Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical with Impact | 50.0 - 105 °C | 122 - 221 °F | Average value: 64.0 °C Grade Count:5 |
Overview of materials for Polystyrene + Polyphenylene Ether, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Unreinforced". Each property range of values reported is minimum and .. |
|||
UL RTI, Mechanical with Impact | 105 - 105 °C @Temperature 105 - 105 °C |
221 - 221 °F @Temperature 221 - 221 °F |
Average value: 105 °C Grade Count:1 |
Overview of materials for PVC, Rigid Grade This property data is a summary of similar materials in the MatWeb database for the category "PVC, Rigid Grade". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
UL RTI, Mechanical with Impact | 65.0 - 105 °C | 149 - 221 °F | Average value: 81.0 °C Grade Count:4 |
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are incl.. |
|||
UL RTI, Mechanical with Impact | 50.0 - 105 °C | 122 - 221 °F | Average value: 86.7 °C Grade Count:3 |
Overview of materials for Polystyrene + Polyphenylene Ether, Glass Filler This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Glass Filler". Each property range of values reported is minimum and .. |