Thermal Properties | Metric | English | Comments |
---|---|---|---|
Pour Point | -25.0 °C | -13.0 °F | Base Oil; ASTM D97 |
Nye Lubricants 794 (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -25.0 °C | -13.0 °F | Base Oil; ASTM D97 |
Nye Lubricants 794RP (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -25.0 °C | -13.0 °F | Base Oil; ASTM D97 |
Nye Lubricants NYOIL Oil Information provided by Nye Lubricants. |
|||
Pour Point | -25.0 °C | -13.0 °F | Base Oil; ASTM D97 |
Nye Lubricants UniFlor 8610 (496) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -25.0 °C | -13.0 °F | Base Oil; ASTM D97 |
Nye Lubricants UniFlor 8612 (849) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -25.0 °C | -13.0 °F | ASTM D97 |
Solvay Specialty Polymers FOMBLIN® YPL1500 PFPE Lubricant FOMBLIN YR perfluoropolyether fluids have excellent high temperature stability, good low temperature properties, very good E.P. and wear characteristics, good evaporative loss, and good viscosity in.. |
|||
Pour Point | -25.0 °C | -13.0 °F | ASTM D97 |
Solvay Specialty Polymers FOMBLIN® YR PFPE Lubricant FOMBLIN YR perfluoropolyether fluids have excellent high temperature stability, good low temperature properties, very good E.P. and wear characteristics, good evaporative loss, and good viscosity in.. |
|||
Pour Point | -25.0 °C | -13.0 °F | ASTM D97, DIN 51 350 |
Chesterton 601 Chain Drive Pin & Bushing Lubricant Description: Chesterton® 601 Chain Drive Pin & Bushing Lubricant is and has been the premium quality light lubricant of choice in industry for over thirty years. This superior lubricant was special.. |
|||
Pour Point | -25.0 °C | -13.0 °F | ASTM D97, ISO 3016 |
Chesterton 610 MT Plus Synthetic Lubricating Fluid Description: Chesterton® 610 MT Plus Synthetic Lubricating Fluid is a premium quality full synthetic lubricant designed to provide lubrication at temperatures ranging from 25°C (-15°F) to those o.. |
|||
Pour Point | -25.0 °C | -13.0 °F | Base Oil (UniFlor 8610); ASTM D97 |
Donnelly Bros HT 500 High Temperature Mold Grease White. Slight odor. Use caution when handling. Light caramel-like texture. Does not migrate, works well in constant metal temperature of 250° F to 500° F. (Note: The plastic molding material .. |
|||
Pour Point | -25.0 °C | -13.0 °F | |
ELM® SoyFluid™ Hydraulic Universal Tractor Biodegradable Tractor Hydraulic-Transmission Fluid Description: ELM SoyFluid™ Hydraulic Universal Tractor is a readily biodegradable tractor hydraulic transmission fluid formulated with Biotechbased™ USA grown natural vegetable oils. This product.. |
|||
Pour Point | -25.0 °C | -13.0 °F | |
3M Fluorinert™ FC-70 Electronic Liquid Fluorinert™ Liquid FC-70 a non-conductive, thermally and chemically stable liquid that offers a high boiling point (215 deg C), it is ideal for many electronics single and two phase heat transfer a.. |
|||
Pour Point | -25.0 °C | -13.0 °F | ASTM D97, ISO 3016 |
Chesterton 652 Pneumatic Lubricant & Conditioner Description: Chesterton® 652 Pneumatic Lubricant & Conditioner is a high performance, low viscosity, lubricating formula designed to creep into the internal workings of air tools, reduce wear and e.. |