Thermal Properties | Metric | English | Comments |
---|---|---|---|
Pour Point | -54.0 °C | -65.2 °F | Base Oil; ASTM D97 |
Nye Lubricants 365 (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -54.0 °C | -65.2 °F | Base Oil; ASTM D97 |
Nye Lubricants 365F (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -54.0 °C | -65.2 °F | Base Oil; ASTM D97 |
Nye Lubricants 622C (SO) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -54.0 °C | -65.2 °F | Base Oil; ASTM D97 |
Nye Lubricants 753MS (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -54.0 °C | -65.2 °F | Base Oil; ASTM D97 |
Nye Lubricants 758G (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -54.0 °C | -65.2 °F | Base Oil; ASTM D97 |
Nye Lubricants 789D (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -54.0 °C | -65.2 °F | Base Oil; ASTM D97 |
Nye Lubricants 789M (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -54.0 °C | -65.2 °F | Base Oil; ASTM D97 |
Nye Lubricants UniFlor 8130 (475) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -54.0 °C | -65.2 °F | Base Oil; ASTM D97 |
Nye Lubricants UniFlor 8132 (832) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -54.0 °C | -65.2 °F | Base Oil; ASTM D97 |
Nye Lubricants UniFlor 8132U (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -54.0 °C | -65.2 °F | Base Oil; ASTM D97 |
Nye Lubricants UniFlor 8512F (842G0) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -54.0 °C | -65.2 °F | Base Oil; ASTM D97 |
Nye Lubricants UniFlor 8512G (842G) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -54.0 °C | -65.2 °F | Base Oil; ASTM D97 |
Nye Lubricants UniFlor 8512S (842S) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -54.0 °C | -65.2 °F | Base Oil; ASTM D97 |
Nye Lubricants UniFlor 8512SC (842S-CP) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | <= -54.0 °C | <= -65.2 °F | ASTM D97 |
ExxonMobil 824 Mobil SHC 800 Series Mobil SHC 800 Series turbine oils are designed specifically to meet the needs of the most severe industrial gas turbine applications with a nominal 10,000 hour TOST life. They are recommended for th.. |
|||
Pour Point | -54.0 °C | -65.2 °F | ASTM D97 |
ExxonMobil Mobil 1 0W-40 Mobil 1 W-40 is the most advanced performance synthetic engine oil designed to provide ultimate cleaning power, wear protection and overall performance. Mobil 1 0W-40, European Car Formula (NA) or P.. |
|||
Pour Point | -54.0 °C | -65.2 °F | |
ExxonMobil Mobil 1 10W-40 Motorcycle Oil MX4T 4-Cycle Mobil 1 Motorcycle Oils are formulated with 100 percent synthetic fluids. The unique, synthetic structure of the Mobil 1 Motorcycle formulations enable them to offer advantages well beyond conventio.. |
|||
Pour Point | -54.0 °C | -65.2 °F | ASTM D97 |
ExxonMobil Mobil 1 5W-30 Mobil 1 5W-30 is a high performance fully synthetic engine oil designed to exceed the industry`s toughest standards and outperform all conventional oils.. Mobil 1 5W-30 is engineered to help keep en.. |
|||
Pour Point | -54.0 °C | -65.2 °F | ASTM D97 |
ExxonMobil Mobil 1 5W-30 Truck & SUV Mobil 1 Truck and SUV 5W-30 is a high performance fully synthetic engine oil designed to exceed the industry`s toughest standards and outperform all conventional oils. Mobil 1 Truck and SUV 5W-30 is.. |
|||
Pour Point | -54.0 °C | -65.2 °F | ASTM D97 |
ExxonMobil Mobil 1 Synthetic ATF Mobil 1 Synthetic ATF is a multi-vehicle, fully synthetic fluid designed to meet the demanding requirements of modern passenger vehicles.Mobil 1 Synthetic ATF is a multi-vehicle formula recommended .. |
|||
Pour Point | -54.0 °C | -65.2 °F | |
ChevronTexaco Rando® HDZ 15 Texaco Rando HDZ oils deliver value through:High oxidation stability — Longer service life than attainable with conventional lubricants used in high pressure service.Protection against rust and cor.. |
|||
Pour Point | -54.0 °C | -65.2 °F | ASTM D97 |
ChevronTexaco Rykon® ISO 15 Premium Oil FeaturesChevron Rykon Premium Oils are designed to give maximum protection to hydraulic pumps.They are formulated with ISOSYN® base stocks incorporating antiwear additives, oxidation and corrosion .. |
|||
Pour Point | -54.0 °C | -65.2 °F | ASTM D97 |
ChevronTexaco TEGRA® ISO 100 Synthetic Compressor Oil FeaturesChevron Tegra Synthetic Compressor Oils are synthetic compressor lubricants formulated with the highest quality polyalphaolefin (PAO) base fluids.They provide excellent thermal and oxidation.. |
|||
Pour Point | -54.0 °C | -65.2 °F | ASTM D97 |
ExxonMobil 624 Mobil SHC 600 Series Mobil SHC 600 Series lubricants are good performance gear and bearing oils designed to provide outstanding service in terms of equipment protection, oil life and problem-free operation. They are for.. |
|||
Pour Point | -54.0 °C | -65.2 °F | |
ExxonMobil Mobil 1 10W-40 Motorcycle Oil MX4T 4-Cycle Mobil 1 Motorcycle Oils are formulated with 100 percent synthetic fluids. The unique, synthetic structure of the Mobil 1 Motorcycle formulations enable them to offer advantages well beyond conventio.. |
|||
Pour Point | -54.0 °C | -65.2 °F | ASTM D97 |
ExxonMobil SAE 40 Mobilgard 1 SHC Mobilgard 1 SHC by ExxonMobil is a supreme performance, synthetic diesel engine oil specifically formulated to address the needs of high power, distillate fueled diesel engines. It provides lubricat.. |
|||
Pour Point | -54.0 °C | -65.2 °F | Base Oil; ASTM D97 |
Nye Lubricants 608 (SO) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -54.0 °C | -65.2 °F | ASTM D97 |
ExxonMobil Mobil 1 5W-30 Mobil 1 5W-30 is a high performance fully synthetic engine oil designed to exceed the industry`s toughest standards and outperform all conventional oils.. Mobil 1 5W-30 is engineered to help keep en.. |
|||
Pour Point | -54.0 °C | -65.2 °F | ASTM D97 |
ExxonMobil Mobil 1 5W-30 Truck & SUV Mobil 1 Truck and SUV 5W-30 is a high performance fully synthetic engine oil designed to exceed the industry`s toughest standards and outperform all conventional oils. Mobil 1 Truck and SUV 5W-30 is.. |
|||
Pour Point | -54.0 °C | -65.2 °F | ASTM D97 |
ExxonMobil 525 Mobil SHC 500 Series Mobil SHC 500 Series oils are supreme performance hydraulic oils formulated from synthesised, wax-free hydrocarbon base fluids combined with a carefully engineered super-stabilised additive system. .. |