Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical with Impact | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics Lexan® 503R PC 10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. UV-stabilized. Internal mold release. |
|||
UL RTI, Mechanical with Impact | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics Lexan® EXL9330S PC Copolymer Opaque PC-Siloxane copolymer with excellent processability. UV stabilized. UL rated V-0/5VA/CTI-PLC-2. Available in limited colors. |
|||
UL RTI, Mechanical with Impact | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics Lexan® EXL9330S PC Copolymer (Asia Pacific) Opaque PC-Siloxane copolymer with excellent processability. UV stabilized. UL rated V-0/5VA/CTI-PLC-2. Available in limited colors. |
|||
UL RTI, Mechanical with Impact | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics Lexan® EXL9330S PC Copolymer (Europe-Africa-Middle East) Opaque PC-Siloxane copolymer with excellent processability. UV stabilized. UL rated V-0/5VA/CTI-PLC-2. Available in limited colors. |
|||
UL RTI, Mechanical with Impact | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics Lexan® FL930 PC (Asia Pacific) Various weight reductions at 0.250"" (6.35 mm) wall, 30% GR. Superior flex strength/modulus, good tensile strength. V-0/5VA at 0.250"" (6.35 mm). |
|||
UL RTI, Mechanical with Impact | 110 °C | 230 °F | Minimum thickness 0.040 inches. |
LyondellBasell Pro-fax 6323 Polypropylene Homopolymer, Easy Molding Primary Processing Method: General PurposeKey Features: easy molding, FDA acceptable, general purpose polypropylene homopolymer resinApplications: containers, closures, hospital and institutional wa.. |
|||
UL RTI, Mechanical with Impact | 110 °C | 230 °F | UL746B |
Idemitsu Kosan Xarec® EA 543 SPS, 40% Glass Filled |
|||
UL RTI, Mechanical with Impact | 110 °C | 230 °F | UL746B |
Idemitsu Kosan Xarec® WA 212 SPS, 30% Glass Filled Crystalline Polymer, Glass Filled, Impact Modified. Used in Automotive and Industrial applications. |
|||
UL RTI, Mechanical with Impact | 110 °C | 230 °F | UL746B |
Idemitsu Kosan Xarec® WA 212LG SPS, 30% Glass Filled |
|||
UL RTI, Mechanical with Impact | 110 °C | 230 °F | |
LG Chemical LUPOY GN1006FT PC, Halogen Free, Flame Retardant Description: Injection Molding, PC, Halogen Free Flame Retardant, Good FlowApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2Information provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 110 °C @Thickness 1.60 mm |
230 °F @Thickness 0.0630 in |
|
LyondellBasell Higlass SB224-2 Polypropylene Copolymer, 20% Glass Fiber Key Features: conventional melt flow, medium modulus, chemically coupled, glass fiber-reinforced polypropylene copolymer, high impact strength, moderate rigidity, good processabilityApplications: of.. |
|||
UL RTI, Mechanical with Impact | 110 °C @Thickness 1.60 mm |
230 °F @Thickness 0.0630 in |
|
LyondellBasell Higlass SB224-3 Polypropylene Copolymer, 30% Glass Fiber Key Features: conventional melt flow, medium high modulus, chemically coupled, glass fiber-reinforced polypropylene copolymer, high impact strength, high stiffness, good processabilityApplications: .. |
|||
UL RTI, Mechanical with Impact | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics Valox® 508 PBT (Europe-Africa-Middle East) VALOX 508 is a 30% glass reinforced PBT+PC blend with good warpage characteristics. Applications: appliance handles, spotlights, electric motors, distributor caps, ignition rotors, voltage regulator.. |
|||
UL RTI, Mechanical with Impact | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics Valox® 553 PBT+PC (Asia Pacific) 30% GR PBT+PC, UL94 V-0. Reduced warpage characteristics.Applications; appliance handles, spotlights, electric motors, pump housings, etc. |
|||
UL RTI, Mechanical with Impact | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics Valox® 553U PBT+PC 30% GR PBT+PC, UL94 V-0. Reduced warpage characteristics.Applications; appliance handles, spotlights, electric motors, pump housings, etc. |
|||
UL RTI, Mechanical with Impact | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics Valox® 815 PBT 15% GR PBT+ PET, excellent surface finish. Typical applications are hot air gun housing assemblies, industrial glue guns, appliance housings and handles. |
|||
UL RTI, Mechanical with Impact | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics Valox® 855 PBT 15% GR PBTP, UL94 V-0 rated. Improved surface appearance. For external housings: steam irons, appliance housings and lighting parts. |
|||
UL RTI, Mechanical with Impact | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics Valox® 865 PBT+PET (Asia Pacific) 30% GR PBTP, UL94 V-0 rated. Non-blooming flame retardant. Improved surface appearance. Same application areas as for VALOX 855. |
|||
UL RTI, Mechanical with Impact | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics LNP Thermocomp RF0057E PA 66 (Asia Pacific) LNP* Thermocomp* RF0057E is a compound based on Nylon 66 resin containing Glass Fiber, Flame Retardant. Added features of this material include: Non-Brominated & Non-Chlorinated Flame Retardant.Thi.. |
|||
UL RTI, Mechanical with Impact | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics NORYL GTX GTX918W PPE+PA (Europe-Africa-Middle East) NORYL GTX918W is an unfilled global grade, which offers an excellent combination of processability and heat resistance. |
|||
UL RTI, Mechanical with Impact | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics Valox® 508 PBT+PC (Asia Pacific) 30% GR PBT+PC. Excellent mechanical and thermal performance. Non-flame retardant. Reduced warpage characteristics. Applications same as VALOX 420. |
|||
UL RTI, Mechanical with Impact | 110 °C | 230 °F | UL 746 |
Styron EMERGEâ„¢ 4701-13 Polycarbonate EMERGEâ„¢ PC 4701-13 advanced resin is formulated with 10% glass fiber and a proprietary flame retardant package. It provides good ignition resistance, rigidity, dimension stability and heat res.. |
|||
UL RTI, Mechanical with Impact | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics LNP VERTON RV00AES PA 66 (Europe-Africa-Middle East) LNP VERTON* RV00AES is a compound based on PA 66 resin containing Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized. |
|||
UL RTI, Mechanical with Impact | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics LNP VERTON RV00AESC PA 66 (Europe-Africa-Middle East) LNP* VERTON* RV00AESC is a compound based on PA 66 resin containing Long Glass Fiber. Added features include; Easy Molding, Heat Stabilized. |
|||
UL RTI, Mechanical with Impact | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics LNP VERTON RV00AESS PA 66 (Europe-Africa-Middle East) LNP* VERTON* RV00AESS is a compound based on PA 66 resin containing Long Glass Fiber. Added features include; Easy Molding, Heat Stabilized. |
|||
UL RTI, Mechanical with Impact | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics LNP VERTON RV00AEX5 PA6.6 (Europe-Africa-Middle East) LNP* VERTON* Is a compound based on PA66 resin containing Long Glass Fiber. Added features include: Easy Molding, Heat Stabilized. |
|||
UL RTI, Mechanical with Impact | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics LNP VERTON RV00AEXP PA 66 (Europe-Africa-Middle East) LNP* VERTON* RV00AEXP is a compound based on PA 66 resin containing Long Glass Fiber. |
|||
UL RTI, Mechanical with Impact | 110 °C | 230 °F | |
Covestro Makrolon® 6485 Polycarbonate, Injection Grade Medium viscosity, flame retardant injection molding grade with easy mold release, not available in transparent colors.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was .. |
|||
UL RTI, Mechanical with Impact | 110 °C | 230 °F | |
Aclo Accuguard Polypropylene HP1362V2CSL Homopolymer Flame Retardant Copper Stabilized |
|||
UL RTI, Mechanical with Impact | 110 °C | 230 °F | |
Aclo Accuguard Polypropylene HP1369V2CSL Homopolymer Flame Retardant Copper Stabilized |