Thermal Properties | Metric | English | Comments |
---|---|---|---|
Pour Point | -73.0 °C | -99.4 °F | Base Oil; ASTM D97 |
Nye Lubricants 741A (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -73.0 °C | -99.4 °F | Base Oil; ASTM D97 |
Nye Lubricants 741B (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -73.0 °C | -99.4 °F | Base Oil; ASTM D97 |
Nye Lubricants 741F (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -73.0 °C | -99.4 °F | Base Oil; ASTM D97 |
Nye Lubricants 741M (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -73.0 °C | -99.4 °F | Base Oil; ASTM D97 |
Nye Lubricants 781A (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -73.0 °C | -99.4 °F | Base Oil; ASTM D97 |
Nye Lubricants 781D (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -73.0 °C | -99.4 °F | Base Oil; ASTM D97 |
Nye Lubricants 781S (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -73.0 °C | -99.4 °F | Base Oil; ASTM D97 |
Nye Lubricants 802-1 (FG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -73.0 °C | -99.4 °F | Base Oil; ASTM D97 |
Nye Lubricants 813-1 (FG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -73.0 °C | -99.4 °F | Base Oil; ASTM D97 |
Nye Lubricants 813S-1 (FG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -73.0 °C | -99.4 °F | ASTM D97 |
ChevronTexaco TEGRA® Synthetic Barrier Fluid Features Chevron Tegra Synthetic Barrier Fluid is formulated to perform as a barrier fluid in dual mechanical seals.Manufactured from the highest quality polyalphaolefin base fluids, it provides pro.. |
|||
Pour Point | -73.0 °C | -99.4 °F | |
3M Fluorinert™ FC-3284 Electronic Liquid 3M™ Fluorinert™ Liquid FC-3284 is a non-conductive, thermally and chemically stable fluid ideal for use in single and two phase heat transfer fluid applications, such as semiconductor package test.. |