Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical with Impact | 85.0 °C | 185 °F | UL 746 |
PolyOne Geon™ Vinyl Rigid Molding M3500 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
UL RTI, Mechanical with Impact | 85.0 °C | 185 °F | UL 746 |
PolyOne Geon™ Vinyl Rigid Molding M5240 Natural Polyvinyl Chloride, Rigid (PVC, Rigid) NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. The weathering performance of.. |
|||
UL RTI, Mechanical with Impact | 85.0 °C | 185 °F | UL 746 |
PolyOne Geon™ Vinyl Rigid Molding M5240 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
UL RTI, Mechanical with Impact | 85.0 °C | 185 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® C2950HF PC+ABS Non-chlorinated and non-brominated flame retardant PC/ABS offering balanced impact and heat properties plus improved flow for various applications. |
|||
UL RTI, Mechanical with Impact | 85.0 °C | 185 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® C6200 PC+ABS (Asia Pacific) Non-chlorinated, nombrominated flame retardant PC/ABS offering balanced heat, flow and impact to meet various application needs. |
|||
UL RTI, Mechanical with Impact | 85.0 °C | 185 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® CY6110 PC+ABS (Asia Pacific) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la.. |
|||
UL RTI, Mechanical with Impact | 85.0 °C | 185 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® CY6310 PC+ABS Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la.. |
|||
UL RTI, Mechanical with Impact | 85.0 °C | 185 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® CY6310 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la.. |
|||
UL RTI, Mechanical with Impact | 85.0 °C @Thickness 0.750 mm |
185 °F @Thickness 0.0295 in |
UL-746B |
Shell Carilon® D26FX100 Polyketone, General-Purpose Extrusion Grade
(discontinued **) Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON Polymer D26FX100 is a general-purpose extrusion grade with mechanical properties that classify it as an eng.. |
|||
UL RTI, Mechanical with Impact | 85.0 °C | 185 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® C6200 PC+ABS Non-chlorinated, nombrominated flame retardant PC/ABS offering balanced heat, flow and impact to meet various application needs. |
|||
UL RTI, Mechanical with Impact | 85.0 °C | 185 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® C6800 PC+ABS PC+ABS, nonchlorinated, nonbrominated flame retardant.This data was supplied by SABIC-IP for the Americas region. |
|||
UL RTI, Mechanical with Impact | 85.0 °C @Thickness 1.57 mm |
185 °F @Thickness 0.0618 in |
|
Covestro Bayblend® 2153 Polycarbonate + ABS Blend, General Purpose
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
UL RTI, Mechanical with Impact | 85.0 °C @Thickness 1.57 mm |
185 °F @Thickness 0.0618 in |
|
Covestro Bayblend® 2773 Polycarbonate + ABS Blend, Automotive
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
UL RTI, Mechanical with Impact | 85.0 °C @Thickness 1.50 mm |
185 °F @Thickness 0.0591 in |
UL 746B |
Aardvark Polymers AARTEL® 2000 Rotational Molding Resin Aartel® 2000 POM is a premium homopolymer acetal for rotational molding applications. Aartel® 2000 offers high performance properties and is a high flow, fast cycling polymer.Information prov.. |
|||
UL RTI, Mechanical with Impact | 85.0 °C | 185 °F | UL 746B |
SABIC Innovative Plastics Valox® 3706 PBT+PC Impact modified PBT+PC resin. Outdoor enclosure. Not available in all colors. |
|||
UL RTI, Mechanical with Impact | 85.0 °C | 185 °F | |
Samsung Cheil Industries Infino® NH-1017D PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
UL RTI, Mechanical with Impact | 85.0 °C | 185 °F | |
Samsung Cheil Industries Infino® GC-1017 PC/ABS, FR Information provided by Samsung Cheil Industries. |
|||
UL RTI, Mechanical with Impact | 85.0 °C | 185 °F | |
Covestro Bayblend® FR 110 Polycarbonate/ABS Blend Flame retardant grade with antimony, chlorine and bromine free, flame retardant package, good light stability.Applications: Housings for business machines.Information provided by Bayer.As of 1 Septe.. |
|||
UL RTI, Mechanical with Impact | 85.0 °C | 185 °F | UL 746 |
ExxonMobil Santoprene® 203-40 Thermoplastic Elastomer A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
UL RTI, Mechanical with Impact | 85.0 °C | 185 °F | UL 746 |
ExxonMobil Santoprene® 8271-55 Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated .. |
|||
UL RTI, Mechanical with Impact | 85.0 °C @Thickness 1.60 mm |
185 °F @Thickness 0.0630 in |
UL-746B |
Axiall CL-6400 Rigid PVC, Molding Georgia Gulf CL-6400 is a high flow clear PVC compound designed for thin wall parts and multi-cavity molds. It is ideally suited for a variety of electrical and appliance applications.Information p.. |
|||
UL RTI, Mechanical with Impact | 85.0 °C @Thickness 1.40 mm |
185 °F @Thickness 0.0551 in |
UL-746B |
Axiall MP-6510 Rigid PVC, Molding Georgia Gulf MP-6510 is a maximum properties electrical grade PVC injection molding compound processing excellent strength and toughness. In addition, it has good processing stability and surface a.. |
|||
UL RTI, Mechanical with Impact | 85.0 °C @Thickness 1.40 mm |
185 °F @Thickness 0.0551 in |
UL-746B |
Axiall SP-7107 Rigid PVC, Molding Georgia Gulf SP-7107 is a general purpose, electrical grade rigid vinyl injection molding compound characterized by excellent flow, heat stability, color hold and surface appearance. This makes it .. |
|||
UL RTI, Mechanical with Impact | 85.0 °C | 185 °F | UL-746B |
Axiall Suprel® SVA 9412 Rigid PVC, Molding Georgia Gulf Suprel® SVA 9412 injection molding alloy features excellent impact resistance, excellent processing characteristics and comprehensive UL listings. The UL listings of Suprel 9412 inclu.. |
|||
UL RTI, Mechanical with Impact | 85.0 °C | 185 °F | UL 746 |
ExxonMobil Santoprene® 191-55PA Thermoplastic Elastomer
(discontinued **) A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to bond to PA-6 and blends thereof for applications where hard/soft .. |
|||
UL RTI, Mechanical with Impact | 85.0 °C | 185 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® CY6310 PC+ABS (Asia Pacific) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow / impact balance for a wide variety of thin wall or la.. |
|||
UL RTI, Mechanical with Impact | 85.0 °C | 185 °F | UL 746B |
SABIC Innovative Plastics NORYL FN170X PPE+PS Foamable resin. All properties at 10% density reduction; 0.250"" thick test specimens. |
|||
UL RTI, Mechanical with Impact | 85.0 °C | 185 °F | |
Covestro Bayblend® FR 2010 Polycarbonate/ABS Blend
(discontinued **) Easy-flowing FR grade. Flame retardant grade with antimony, chlorine and bromine free, flame retardant package, optimized processability.Applications: Housings for office equipment, electrical engin.. |
|||
UL RTI, Mechanical with Impact | 85.0 °C | 185 °F | UL-746B |
Axiall SP-6235 Rigid PVC, Molding Georgia Gulf SP-6235 is a high flow rigid PVC compound designed for electrical and custom molding applications. This compound features excellent physical properties, high melt flow and exceptionall.. |