Thermal Properties | Metric | English | Comments |
---|---|---|---|
Pour Point | -85.0 °C | -121 °F | Base Oil; ASTM D97 |
Nye Lubricants UniFlor 8900 (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -85.0 °C | -121 °F | Base Oil; ASTM D97 |
Nye Lubricants UniFlor 8901 (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -85.0 °C | -121 °F | Base Oil; ASTM D97 |
Nye Lubricants UniFlor 8960 (498A) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -85.0 °C | -121 °F | Base Oil; ASTM D97 |
Nye Lubricants UniFlor 8961 (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -85.0 °C | -121 °F | Base Oil; ASTM D97 |
Nye Lubricants UniFlor 8961F (896-1) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -85.0 °C | -121 °F | Base Oil; ASTM D97 |
Nye Lubricants UniFlor 8961R (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -85.0 °C | -121 °F | Base Oil; ASTM D97 |
Nye Lubricants UniFlor 8961UF (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -85.0 °C | -121 °F | ASTM D97 |
Solvay Specialty Polymers FOMBLIN® M03 PFPE Lubricant Information provided by Solvay Solexis, Inc. |
|||
Pour Point | -85.0 °C | -121 °F | |
Solvay Specialty Polymers Galden® D03 PFPE Fluid Galden® D grades are specifically recommended for electronic reliability testing, including thermal shock and hermetic seal testing.Galden® PFPE is a line of high-performance, inert, fluorinat.. |
|||
Pour Point | <= -85.0 °C | <= -121 °F | |
Solvay Specialty Polymers Galden® HT200 PFPE Heat Transfer Fluid Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service.. |
|||
Pour Point | -85.0 °C | -121 °F | |
Dow Corning 1248 Fluid Silicone glycol graft copolymer with secondary hydroxyl functionality. The polymer has a combination of organoreactivity from the glycol group as well as properties typical of a polydimethylsiloxane.. |