Thermal Properties | Metric | English | Comments |
---|---|---|---|
Pour Point | -18.0 °C | -0.400 °F | Base Oil; ASTM D97 |
Nye Lubricants 835D (FG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -18.0 °C | -0.400 °F | Base Oil; ASTM D97 |
Nye Lubricants 875MS-G0 (FG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -18.0 °C | -0.400 °F | Base Oil; ASTM D97 |
Nye Lubricants 875R (FG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -18.0 °C | -0.400 °F | ASTM D97 |
ExxonMobil 1500 Mobilgear SHC Series The Mobilgear SHC Series lubricants are heavy-duty gear oils primarily designed for all kinds of enclosed gearing as well as plain and rolling element bearings. They are formulated from wax-free pol.. |
|||
Pour Point | -18.0 °C | -0.400 °F | ASTM D97 |
ExxonMobil 632 Mobilgear 600 Series The Mobilgear 600 Series are extra high performance gear oils having outstanding extreme pressure characteristics and load-carrying properties, intended for use in all types of enclosed gear drives .. |
|||
Pour Point | -18.0 °C | -0.400 °F | ASTM D97 |
ExxonMobil Light Mobil DTE Oil Named Series The Mobil DTE Oil Named Series of lubricants are premium performance circulating lubricants designed for applications including steam and hydro turbine sets and other systems where long lubricant se.. |
|||
Pour Point | -18.0 °C | -0.400 °F | ASTM D97 |
ExxonMobil Mobil Delvac 50 1650 Mobil Delvac 1630, 1640, and 1650 are high performance monograde diesel engine oils formulated from advanced technology base oils and a balanced additive system. They are specifically engineered f.. |
|||
Pour Point | <= -18.0 °C | <= -0.400 °F | |
ExxonMobil Mobilarma 524 Mobilarma 500 Series oils are premium performance products primarily intended as run-in or lay-up lubricants, which provide effective rust preventive films on the internal surfaces of machinery. The.. |
|||
Pour Point | -18.0 °C | -0.400 °F | ASTM D97 |
ExxonMobil Mobil Vaculine 533 Mobil Vacuoline 500 Series are extra high performance heavy duty circulating oils specifically designed to meet the critical requirements of the Morgan Construction Companys high speed No-Twist® Ro.. |
|||
Pour Point | -18.0 °C | -0.400 °F | ASTM D97 |
ChevronTexaco Delo® 477 CFO Marine Engine Oil, SAE 40 FeaturesChevron Marine Engine Oils Delo 477 CFO are superior high dispersancy, high alkalinity, 17 base Number engine oils.They are manufactured using the highest quality paraffinic base oils, a non.. |
|||
Pour Point | -18.0 °C | -0.400 °F | ASTM D97 |
ChevronTexaco Dura-Lith® NLGI 1 Grease EP FeaturesChevron Dura-Lith Greases EP are multipurpose extreme pressure greases.They are manufactured using selected highly refined medium viscosity index base oils, a lithium 12-hydroxystearate thic.. |
|||
Pour Point | -18.0 °C | -0.400 °F | ASTM D97 |
ChevronTexaco Dura-Lith® NLGI 3 Grease EP FeaturesChevron Dura-Lith Greases EP are multipurpose extreme pressure greases.They are manufactured using selected highly refined medium viscosity index base oils, a lithium 12-hydroxystearate thic.. |
|||
Pour Point | -18.0 °C | -0.400 °F | ASTM D97 |
ChevronTexaco Gear Compounds EP J, ISO 320 FeaturesChevron Gear Compounds EP J are multipurpose gear lubricants.They are formulated with highly refined, high viscosity
index paraffinic base oils and a new generation sulfurphosphorus additive.. |
|||
Pour Point | -18.0 °C | -0.400 °F | ASTM D97 |
ChevronTexaco HDAX® SAE 40 LFG Gas Engine Oil FeaturesChevron HDAX LFG Gas Engine Oil is a premium quality, medium ash, dispersant/detergent type gas engine oil formulated especially for landfill gas and sour gas application.It is formulated wi.. |
|||
Pour Point | -18.0 °C | -0.400 °F | ASTM D97 |
ChevronTexaco ISO 220 Marine Oil E FeaturesChevron Marine Oils E are formulated using a blend of high grade, medium viscosity index base oils and carefully balanced additive package to meet the crankcase need of marine steam engines... |
|||
Pour Point | -18.0 °C | -0.400 °F | ASTM D97 |
ChevronTexaco NLGI 2 Moly Grease EP FeaturesChevron Moly Greases EP are general purpose, extreme pressure (EP) greases. They are manufactured using highly refined selected base oils, a lithium-12-hydroxystearate thickener, 3% molybden.. |
|||
Pour Point | -18.0 °C | -0.400 °F | |
ChevronTexaco Taro® 20 DP SAE 40 Texaco Taro 20 DP delivers value through:Wear protection — Performance results in the latest design medium speed trunk piston diesel engines have shown that the high level of alkalinity of this lub.. |
|||
Pour Point | -18.0 °C | -0.400 °F | |
ChevronTexaco Taro® 30 DP SAE 30 Texaco Taro 30 DP delivers value through:Wear protection — Performance results in the latest design medium speed trunk piston diesel engines have shown that the high level of alkalinity of this lub.. |
|||
Pour Point | -18.0 °C | -0.400 °F | |
ChevronTexaco Taro® 30 DP SAE 40 Texaco Taro 30 DP delivers value through:Wear protection — Performance results in the latest design medium speed trunk piston diesel engines have shown that the high level of alkalinity of this lub.. |
|||
Pour Point | -18.0 °C | -0.400 °F | |
ChevronTexaco Texmar ZF 17 SAE 40 Texaco Texmar 17 deliver value through:Ability to maximize oil and filter lifeImproved wear controlExtended drainsExtends oil drains in new low oil consumption GE locomotives, reducing oil costsBett.. |
|||
Pour Point | -18.0 °C | -0.400 °F | ASTM D97 |
ChevronTexaco Vistac® ISO 32 Way Oil D FeaturesChevron Way Oils Vistac D are high quality lubricants designed to meet the critical lubrication demands for the slides and ways of machine tools.Chevron Way Oils Vistac D is formulated with .. |
|||
Pour Point | -18.0 °C | -0.400 °F | ASTM D97 |
ExxonMobil 100 Mobil DTE FM Series Mobil DTE FM Series oils are high performance lubricants designed to satisfy a wide range of multi-use equipment requirements for the food processing and packaging industry. These lubricants are qua.. |
|||
Pour Point | -18.0 °C | -0.400 °F | ASTM D97 |
ExxonMobil 30 Mobiltrans HD Mobiltrans HD 10W, 30, 50, and 60 are extra high performance transmission and drive-train lubricants engineered to meet the rigorous specifications required by Caterpillar TO-4. This product line .. |
|||
Pour Point | -18.0 °C | -0.400 °F | ASTM D97 |
ExxonMobil HD Plus 85W-140 Mobilube HD Plus 80W-90 and 85W-140 are extra high performance commercial gear lubricants formulated from select base oils and an advanced additive system. These lubricants are engineered for perfor.. |
|||
Pour Point | -18.0 °C | -0.400 °F | ASTM D97 |
ExxonMobil Light Mobil DTE Oil Named Series The Mobil DTE Oil Named Series of lubricants are premium performance circulating lubricants designed for applications including steam and hydro turbine sets and other systems where long lubricant se.. |
|||
Pour Point | -18.0 °C | -0.400 °F | ASTM D97 |
ExxonMobil Mobil Delvac 50 1650 Mobil Delvac 1630, 1640, and 1650 are high performance monograde diesel engine oils formulated from advanced technology base oils and a balanced additive system. They are specifically engineered f.. |
|||
Pour Point | -18.0 °C | -0.400 °F | ASTM D97 |
ExxonMobil Mobil Vaculine 533 Mobil Vacuoline 500 Series are extra high performance heavy duty circulating oils specifically designed to meet the critical requirements of the Morgan Construction Companys high speed No-Twist® Ro.. |
|||
Pour Point | -18.0 °C | -0.400 °F | ASTM D97 |
ExxonMobil Spartan EP 320 Exxon SPARTAN EP lubricants are a family of premium quality extreme pressure gear lubricants. They are formulated with high quality mineral oils, which help reduce sludge formation and oil thickenin.. |
|||
Pour Point | -18.0 °C | -0.400 °F | |
ChevronTexaco Aquagear® EP 460 Texaco Aquagear EP oils deliver value through:Long equipment life — Effective sulfur-phosphorus extreme-pressure additives provide high film thickness that protects gear teeth from wear and prematu.. |
|||
Pour Point | -18.0 °C | -0.400 °F | ASTM D97 |
ExxonMobil 30 Mobiltrans HD Mobiltrans HD 10W, 30, 50, and 60 are extra high performance transmission and drive-train lubricants engineered to meet the rigorous specifications required by Caterpillar TO-4. This product line .. |