Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical without Impact | 200 °C | 392 °F | E54153 |
Arlon 31580R020 0.020" (0.508 mm) Uncured Silicone Rubber on HDPE Carrier
(discontinued **) Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: High Density PolyethyleneAppearance: Red silicone gum on polymer linerThis data represents typical values for the.. |
|||
UL RTI, Mechanical without Impact | 200 °C | 392 °F | per UL Card E54153 |
Arlon 48571R005 0.0055" (0.140 mm) Uncured Silicone Rubber with Fiberglass Substrate
(discontinued **)&l Design/Construction:Side 1: Uncured RubberSide 2: Uncured RubberThis data represents typical values for the production material. The data should not be used to write, or in place of, material specif.. |
|||
UL RTI, Mechanical without Impact | 200 °C | 392 °F | E54153 |
Arlon 19146R025 0.025" (0.635 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 1523 FiberglassSide 2: Uncured Silicone RubberInterleave: PolyethyleneAppearance: Black silicone gum and rubber on fiberglass clothT.. |
|||
UL RTI, Mechanical without Impact | 200 °C | 392 °F | per UL Card E54153 |
Arlon 19576R028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Red silicone gum and rubber on fiberglass clothThis data represents typical values for the production mat.. |
|||
UL RTI, Mechanical without Impact | 200 °C | 392 °F | per UL Card E54153 |
Arlon 30570R010 0.010" (0.254 mm) Uncured/Unsupported Silicone Rubber on a Release Carrier Design/Construction:Side 1: Uncured/Unsupported Silicone Rubber on a Release Carrier Appearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The.. |
|||
UL RTI, Mechanical without Impact | 200 °C | 392 °F | E63753 |
Arlon 41570R020 0.020" Uncured, Unsupported Silicone Rubber on Release Carrier Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured, Unsupported Silicone RubberSubstrate: Holland Cloth CarrierThis data represents typical values for the production material and .. |
|||
UL RTI, Mechanical without Impact | 200 °C | 392 °F | |
Arlon 51571B015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone RubberInterleave 2: Polyethylene This data represents typical.. |
|||
UL RTI, Mechanical without Impact | 200 °C | 392 °F | per card E54153 |
Arlon 51571XC015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place .. |
|||
UL RTI, Mechanical without Impact | 200 °C | 392 °F | |
Arlon 51576R024A 0.024" (0.610 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone Rubber This data represents typical values for the production mat.. |
|||
UL RTI, Mechanical without Impact | 200 °C | 392 °F | E54153 |
Arlon 55572GA028 0.028" Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: LDPESide 1: Cured Silicone RubberSubstrate: Style 162 FiberglassThis data represents typical values for the production material and should not be used as material .. |
|||
UL RTI, Mechanical without Impact | 200 °C | 392 °F | E54153 |
Arlon 55572R030 0.030" (0.762 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 162 Fiberglass Appearance: Red silicone rubber on fiberglass clothThis data Represents typical values for the production material. T.. |
|||
UL RTI, Mechanical without Impact | 200 °C | 392 °F | E54153 |
Arlon 55578R036 0.036" (0.914 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 2, Layer 2: Uncured Silicone Rubber Side 2, Layer 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Side 1: Cured Silicone Rubber Appearance:.. |
|||
UL RTI, Mechanical without Impact | 200 °C | 392 °F | E54153 |
Arlon 55578XA030 0.032" (0.813 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 2, Layer 2: Uncured Silicone Rubber Side 2, Layer 1: Cured Silicone Rubber Substrate: 162 Style Fiberglass Side 1: Cured Silicone Rubber (Skim Coat).. |
|||
UL RTI, Mechanical without Impact | 200 °C | 392 °F | File E54153 |
Arlon 55866R028 0.0295" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil PESide 2: Uncured Silicone RubberSubstrate: Style 162 FiberglassSide 1: Cured Silicone RubberThis data represents typical values for the production material .. |
|||
UL RTI, Mechanical without Impact | 200 °C | 392 °F | File E54153 |
Arlon 55869R062 0.062" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil PELayer 2: Uncured Silicone RubberLayer 1: Cured Silicone RubberSubstrate: Style 162 FiberglassThis data represents typical values for the production materia.. |
|||
UL RTI, Mechanical without Impact | 200 °C | 392 °F | E54153 |
Arlon 56141R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 2: Uncured Silicone Rubber Substrate: 1564 Style Fiberglass Side 1: Uncured Silicone Rubber This data represents typical values for the production m.. |
|||
UL RTI, Mechanical without Impact | 200 °C | 392 °F | E54153 |
Arlon 56146R028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 2: Uncured Silicone Rubber Substrate: 1564 Style Fiberglass Side 1: Cured Silicone Rubber Product Use: Flexible heater insulationAppearance: Red si.. |
|||
UL RTI, Mechanical without Impact | 200 °C | 392 °F | File E54153 |
Arlon 56579R028 0.0295" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 2.5 mil PELayer 2: Uncured Silicone RubberLayer 1: Cured Silicone RubberSubstrate: Style 1564 FiberglassThis data represents typical values for the production mate.. |
|||
UL RTI, Mechanical without Impact | 200 °C | 392 °F | |
Arlon CP-410XD Bulk Compound Design/Construction:Bulk Compound (packaged in polyethylene) This data Represents typical values for the production material. The data should not be used to write, or in place of, material specifica.. |
|||
UL RTI, Mechanical without Impact | 200 °C | 392 °F | per UL card E54153 |
Arlon R34931R010 0.011" (0.279 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place .. |
|||
UL RTI, Mechanical without Impact | 200 °C | 392 °F | per UL Car E54153 |
Arlon 44572R010 0.010" (0.254 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberAppearance: Red silicone rubber on fiberglass clothThis data represents typical values for the production material. The data should not be used to wr.. |
|||
UL RTI, Mechanical without Impact | 200 °C | 392 °F | per UL Car E54153 |
Arlon 44576R016 0.016" (0.406 mm) Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber This data represents typical values for the production material. The data should not be used to write, or in place of.. |
|||
UL RTI, Mechanical without Impact | 200 °C | 392 °F | E54153 |
Arlon 51149R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Layer 2: Uncured Silicone RubberSubstrate: Style 7628 FiberglassLayer 1: Cured Silicone RubberThis data represents typical values for the production mat.. |
|||
UL RTI, Mechanical without Impact | 200 °C | 392 °F | |
Arlon 51276R020 Silicone Rubber/Fiberglass Laminate Side 1: cured silicone rubber; Substrate: 7628 fiberglass; Side 2: uncured silicone rubber; Interleave: 3 mil polyethylene |
|||
UL RTI, Mechanical without Impact | 200 °C | 392 °F | |
Arlon 51576R031 0.031" (0.787 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone Rubber This data represents typical values for the production mat.. |
|||
UL RTI, Mechanical without Impact | 200 °C | 392 °F | |
Arlon 55143R060 Silicone Rubber/Fiberglass Laminate Interleave: 3 mil PE; Side 2: cured silicone rubber; Substrate: 162 fiberglass; Side 1: cured silicone rubber |
|||
UL RTI, Mechanical without Impact | 200 °C | 392 °F | per UL card E54153 |
Arlon 55578XA030M 0.0305" (0.775 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured/Uncured Layers This data Represents typical values for the production material. The data should not be used to write, or in place of, m.. |
|||
UL RTI, Mechanical without Impact | 200 °C | 392 °F | E54153 |
Arlon 55586R040 0.040" (1.02 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone Rubber Substrate: Style 162 FiberglassSide 2: Uncured Silicone RubberInterleave: LDPEAppearance: Red silicone gum and rubber on fiberglass clothThis data .. |
|||
UL RTI, Mechanical without Impact | 200 °C | 392 °F | per UL Car E54153 |
Arlon 44570B010 0.010" (0.254 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Layers Silicone Rubber This data represents typical values for the production material. The data should not be used to write, or in place of, material specificati.. |
|||
UL RTI, Mechanical without Impact | 200 °C | 392 °F | per UL Car E54153 |
Arlon 44580R010 0.010" (0.254 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberAppearance: Red silicone gum on fiberglass clothThis data represents typical values for the production material. The data should not be used to wri.. |