |
|||
Glow Wire Test | 650 °C | 1200 °F | Average value: 650 °C Grade Count:3 |
Overview of materials for Nylon 66, 60% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 60% Glass Fiber Filled". Specific grades with glass content between 55% and 64% are included. .. |
|||
Glow Wire Test | 650 °C | 1200 °F | IEC 695-2-1 |
Lucite International Diakon® ST35G6 Toughened Acrylic Polymer The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness. The grades in the Diakon® series can be processed b.. |
|||
Glow Wire Test | 650 °C | 1200 °F | IEC 695-2-1 |
Lucite International Diakon® TD510 Toughened Acrylic Compound The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness.The grades in the Diakon® series can be processed by.. |
|||
Glow Wire Test | 650 °C | 1200 °F | GWFI; IEC 60695-2-12 |
Ineos ABS Lustran® ABS M406 Lustran® ABS M406 has very high impact strength and increased chemical and dynamic resistance. It is used for the production of molded plastic articles. |
|||
Glow Wire Test | 650 °C @Thickness 1.60 mm |
1200 °F @Thickness 0.0630 in |
ISO 60695-2-12 |
Solvay TECHNYL® B 218 Black 21 N PA66/6, DRY Description: Unreinforced copolyamide PA 66/6 , heat stabilized , medium viscosity, for injection molding.Available in: EuropeProduct Applications: TECHNYL® B 218 offers all of the primary proper.. |
|||
Glow Wire Test | 650 °C @Thickness 1.60 mm |
1200 °F @Thickness 0.0630 in |
ISO 60695-2-12 |
Solvay TECHNYLSTARâ„¢ S 216 V30 PA6, 30% glass filled, DRY Description: TECHNYL STAR TM Polyamide, reinforced with 30% of glass fiber, for injection molding. Characterized by a high fluidity of the melt.Available in: Asia Pacific, Europe and North AmericaPr.. |
|||
Glow Wire Test | 650 °C @Thickness 2.00 mm |
1200 °F @Thickness 0.0787 in |
IEC 60695-2-12 |
SABIC Innovative Plastics LNP THERMOCOMP PF004 PA 6 (Europe-Africa-Middle East) 20% glass fibre reinforced Polyamide 6 injection moulding resin. |
|||
Glow Wire Test | 650 °C | 1200 °F | IE/CEN 60695-2-12 |
Sax Polymers SAXLAC 310T Acrylonitrile Butadiene Styrene Saxalac 310T is an antistatic, high impact resistant ABS injection molding grade, characterized by good processability and high stiffness.Mechanical property data tested at 50% RH.Information provid.. |
|||
Glow Wire Test | 650 °C @Thickness 3.00 mm |
1200 °F @Thickness 0.118 in |
IEC 60695-2-12 |
SABIC Innovative Plastics NORYL PPX PPX830 PPE+PP (Europe-Africa-Middle East) Noryl* PPX830 Polyphenylene Oxide (PPO*) + Polypropylene (PP) resin is a 30 % Glass Reinforced, injection moldable grade with a HDT /1.8MPa temperature resistance of 153 deg C and a Tensile modulus .. |
|||
Glow Wire Test | 650 °C | 1200 °F | GWIT; IEC 60695 |
Polyram PlusTek PA340S8 Nylon 6.6 for Injection Molding, 40% Glass-beads Reinforced 40% Glass-beads reinforced Nylon 6.6 for injection molding applications.Information provided by Polyram. |
|||
Glow Wire Test | 650 °C @Thickness 2.00 mm |
1200 °F @Thickness 0.0787 in |
I.E.C. 695-2-1 |
Cossa Polimeri ESTADIENE 2020 MT Acrylonitrile Butadiene Styrene ABSMedium heat resistance, good impact resistance, good melt flow rate, high gloss, with antistatic, excellent processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Glow Wire Test | 650 °C @Thickness 2.00 mm |
1200 °F @Thickness 0.0787 in |
plaque; IEC 60695 |
Eurotec® Tecomid® NA40 MR15 NL IL PA 6.6 15% mineral reinforced, impact modified Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Glow Wire Test | 650 °C @Thickness 2.00 mm |
1200 °F @Thickness 0.0787 in |
plaque; IEC 60695 |
Eurotec® Tecomid® NB40 GR25 NL PA 6 25% glass fiber reinforced Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Glow Wire Test | 650 °C @Thickness 1.60 mm |
1200 °F @Thickness 0.0630 in |
ICE 60695-12 |
Akro-Plastic Akromid® A3 GF 60 (2424) PA 6.6 Dry, 60% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Glow Wire Test | 650 - 750 °C | 1200 - 1380 °F | Average value: 683 °C Grade Count:3 |
Overview of materials for Polypropylene with 10% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Talc Filler". Specific grades with primary filler content between 5% and 14% are .. |