Thermal Properties | Metric | English | Comments |
---|---|---|---|
Pour Point | 18.0 °C | 64.4 °F | Base Oil; ASTM D97 |
Nye Lubricants PG-44A Grease Information provided by Nye Lubricants. |
|||
Pour Point | 18.0 °C | 64.4 °F | |
Solvay ANTAROX® PLG 254 Surfactant Description: EO.PO block polymer. Multipurpose dispersing agent for suspension concentrate.Chemical Name: ETHYLENE/PROPYLENE OXIDE BLOCK POLYMERSolubility: Soluble in water and most polar solvents. .. |
|||
Pour Point | 18.0 °C | 64.4 °F | |
BASF Pluronic® 17 R4 Block Copolymer Surfactant Description: Pluronic 17R4 is a difunctional block copolymer surfactant with terminal secondary hydroxyl groups. A nonionic surfactant that is 100% active and relatively non-toxic.Information provi.. |
|||
Pour Point | 18.0 °C | 64.4 °F | |
Solvay RHODASURF® B7 Surfactant Description: Ethoxylated alcohol Emulsifier, wetting agent, detergent for lubricants and metal degreasing. APE-Free nonionic emulsifier. The selection of the appropriate balance for specific monomer.. |
|||
Pour Point | 18.0 - 20.0 °C | 64.4 - 68.0 °F | |
Solvay RHODASURF® BC-720 Surfactant Description: Rhodasurf BC-720/E is non ionic low foaming agent for textile, processing and alkaline spray cleaners. Emulsification for Silicones, agricultural chemicals and petroleum oils.Chemical N.. |
|||
Pour Point | 18.0 °C | 64.4 °F | |
Solvay SOPROPHOR® TS/16 Surfactant Description: Multipurpose dispersing agent for SC formulationsIdentification: ETHOXYLATED TRISTYRYLPHENOLCAS: 104376 – 75 – 2Solubility: Soluble in water and most polar and aromatic solvents.Avail.. |