Thermal Properties | Metric | English | Comments |
---|---|---|---|
Strain Point | 593 °C | 1100 °F | |
Corning 7059 Barium Borosilicate Glass Features a low alkali content of less than 0.3%. In thin sheet form, it is an ideal substrate glass that is also used for low-end LCD applications. Also available crushed/powdered for sealing and o.. |