Thermal Properties | Metric | English | Comments |
---|---|---|---|
Pour Point | -54.0 °C | -65.2 °F | Base Oil; ASTM D97 |
Nye Lubricants 365 (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -54.0 °C | -65.2 °F | Base Oil; ASTM D97 |
Nye Lubricants 365FT (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -54.0 °C | -65.2 °F | Base Oil; ASTM D97 |
Nye Lubricants 605A (SO) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -54.0 °C | -65.2 °F | Base Oil; ASTM D97 |
Nye Lubricants 605G (SO) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -54.0 °C | -65.2 °F | Base Oil; ASTM D97 |
Nye Lubricants 610B (SO) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -54.0 °C | -65.2 °F | Base Oil; ASTM D97 |
Nye Lubricants 623B (SO) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -54.0 °C | -65.2 °F | Base Oil; ASTM D97 |
Nye Lubricants 723K (RL) Rheolube Grease Information provided by Nye Lubricants. |
|||
Pour Point | -54.0 °C | -65.2 °F | Base Oil; ASTM D97 |
Nye Lubricants 753MS (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -54.0 °C | -65.2 °F | Base Oil; ASTM D97 |
Nye Lubricants 758G (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -54.0 °C | -65.2 °F | Base Oil; ASTM D97 |
Nye Lubricants NPE-UC9 Oil Information provided by Nye Lubricants. |
|||
Pour Point | -54.0 °C | -65.2 °F | Base Oil; ASTM D97 |
Nye Lubricants UniFlor 8122 (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -54.0 °C | -65.2 °F | Base Oil; ASTM D97 |
Nye Lubricants UniFlor 8132 (832) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -54.0 °C | -65.2 °F | Base Oil; ASTM D97 |
Nye Lubricants UniFlor 8132U (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -54.0 °C | -65.2 °F | Base Oil; ASTM D97 |
Nye Lubricants UniFlor 8511 (853-2) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -54.0 °C | -65.2 °F | Base Oil; ASTM D97 |
Nye Lubricants UniFlor 8512-FG (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | <= -54.0 °C | <= -65.2 °F | ASTM D97 |
ExxonMobil 824 Mobil SHC 800 Series Mobil SHC 800 Series turbine oils are designed specifically to meet the needs of the most severe industrial gas turbine applications with a nominal 10,000 hour TOST life. They are recommended for th.. |
|||
Pour Point | <= -54.0 °C | <= -65.2 °F | ASTM D97 |
ExxonMobil Gargoyle Arctic 224 SHC 200 Series Gargoyle Arctic SHC 200 Series are fully synthetic, supreme performance lubricants, specifically designed for use in refrigeration compressors and heat pumps. They are formulated from wax-free, synt.. |
|||
Pour Point | -54.0 °C | -65.2 °F | ASTM D97 |
ExxonMobil Mobil 1 0W-30 Mobil 1 W-30 is an advanced high performance synthetic engine oil designed to provide outstanding wear protection and enhanced fuel economy performance. Mobil 1 0W-30 exceeds the requirements of the.. |
|||
Pour Point | -54.0 °C | -65.2 °F | ASTM D97 |
ExxonMobil Mobil 1 0W-40 Mobil 1 W-40 is the most advanced performance synthetic engine oil designed to provide ultimate cleaning power, wear protection and overall performance. Mobil 1 0W-40, European Car Formula (NA) or P.. |
|||
Pour Point | -54.0 °C | -65.2 °F | ASTM D97 |
ExxonMobil Mobil 1 5W-30 Mobil 1 5W-30 is a high performance fully synthetic engine oil designed to exceed the industry`s toughest standards and outperform all conventional oils.. Mobil 1 5W-30 is engineered to help keep en.. |
|||
Pour Point | -54.0 °C | -65.2 °F | ASTM D97 |
ExxonMobil Mobil 1 5W-30 Truck & SUV Mobil 1 Truck and SUV 5W-30 is a high performance fully synthetic engine oil designed to exceed the industry`s toughest standards and outperform all conventional oils. Mobil 1 Truck and SUV 5W-30 is.. |
|||
Pour Point | -54.0 °C | -65.2 °F | ASTM D97 |
ExxonMobil SAE 40 Mobilgard 1 SHC Mobilgard 1 SHC by ExxonMobil is a supreme performance, synthetic diesel engine oil specifically formulated to address the needs of high power, distillate fueled diesel engines. It provides lubricat.. |
|||
Pour Point | -54.0 °C | -65.2 °F | ASTM D97 |
ChevronTexaco TEGRA® ISO 68 Synthetic Compressor Oil FeaturesChevron Tegra Synthetic Compressor Oils are synthetic compressor lubricants formulated with the highest quality polyalphaolefin (PAO) base fluids.They provide excellent thermal and oxidation.. |
|||
Pour Point | <= -54.0 °C | <= -65.2 °F | ASTM D97 |
ExxonMobil 824 Mobil SHC 800 Series Mobil SHC 800 Series turbine oils are designed specifically to meet the needs of the most severe industrial gas turbine applications with a nominal 10,000 hour TOST life. They are recommended for th.. |
|||
Pour Point | -54.0 °C | -65.2 °F | ASTM D97 |
ExxonMobil Mobil 1 0W-30 Mobil 1 W-30 is an advanced high performance synthetic engine oil designed to provide outstanding wear protection and enhanced fuel economy performance. Mobil 1 0W-30 exceeds the requirements of the.. |
|||
Pour Point | -54.0 °C | -65.2 °F | |
ExxonMobil Mobil 1 10W-40 Motorcycle Oil MX4T 4-Cycle Mobil 1 Motorcycle Oils are formulated with 100 percent synthetic fluids. The unique, synthetic structure of the Mobil 1 Motorcycle formulations enable them to offer advantages well beyond conventio.. |
|||
Pour Point | -54.0 °C | -65.2 °F | ASTM D97 |
ExxonMobil 525 Mobil SHC 500 Series Mobil SHC 500 Series oils are supreme performance hydraulic oils formulated from synthesised, wax-free hydrocarbon base fluids combined with a carefully engineered super-stabilised additive system. .. |
|||
Pour Point | -54.0 °C | -65.2 °F | ASTM D97 |
ExxonMobil Mobil 1 5W-30 Truck & SUV Mobil 1 Truck and SUV 5W-30 is a high performance fully synthetic engine oil designed to exceed the industry`s toughest standards and outperform all conventional oils. Mobil 1 Truck and SUV 5W-30 is.. |
|||
Pour Point | -54.0 °C | -65.2 °F | ASTM D97 |
ExxonMobil 525 Mobil SHC 500 Series Mobil SHC 500 Series oils are supreme performance hydraulic oils formulated from synthesised, wax-free hydrocarbon base fluids combined with a carefully engineered super-stabilised additive system. .. |