Thermal Properties | Metric | English | Comments |
---|---|---|---|
Pour Point | -23.3 °C | -10.0 °F | |
Lubriplate 32 Turbine Oil Petroleum-Based Air Compressor Fluid This high-performance, zinc-free fluid meets the requirements of most centrifugal air compressors. Provides excellent oxidation resistance. Turbine Oil 32 is available in Drums.Information provided .. |
|||
Pour Point | -23.3 °C | -10.0 °F | |
Lubriplate AC-3 Petroleum-Based Air Compressor Fluid Formulated to reduce carbon & varnish buildup. They contain fluid zinc to effectively fight friction & wear thus reducing heat & foaming. Available in six ISO grades.AC Series Air Compressor Oils ar.. |
|||
Pour Point | -23.3 °C | -10.0 °F | |
Lubriplate FMO 350 AW USP Mineral Oil-Based Food Machinery Grade Oil For use where a Class H-1 oil is required. Manufactured in nine ISO grades for a variety of applications. Anti-wear fortified. NOTE: FMO-350AW is also available in a red and orange color which helps.. |
|||
Pour Point | -23.3 °C | -10.0 °F | |
Lubriplate H0-3 Petroleum-Based Heavy-Duty Hydraulic Oil Formulated for superior performance, this series contains fluid zinc to effectively reduce ring & vane wear. Excellent anti-rust, anti-corrosion, anti-foam and anti-oxidation properties. High anilin.. |
|||
Pour Point | -23.3 °C | -10.0 °F | |
Lubriplate SPO-255 Petroleum-Based Gear, Bearing, & Recirculating Oil Petroleum-based oils specifically designed for industrial applications such as gear cases, bearings, chains, machine ways, and general oiling. These tacky lubricants will provide anti-wear lubricati.. |
|||
Pour Point | -23.3 °C | -10.0 °F | |
ConocoPhillips Hydroclear® 150 AW Hydraulic Fluid Description: Conoco Hydroclear AW Hydraulic Fluid is specifically designed for use in high-pressure systems which require greater wear protection and deposit control than that provided by standard a.. |
|||
Pour Point | -23.3 °C | -10.0 °F | |
ConocoPhillips Hydroclear® 150 Rock Oil Description: Conoco Hydroclear Rock Drill Oil is a high-quality, heavy-duty, extreme-pressure pneumatic tool lubricant formulated from premium Conoco hydrocracked base stocks. Hydroclear Rock Drill .. |