Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : UL RTI, Mechanical without Impact = 110 °C Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
UL RTI, Mechanical without Impact 110 °C
230 °F
UL 746B
SABIC Innovative Plastics Lexan® FL930 PC
Various weight reductions at 0.250"" (6.35 mm) wall, 30% GR. Superior flex strength/modulus, good tensile strength. V-0/5VA at 0.250"" (6.35 mm).
UL RTI, Mechanical without Impact 110 °C
230 °F
UL 746B
SABIC Innovative Plastics Lexan® FL930 PC (Asia Pacific)
Various weight reductions at 0.250"" (6.35 mm) wall, 30% GR. Superior flex strength/modulus, good tensile strength. V-0/5VA at 0.250"" (6.35 mm).
UL RTI, Mechanical without Impact 110 °C
230 °F
UL746B
Idemitsu Kosan Xarec® WA 212 SPS, 30% Glass Filled
Crystalline Polymer, Glass Filled, Impact Modified. Used in Automotive and Industrial applications.
UL RTI, Mechanical without Impact 110 °C
230 °F
UL746B
Idemitsu Kosan Xarec® WA 212LG SPS, 30% Glass Filled
UL RTI, Mechanical without Impact 110 °C
230 °F
UL 746B
SABIC Innovative Plastics NORYL PX9406 PPE+PS
Nonbrominated, nonchlorinated, flame retarded. Improved productivity and reliability. 252F HDT. UL94 V-0 rated. Electrical applications.
UL RTI, Mechanical without Impact 110 °C
230 °F
UL 746B
SABIC Innovative Plastics NORYL PX9406 PPE+PS (Asia Pacific)
Nonbrominated, nonchlorinated, flame retarded. Improved productivity and reliability. 252F HDT. UL94 V-0 rated. Electrical applications.
UL RTI, Mechanical without Impact 110 °C
230 °F
UL 746B
SABIC Innovative Plastics NORYL PX9406K PPE+HIPS (Asia Pacific)
NORYL* PX9406K resin may be suitable for consumer electronics applications. Flame retardant used is non-halogenated. UL94 V0 at 1.5 mm, 5VB at 2 mm, and 5VA at 2.5 mm. RTI (impact) = 105 C
UL RTI, Mechanical without Impact 110 °C
230 °F
UL 746B
SABIC Innovative Plastics NORYL PX9406P PPE
NORYL* PX9406P resin is an FR (non-halogenated) grade potentially suitable for a variety of electronics applications. RTI (impact) = 105 C. F1 listed in BK color.
UL RTI, Mechanical without Impact 110 °C
230 °F
UL 746B
SABIC Innovative Plastics NORYL PX9406P PPE+PS (Europe-Africa-Middle East)
UL RTI, Mechanical without Impact 110 °C
230 °F
UL 746B
SABIC Innovative Plastics NORYL RN1300 PPE (Asia Pacific)
15% glass/mineral reinforced PPE. Nonchlorinated, nonbrominated, flame-retardant. Black and gray.
UL RTI, Mechanical without Impact 110 °C
230 °F
UL 746B
SABIC Innovative Plastics NORYL SE1GFN1 PPE+PS (Asia Pacific)
10% GR. UL94 V-1 rated. Halogen free flame retardant. Typical applications are TV chassis, deflection yokes and connectors.
UL RTI, Mechanical without Impact 110 °C
230 °F
UL 746B
SABIC Innovative Plastics NORYL SE1GFN2 PPE+HIPS (Europe-Africa-Middle East)
Noryl* SE1GFN2 is a 20% glass reinforced, injection moldable modified polyphenylene ether resin. Designed for improved dimensional stability and good flow , this resin also uses non-chlorinated, non..
UL RTI, Mechanical without Impact 110 °C
230 °F
UL 746B
SABIC Innovative Plastics NORYL SE1GFN2 PPE+PS
PPE+PS blend. 20% Glass reinforced. Non-brominated, non-chlorinated FR system. UL94 V1 and 5VA listing. RTI 110/105/110. Dielectric strength. Dimensional stability. Suitable for E/E applications.
UL RTI, Mechanical without Impact 110 °C
230 °F
UL 746B
SABIC Innovative Plastics NORYL SE1GFN3 PPE+PS
PPE+PS blend. 30% Glass reinforced. Non-brominated, non-chlorinated FR system. UL94 V1 listing. RTI 110/105/110. Dielectric strength. Dimensional stability. Suitable for E/E applications.
UL RTI, Mechanical without Impact 110 °C
230 °F
UL 746B
SABIC Innovative Plastics NORYL SE1GFN3 PPE+PS (Asia Pacific)
GR 30%. 275F (135C) DTUL. UL94 V-1 rated. Halogen free flame retardant. For electrical construction market.
UL RTI, Mechanical without Impact 110 °C
230 °F
UL 746B
SABIC Innovative Plastics NORYL SE1X PPE+PS
PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V1, UL746C F1. Dielectric strength. Suitable for E/E market indoor/outdoor applications.
UL RTI, Mechanical without Impact 110 °C
230 °F
UL 746B
SABIC Innovative Plastics Valox® 865 PBT+PET
30% GR PBTP, UL94 V-0 rated. Non-blooming flame retardant. Improved surface appearance. Same application areas as for VALOX 855.
UL RTI, Mechanical without Impact 110 °C
230 °F
UL 746B
SABIC Innovative Plastics Valox® 865 PBT+PET (Asia Pacific)
30% GR PBTP, UL94 V-0 rated. Non-blooming flame retardant. Improved surface appearance. Same application areas as for VALOX 855.
UL RTI, Mechanical without Impact 110 °C
230 °F
UL 746B
SABIC Innovative Plastics NORYL NH5020 PPE+PS
Noryl* NH5020 Resin is an unreinforced blend of Polyphenylene Ether(PPE) + Polystyrenre resin. The material offers a good balance of heat, flow, hydrolytic stability, and non-halogenated flame reta..
UL RTI, Mechanical without Impact 110 °C
230 °F
UL 746B
SABIC Innovative Plastics NORYL NH6020 PPE+HIPS (Europe-Africa-Middle East)
Noryl* NH6020 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 0.8 mm an..
UL RTI, Mechanical without Impact 110 °C
230 °F
UL 746B
SABIC Innovative Plastics NORYL NH7112 PPE+HIPS
Noryl* NH7112 resin is a 10% glass reinforced, modified PPE-PS blend. The material offers an exceptional balance of strength and dimensional stability while using non-halogenated flame retardants to..
UL RTI, Mechanical without Impact 110 °C
230 °F
UL 746B
SABIC Innovative Plastics NORYL NH7112 PPE+HIPS (Europe-Africa-Middle East)
Noryl* NH7112 resin is a 10% glass reinforced, modified PPE-PS blend. The material offers an exceptional balance of strength and dimensional stability while using non-halogenated flame retardants to..
UL RTI, Mechanical without Impact 110 °C
230 °F
UL 746B
SABIC Innovative Plastics NORYL NH7114 PPE+HIPS (Asia Pacific)
Noryl* NH7114 resin is a 20% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve UL94 flame ratings while offering an exceptional balance of streng..
UL RTI, Mechanical without Impact 110 °C
230 °F
UL 746B
SABIC Innovative Plastics NORYL NH8006 PPE+HIPS (Asia Pacific)
Noryl* NH8006 resin is a 30% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve a UL94 V0 flame rating (color specific) while offering an exceptio..
UL RTI, Mechanical without Impact 110 °C
230 °F
UL 746B
SABIC Innovative Plastics LNP THERMOCOMP Noryl_PX5379 PPE+HIPS (Europe-Africa-Middle East)
LNP* Thermocomp* Noryl_PX5379 compound is a 10% GR. UL94 V-1 rated. Halogen free flame retardant. Typical applications are TV chassis, deflection yokes and connectors.
UL RTI, Mechanical without Impact 110 °C
230 °F
UL 746B
SABIC Innovative Plastics LNP VERTON RV00AESP PA 66 (Europe-Africa-Middle East)
LNP* VERTON* RV00AESP is a compound based on PA66 resin containing Long Glass Fiber. Added features include : Easy Molding, Heat Stabilized.
UL RTI, Mechanical without Impact 110 °C
230 °F
UL 746B
SABIC Innovative Plastics LNP VERTON RV00AESS PA 66 (Europe-Africa-Middle East)
LNP* VERTON* RV00AESS is a compound based on PA 66 resin containing Long Glass Fiber. Added features include; Easy Molding, Heat Stabilized.
UL RTI, Mechanical without Impact 110 °C
230 °F
UL 746B
SABIC Innovative Plastics LNP VERTON RV00AEXP PA 66 (Europe-Africa-Middle East)
LNP* VERTON* RV00AEXP is a compound based on PA 66 resin containing Long Glass Fiber.
UL RTI, Mechanical without Impact 110 °C
230 °F
Aclo Accuguard Polypropylene HP1369V2CSL Homopolymer Flame Retardant Copper Stabilized
UL RTI, Mechanical without Impact 110 - 130 °C
230 - 266 °F
Average value: 122 °C Grade Count:16
Overview of materials for Nylon 46, Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum values ..
Copyright © lookpolymers.com All Rights Reserved