Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical without Impact | 140 °C @Thickness 0.750 mm |
284 °F @Thickness 0.0295 in |
UL 746B |
DuPont Performance Polymers Crastin® SK645FR BK851 PBT
(Unverified Data**) Crastin® SK645FR BK851 is a flame retardant , 30% glass reinforced black polybutylene terephthalate molding resin. It is recognized as UL94V-0 at 0.75mm.Information provided by DuPont Performance P.. |
|||
UL RTI, Mechanical without Impact | 140 - 150 °C | 284 - 302 °F | Average value: 149 °C Grade Count:4 |
Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 30% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 30% Glass Reinforced".Specific grades with glass content between 25% and 34% are included. .. |
|||
UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics ULTEM LTX300B PEI Standard flow Polyetherimide blend with low toxicity, smoke, and flame evolution. ECO Compliant, UL94 V0 listing. |
|||
UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics Valox® 325 PBT General purpose, unreinforced, improved processing. Applications like sprinklers and nozzles, pumps, door handle, tank covers, pens, pencils etc. |
|||
UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics Valox® 735 PBT 40% glass/mineral, excellent thermal performance/low shrink. Motorized heating appliances, adaptor rings, oven grills, etc. Black/natural only.This data was supplied by SABIC-IP for the Americas re.. |
|||
UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics Valox® 735 PBT (Asia Pacific) 40% glass/mineral, excellent thermal performance/low shrink. Motorized heating appliances, adaptor rings, oven grills, etc. Black/natural only. |
|||
UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics Valox® 771 PBT 35% mineral/glass reinforced flame retardant grade with a CTI performance level class of 0 rating. Applications which may see electrical arcing. |
|||
UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics Valox® 780 PBT (Asia Pacific) 40% gl/min, UL94 V-0 rated. Nonblooming flame retardant. Circuit breaker handles/housings, motor coil housings. |
|||
UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics Valox® DR51M PBT (Asia Pacific) 15% GR; exc. mechanical/thermal/electrical performance; nonflame retardant. For spotlights, appliance housings, handles. Easy flow/int. mold release.This data was supplied by SABIC-IP for the Asia .. |
|||
UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics Valox® ENH4565 PBT (Asia Pacific) 33% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin, Good thermal shock resistance and low CTE. |
|||
UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics Valox® EXVX0095 PBT (Europe-Africa-Middle East) VALOX EXVX0095 will be GLOBAL 420SE0 per January 2009.
30% GF PBT Flame Retardant.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics Valox® IQ357 PBT+PC (Europe-Africa-Middle East) Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified. |
|||
UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics Valox® IQ357U PBT+PC Valox* Resin IQ357U: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified and UV stabilized resin. |
|||
UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics Valox® IQ420 PBT Environmentally responsible Valox iQ420 resin: iQ-PBT+ 30% glass fiber reinforcement. Targeted for use in electrical motors, connectors, pump housings, spotlights, appliance handles, etc. |
|||
UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics Valox® IQ420 PBT (Asia Pacific) Environmentally responsible Valox iQ420 resin: iQ-PBT+ 30% glass fiber reinforcement. Targeted for use in electrical motors, connectors, pump housings, spotlights, appliance handles, etc. |
|||
UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics Xenoy® 6370 PBT+PC 30% glass-reinforced, impact modified thermoplastic alloy. Improved toughness and ductility. |
|||
UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics Xenoy® 6370 PBT+PC (Europe-Africa-Middle East) XENOY 6370 is an impact modified semi-crystalline thermoplastic. blend with 30% glass fibre reinforcement offering toughness and ductility. |
|||
UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics LNP Thermocomp RF0057E PA 66 (Asia Pacific) LNP* Thermocomp* RF0057E is a compound based on Nylon 66 resin containing Glass Fiber, Flame Retardant. Added features of this material include: Non-Brominated & Non-Chlorinated Flame Retardant.Thi.. |
|||
UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics LNP Thermocomp RF0057E PA 66 (Europe-Africa-Middle East) LNP* Thermocomp* RF0057E is a compound based on Nylon 66 resin containing Glass Fiber, Flame Retardant. Added features of this material include: Non-Brominated & Non-Chlorinated Flame Retardant.Thi.. |
|||
UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics Valox® 430 PBT (Asia Pacific) 33 % glass reinforced, impact modified. Connectors, etc. |
|||
UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics Valox® 451E PBT (Asia Pacific) 20% GR. Easy flow version of VALOX 451. |
|||
UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics Valox® EXVX1403 PBT (Asia Pacific) 33% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin, Good thermal shock resistance and low CTE. |
|||
UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics Valox® IQ357M PBT+PC (Europe-Africa-Middle East) Valox* Resin IQ357M: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified, easy flow product with mold release. |
|||
UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics Valox® IQNH4550 PBT (Europe-Africa-Middle East) Valox* iQNH4550 resin is a non-brominated/non-chlorinated flame retardant product based on an environmentally sustainable Valox iQ* PBT resin. Post-consumer recycle (PCR) usage is 31% based on EPEAT.. |
|||
UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics Valox® IQNH4565 PBT (Asia Pacific) Valox* iQNH4565 resin is a non-brominated/non-chlorinated flame retardant product based on an environmentally sustainable Valox iQ* PBT resin. Post-consumer recycle (PCR) usage is 29% based on EPEAT.. |
|||
UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics Xenoy® X3108UV PBT+PC (Asia Pacific) Unreinforced, UV-stabilized, flame retardant, impact modified PBT+PC with V0 at 0.8mm thickness. For interior and exterior applications like wall switches and electrical enclosures.This data was sup.. |
|||
UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
DuPont Performance Polymers Rynite® 530 BK503 PET
(Unverified Data**) Rynite® 530 BK503 is a 30% glass reinforced modified polyethylene terephthalate with outstanding balance of strength, stiffness, and toughness, excellent electrical properties, surface appearance, .. |
|||
UL RTI, Mechanical without Impact | 140 °C @Thickness 1.50 mm |
284 °F @Thickness 0.0591 in |
UL 746B |
DuPont Performance Polymers Rynite® 530 BK503 PET
(Unverified Data**) Rynite® 530 BK503 is a 30% glass reinforced modified polyethylene terephthalate with outstanding balance of strength, stiffness, and toughness, excellent electrical properties, surface appearance, .. |
|||
UL RTI, Mechanical without Impact | 140 °C @Thickness 0.810 mm |
284 °F @Thickness 0.0319 in |
UL 746B |
DuPont Performance Polymers Rynite® 530 BK503 PET
(Unverified Data**) Rynite® 530 BK503 is a 30% glass reinforced modified polyethylene terephthalate with outstanding balance of strength, stiffness, and toughness, excellent electrical properties, surface appearance, .. |