Thermal Properties | Metric | English | Comments |
---|---|---|---|
Pour Point | 10.0 °C | 50.0 °F | Base Oil; ASTM D97 |
Nye Lubricants 439 (SO) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | 10.0 °C | 50.0 °F | Base Oil; ASTM D97 |
Nye Lubricants 520C-2 (NT) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | 10.0 °C | 50.0 °F | Base Oil; ASTM D97 |
Nye Lubricants 520M-2 (NT) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | 10.0 °C | 50.0 °F | Base Oil; ASTM D97 |
Nye Lubricants 520M-2-UV (NT) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | 10.0 °C | 50.0 °F | Base Oil; ASTM D97 |
Nye Lubricants 523V-2-UV (NT) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | 10.0 °C | 50.0 °F | |
Solvay ALKAMULS® EL 620 LI E Surfactant Description: Biodegradable castor oil ethoxylate emulsifier, solubiliser for a wide range of formulations with an HLB of around 12.Identification: CASTOR OIL ETHOXYLATE (30)CAS: 61791 – 12 â€.. |
|||
Pour Point | 10.0 °C | 50.0 °F | |
Solvay ALKAMULS® EL 719 E Surfactant Identification: ETHOXYLATED CASTOR OILCAS: 61791 – 12 – 6Solubility: Soluble in water and most polar and aromatic solvents.Available in: Asia Pacific, Europe, Latin America and North Ameri.. |
|||
Pour Point | 10.0 °C | 50.0 °F | ASTM D97 |
ChevronTexaco 800 NC Open Gear Lubricant FeaturesChevron Open Gear Lubricants are black, viscous lubricants formulated with an asphaltic base and diluted with a nonchlorinated solvent for easy application by hand or through automatic lubri.. |
|||
Pour Point | 10.0 °C | 50.0 °F | |
ChevronTexaco Sugartex® Heavy Texaco Sugartex delivers value through:Reliability — High lubricant film strength withstands heavy shock loads and provides protection under boundary lubrication to minimize wear rate and prevent f.. |
|||
Pour Point | 10.0 °C | 50.0 °F | |
ConocoPhillips Inca® 1000 Oil, AGMA No. 8A Comp. Description: Conoco Inca Oil is a high-quality compounded lubricant recommended for use in heavily loaded industrial and automotive worm gears and bearings operating at moderate to high temperatures.. |
|||
Pour Point | 10.0 °C | 50.0 °F | |
ChevronTexaco Sugartex® Texaco Sugartex delivers value through:Reliability — High lubricant film strength withstands heavy shock loads and provides protection under boundary lubrication to minimize wear rate and prevent f.. |
|||
Pour Point | 10.0 °C | 50.0 °F | |
Solvay LUBRHOPHOS® RD 510 E Surfactant Identification: POLYOXYETHYLENE LAURYL ETHER PHOSPHATECAS: 39464 – 66 – 9Solubility: Dispersible in water. Soluble in most polar and aromatic solvents.Available in: Asia Pacific, Europe, Latin Ame.. |
|||
Pour Point | 10.0 °C | 50.0 °F | |
Solvay RHODASURF® CET 5 Surfactant Identification: ETHOXYLATED OLEYL CETYL ALCOHOLCAS: 68920 – 66 – 1Solubility: Dispersible in water. Soluble in most polar and aromatic solvents.Available in: Asia Pacific, Europe, Latin America an.. |