Thermal Properties | Metric | English | Comments |
---|---|---|---|
Pour Point | -29.0 °C | -20.2 °F | Base Oil; ASTM D97 |
Nye Lubricants 174 (SO) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -29.0 °C | -20.2 °F | Base Oil; ASTM D97 |
Nye Lubricants 174A (SO) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -29.0 °C | -20.2 °F | Base Oil; ASTM D97 |
Nye Lubricants 444 (SO) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -29.0 °C | -20.2 °F | Base Oil; ASTM D97 |
Nye Lubricants 502AU (NT) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -29.0 °C | -20.2 °F | Base Oil; ASTM D97 |
Nye Lubricants 502J-20-UV (NT) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -29.0 °C | -20.2 °F | Base Oil; ASTM D97 |
Nye Lubricants 502J-65-UV (NT) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -29.0 °C | -20.2 °F | Base Oil; ASTM D97 |
Nye Lubricants 502UV (NT) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -29.0 °C | -20.2 °F | Base Oil; ASTM D97 |
Nye Lubricants 782D (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -29.0 °C | -20.2 °F | Base Oil; ASTM D97 |
Nye Lubricants 782DL (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -29.0 °C | -20.2 °F | Base Oil; ASTM D97 |
Nye Lubricants UniFlor 8180 (479) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -29.0 °C | -20.2 °F | Base Oil; ASTM D97 |
Nye Lubricants UniFlor 8182 (837) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -29.0 °C | -20.2 °F | Base Oil; ASTM D97 |
Nye Lubricants UniFlor 8182R (837RP) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -29.0 °C | -20.2 °F | |
Teknor Apex TruVis Esters™ TTDTM Tri-Tridecyl Trimellitate |
|||
Pour Point | -29.0 °C | -20.2 °F | ASTM D97 |
ChevronTexaco Aero 20W-50 Engine Oil AD FeaturesChevron Aero Engine Oils AD are premium quality ashless dispersant oils for four-stroke aircraft piston engines.Chevron Aero Engine Oils AD are blended with high quality, high viscosity ind.. |
|||
Pour Point | -29.0 °C | -20.2 °F | ASTM D97 |
ChevronTexaco ECO® SAE 15W-40 Heavy Duty Motor Oil Features:Chevron ECO Heavy Duty Motor Oils are formulated to be environmentally responsible engine lubricants. They use the highest quality re-refined base oils and specially selected additives desi.. |
|||
Pour Point | -29.0 °C | -20.2 °F | ASTM D97 |
ChevronTexaco Supreme SAE 20W-50 Motor Oil FeaturesChevron Supreme Motor Oils are premium quality automotive engine oils.Chevron Supreme Motor Oils SAE 5W-20, 5W-30, 10W-30, 10W-40, and 20W-50 are formulated with ISO-SYN™ base stocks, a she.. |
|||
Pour Point | -29.0 °C | -20.2 °F | |
ChevronTexaco Capella® WF 100 Texaco Capella WF oils delivers value through:Wax-free — Suitable for ultra-low temperature service.Water-free — Low moisture content prevents icing in refrigeration expansion valves and helps pre.. |
|||
Pour Point | -29.0 °C | -20.2 °F | Base Oil; ASTM D97 |
Nye Lubricants 502M-20-UV (NT) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -29.0 °C | -20.2 °F | Base Oil; ASTM D97 |
Nye Lubricants 782D-G4 (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -29.0 °C | -20.2 °F | ASTM D97, ISO 3016 |
Chesterton 651 Detergent Lubricating Oil Description: Chesterton® 651 Detergent Lubricating Oil is the plant-wide product of choice for superior-quality, low-viscosity, industrial lubricating needs. It is a cost-effective oil with high de.. |
|||
Pour Point | -29.0 °C | -20.2 °F | |
ChevronTexaco Havoline® SAE 20W-50 Motor Oil All grades of Havoline Motor Oils are formulated with high quality base stocks, a shear-stable viscosity index improver, and contain detergent, dispersant, wear control, antioxidant, corrosion inhib.. |