Thermal Properties | Metric | English | Comments |
---|---|---|---|
Pour Point | -31.7 °C | -25.0 °F | |
Lubriplate 68 SYN High Temp 100% Ester-Based Multi-Purpose Synthetic Fluid These 100% ester-based synthetic lubricants are recommended for applications that are exposed to high operating temperatures and must maintain a clean lubricated surface. Available in ISO viscosity .. |
|||
Pour Point | -31.7 °C | -25.0 °F | |
Lubriplate AC-1 Petroleum-Based Air Compressor Fluid Formulated to reduce carbon & varnish buildup. They contain fluid zinc to effectively fight friction & wear thus reducing heat & foaming. Available in six ISO grades.AC Series Air Compressor Oils ar.. |
|||
Pour Point | -31.7 °C | -25.0 °F | |
Lubriplate APG 80W-140 Petroleum-Based Gear, Bearing, & Recirculating Oil These heavy-duty, EP (extreme pressure) type oils were developed to meet gear oil needs of most automotive, truck, heavy equipment, and industrial gear boxes requiring an extreme pressure. Meets mil.. |
|||
Pour Point | -31.7 °C | -25.0 °F | |
Lubriplate FMO 200 AW USP Mineral Oil-Based Food Machinery Grade Oil For use where a Class H-1 oil is required. Manufactured in nine ISO grades for a variety of applications. Anti-wear fortified. NOTE: FMO-350AW is also available in a red and orange color which helps.. |
|||
Pour Point | -31.7 °C | -25.0 °F | |
Lubriplate H0-1 Petroleum-Based Heavy-Duty Hydraulic Oil Formulated for superior performance, this series contains fluid zinc to effectively reduce ring & vane wear. Excellent anti-rust, anti-corrosion, anti-foam and anti-oxidation properties. High anilin.. |
|||
Pour Point | -31.7 °C | -25.0 °F | |
Lubriplate SPO-244 Petroleum-Based Gear, Bearing, & Recirculating Oil Petroleum-based oils specifically designed for industrial applications such as gear cases, bearings, chains, machine ways, and general oiling. These tacky lubricants will provide anti-wear lubricati.. |
|||
Pour Point | -31.7 °C | -25.0 °F | |
Lubriplate SPO-MG Petroleum-Based Gear, Bearing, & Recirculating Oil Petroleum-based oils specifically designed for industrial applications such as gear cases, bearings, chains, machine ways, and general oiling. These tacky lubricants will provide anti-wear lubricati.. |
|||
Pour Point | -31.7 °C | -25.0 °F | |
Lubriplate SYNAC 150 Diester-Based Synthetic Air Compressor Fluid These diester-based synthetic air compressor fluids are outstanding for applications where the fluid is subjected to high temperature and high stress conditions over extended drain intervals.Synac S.. |
|||
Pour Point | -31.7 °C | -25.0 °F | |
Lubriplate NO. 3 NO.3 Petroleum-Based Machine Tool Oil Compounded to impart a unique load carrying film, exceptional lubricity, and anti-friction properties not found in conventional oils of the same viscosity. Machine Tool Oils are available in Bottles.. |
|||
Pour Point | -31.7 °C | -25.0 °F | |
Lubriplate NO.3V Petroleum-Based Machine Tool Oil Compounded to impart a unique load carrying film, exceptional lubricity, and anti-friction properties not found in conventional oils of the same viscosity. Machine Tool Oils are available in Bottles.. |
|||
Pour Point | -31.7 °C | -25.0 °F | |
ConocoPhillips Syncon® 80W-140 HP Synthetic Gear Oil Description: Conoco Syncon HP Synthetic Gear Oil is recommended for conventional and limited-slip differentials, as well as some manual transmissions commonly found in passenger cars, race cars, tru.. |
|||
Pour Point | -31.7 °C | -25.0 °F | |
ConocoPhillips 100 Super Hydraulic Oil Description: Conoco Super Hydraulic Oil is a high-quality antiwear hydraulic fluid formulated from premium Conoco hydrocracked base stocks to provide superior water separation, antiwear protection, .. |
|||
Pour Point | -31.7 °C | -25.0 °F | |
ConocoPhillips 100 Ultra-Clean Super Hydraulic Oil Description: Conoco Ultra-Clean Super Hydraulic Oils have the same high performance characteristics of regular Super Hydraulic Oils with the added advantage of a guaranteed ISO cleanliness code of 1.. |
|||
Pour Point | -31.7 °C | -25.0 °F | |
ConocoPhillips Hydroclear® 100 Rock Oil Description: Conoco Hydroclear Rock Drill Oil is a high-quality, heavy-duty, extreme-pressure pneumatic tool lubricant formulated from premium Conoco hydrocracked base stocks. Hydroclear Rock Drill .. |
|||
Pour Point | -31.7 °C | -25.0 °F | |
ConocoPhillips 32 Spectrum Cutting Oil Description: Conoco Spectrum Cutting Oil is a multifunctional cutting fluid formulated with a sulfurized base oil, is a balanced additive system and is suited for a wide variety of machining applica.. |
|||
Pour Point | -31.7 °C | -25.0 °F | |
ConocoPhillips 100 Gear Oil AGMA Lubricant No. 3 EP Description: Conoco Gear Oil is a heavy-duty extreme-pressure industrial gear lubricant formulated from high-quality hydrocracked base stocks to provide excellent oxidation inhibition, EP load-carry.. |