Thermal Properties | Metric | English | Comments |
---|---|---|---|
Pour Point | -53.0 °C | -63.4 °F | Base Oil; ASTM D97 |
Nye Lubricants DHL-600 Oil Information provided by Nye Lubricants. |
|||
Pour Point | -53.0 °C | -63.4 °F | Base Oil; ASTM D97 |
Nye Lubricants UniFlor 8770 (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -53.0 °C | -63.4 °F | Base Oil; ASTM D97 |
Nye Lubricants UniFlor 8771 (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -53.0 °C | -63.4 °F | Base Oil; ASTM D97 |
Nye Lubricants UniFlor 8771R (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -53.0 °C | -63.4 °F | |
ChevronTexaco Rando® HDZ 22 Texaco Rando HDZ oils deliver value through:High oxidation stability — Longer service life than attainable with conventional lubricants used in high pressure service.Protection against rust and cor.. |