Thermal Properties | Metric | English | Comments |
---|---|---|---|
Pour Point | -24.0 °C | -11.2 °F | Base Oil; ASTM D97 |
Nye Lubricants 774H (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -24.0 °C | -11.2 °F | Base Oil; ASTM D97 |
Nye Lubricants 868H (FG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -24.0 °C | -11.2 °F | Base Oil; ASTM D97 |
Nye Lubricants 868H-MS (FG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -24.0 °C | -11.2 °F | ASTM D97 |
ExxonMobil 20W-50 Exxon Aviation Oil Aviation Oil 100, 120 and 20W-50 are non-dispersant, mineral oil-based lubricants for piston engines of commercial, military and private aircraft. They contain very low concentrations of anti-oxid.. |
|||
Pour Point | -24.0 °C | -11.2 °F | ASTM D97 |
ExxonMobil 630 Mobilgear 600 Series The Mobilgear 600 Series are extra high performance gear oils having outstanding extreme pressure characteristics and load-carrying properties, intended for use in all types of enclosed gear drives .. |
|||
Pour Point | -24.0 °C | -11.2 °F | |
ExxonMobil Diol 17 RD 2040 DIOL railroad oils are a full line of heavy-duty crankcase lubricants for locomotive diesel engines. These products are designed to meet the severe service demands imposed by newer railroad diesel l.. |
|||
Pour Point | -24.0 °C | -11.2 °F | ASTM D97 |
ExxonMobil Enmist EP 100 Esso ENMIST EP is a family of premium quality industrial lubricants designed for the oil-fog or mist-lubrication of machine components such as slideways, bearings, gears, chains etc. ENMIST EP mist .. |
|||
Pour Point | -24.0 °C | -11.2 °F | ASTM D97 |
ExxonMobil Mobil Almo 529 Mobil Almo 500 Series lubricants are premium quality high performance products primarily intended for the lubrication of pneumatically operated rock drills in underground and surface mining operatio.. |
|||
Pour Point | <= -24.0 °C | <= -11.2 °F | ASTM D97 |
ExxonMobil Mobilarma 522 Mobilarma 500 Series oils are premium performance products primarily intended as run-in or lay-up lubricants, which provide effective rust preventive films on the internal surfaces of machinery. The.. |
|||
Pour Point | -24.0 °C | -11.2 °F | ASTM D97 |
ExxonMobil Nuto 32 H Series Exxon Nuto H Series oils are premium quality anti-wear hydraulic oils intended for industrial and mobile service applications where anti-wear lubricants are required. They are formulated with high q.. |
|||
Pour Point | -24.0 °C | -11.2 °F | |
ChevronTexaco 120 Aircraft Engine Oils Premium AD Texaco Aircraft Engine Oils Premium AD deliver value through:Clean engines due to the dispersancy action. Minimal deposits in the combustion chamber, spark plugs, rings, valves, etc.Low wear — Maxi.. |
|||
Pour Point | -24.0 °C | -11.2 °F | |
ChevronTexaco Aquagear® EP 220 Texaco Aquagear EP oils deliver value through:Long equipment life — Effective sulfur-phosphorus extreme-pressure additives provide high film thickness that protects gear teeth from wear and prematu.. |
|||
Pour Point | -24.0 °C | -11.2 °F | |
ChevronTexaco Aries® 150 Texaco Aries lubricants deliver value through:Long equipment life — Extreme pressure performance withstands heavy shock loads typical of rock drill service, protecting the equipment against rapid w.. |
|||
Pour Point | -24.0 °C | -11.2 °F | ASTM D97 |
ChevronTexaco Drive Train Fluid HD, SAE 30 FeaturesChevron Drive Train Fluids HD are high performance lubricants designed for use in transmissions, final drives, and hydraulic systems requiring a fluid meeting Caterpillar TO-4 or Allison C4 .. |
|||
Pour Point | -24.0 °C | -11.2 °F | ASTM D97 |
ChevronTexaco Elite-Cut® NM Metal Working Fluid FeaturesChevron -Cut Metalworking Fluids are a complete line of chlorinated cutting oils. The line consists of individual products with antiweld and lubricity properties to cover practically all met.. |
|||
Pour Point | -24.0 °C | -11.2 °F | ASTM D97 |
ChevronTexaco Gear Compounds EP J, ISO 220 FeaturesChevron Gear Compounds EP J are multipurpose gear lubricants.They are formulated with highly refined, high viscosity
index paraffinic base oils and a new generation sulfurphosphorus additive.. |
|||
Pour Point | -24.0 °C | -11.2 °F | |
ChevronTexaco Geotex® Ashless SAE 30 Texaco Geotex Ashless oils deliver value through:Low maintenance cost and long engine lifeNo ash deposits — Eliminates spark plug fouling due to lubricating oil ash deposits. Minimizes deposits on .. |
|||
Pour Point | -24.0 °C | -11.2 °F | ASTM D97 |
ChevronTexaco HPLX SAE 30 Chevron HPLX Low Ash Gas Engine Oil FeaturesChevron HPLX Low Ash Gas Engine Oils are high quality, bright stock-free, low ash, dispersant/detergent type engine oils.They are formulated with ISOSYN™ base stocks and an additive package.. |
|||
Pour Point | -24.0 °C | -11.2 °F | ASTM D97 |
ChevronTexaco ISO 100 AIO FeaturesChevron AIO (Chevron Authentic Industrial Oils) provide rust protection, oxidation inhibition, and foam suppression.Chevron AIO are good quality lubricants for any application not requiring .. |
|||
Pour Point | -24.0 °C | -11.2 °F | ASTM D97 |
ChevronTexaco ISO 150 Red Chain Bar Oil FeaturesChevron Red Chain Bar Oils are very tacky, tough, lubricants made from special high viscosity base oils having the desired flow and pumpability properties to assure adequate lubrication over.. |
|||
Pour Point | -24.0 °C | -11.2 °F | ASTM D97 |
ChevronTexaco Regal® 100 R&O Texaco Regal R&O oils deliver value through:Prolonged oil service life — Excellent oxidation stability provided by the multi-component inhibitor system resists oil breakdown during exposure to high.. |
|||
Pour Point | -24.0 °C | -11.2 °F | ASTM D97 |
ChevronTexaco Vistac® ISO 100 Rock Drill Oil FeaturesChevron Rock Drill Oils Vistac are designed to give maximum protection to percussion rock drills.They are formulated from highly refined, high viscosity index, paraffinic base stocks and add.. |
|||
Pour Point | -24.0 °C | -11.2 °F | ASTM D97 |
ChevronTexaco Vistac® ISO 46 Rock Drill Oil FeaturesChevron Rock Drill Oils Vistac are designed to give maximum protection to percussion rock drills.They are formulated from highly refined, high viscosity index, paraffinic base stocks and add.. |
|||
Pour Point | -24.0 °C | -11.2 °F | ASTM D97 |
ExxonMobil 630 Mobilgear 600 Series The Mobilgear 600 Series are extra high performance gear oils having outstanding extreme pressure characteristics and load-carrying properties, intended for use in all types of enclosed gear drives .. |
|||
Pour Point | <= -24.0 °C | <= -11.2 °F | ASTM D97 |
ExxonMobil Mobilarma 522 Mobilarma 500 Series oils are premium performance products primarily intended as run-in or lay-up lubricants, which provide effective rust preventive films on the internal surfaces of machinery. The.. |
|||
Pour Point | -24.0 °C | -11.2 °F | ASTM D97 |
ExxonMobil Spartan EP 220 Exxon SPARTAN EP lubricants are a family of premium quality extreme pressure gear lubricants. They are formulated with high quality mineral oils, which help reduce sludge formation and oil thickenin.. |
|||
Pour Point | -24.0 °C | -11.2 °F | ASTM D97 |
ChevronTexaco Dura-Lith® NLGI 00 Grease EP FeaturesChevron Dura-Lith Greases EP are multipurpose extreme pressure greases.They are manufactured using selected highly refined medium viscosity index base oils, a lithium 12-hydroxystearate thic.. |
|||
Pour Point | -24.0 °C | -11.2 °F | |
ChevronTexaco Summer Chain Bar Oil Texaco Chain Bar Oil Summer Grade delivers value through:Reduced wear — Minimize wear for the chain, bar, and sprocket.Tackiness — The increased tackiness additive keeps the oil on the chain and p.. |
|||
Pour Point | -24.0 °C | -11.2 °F | ASTM D97 |
ExxonMobil Nuto 46 H Series Exxon Nuto H Series oils are premium quality anti-wear hydraulic oils intended for industrial and mobile service applications where anti-wear lubricants are required. They are formulated with high q.. |
|||
Pour Point | -24.0 °C | -11.2 °F | |
ChevronTexaco SAE 30 Transmission and Drive Train TO-4 Oil Texaco Transmission and Drive Train TO-4 Oils deliver value through:Longer equipment life — Special additives protect metal surfaces against scuffing and wear even under severe operating conditions.. |