Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 1.50 mm |
149 °F @Thickness 0.0591 in |
UL 746 |
Polymer Resources PPX-GP1-[color]-EN Modified-PPO, Extrusion Grade Modified-Polyphenylene Oxide, Extrusion Grade, 265F HDTFeatures: • Hydrolytically Stable • Low to No Water AbsorptionProcess: Extrusion Notes: All physical, mechanical and thermal testing conduc.. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 1.50 mm |
149 °F @Thickness 0.0591 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® 73G35HSL BK262 Nylon 6
(Unverified Data**) Zytel® 73G35HSL BK262 is a 35% glass fiber reinforced, heat stabilized, black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
UL RTI, Mechanical with Impact | 65.0 - 80.0 °C | 149 - 176 °F | Average value: 72.5 °C Grade Count:3 |
Overview of materials for Nylon 6-3 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6-3". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
UL RTI, Mechanical with Impact | 65.0 °C | 149 °F | Minimum thickness of 0.039 inches. |
LyondellBasell Pro-fax SB891 Polypropylene Impact Copolymer Key Features: high flow, compatible with hindered amine light stabilizers, good cold impact resistance, good stiffness and impact balance, high flow for ease of mold filling and minimum warpageAppli.. |
|||
UL RTI, Mechanical with Impact | 65.0 °C | 149 °F | Minimum thickness of 0.059 inches. |
LyondellBasell Pro-fax SD242 Polypropylene Impact Copolymer Key Features: short cycle times for high productivity, good cold impact resistance, good stiffness and impact balance, high flow ease of mold filling and minimum warpage, low odor and low taste tran.. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness >=0.750 mm |
149 °F @Thickness >=0.0295 in |
|
LG Chemical LUMID GP2500A(W) PA6+GF50%, General Purpose Feature: Injection Molding, PA6+GF50%, General PurposeApplication: Automotive (Gear Shift Housing)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 65.0 °C | 149 °F | UL 746B |
SABIC Innovative Plastics Noryl PX9406N PPE+HIPS (Europe-Africa-Middle East) Noryl PX9406N is an unfilled, halogen free (according VDE/DIN 472 part 813) flame retardant material with medium heat resistance. This material is V0 at 1.0 mm according to UL94.This data was suppli.. |
|||
UL RTI, Mechanical with Impact | 65.0 °C | 149 °F | UL 746B |
SABIC Innovative Plastics NORYL V090 PPE+HIPS (Europe-Africa-Middle East) NORYL V090 is an unfilled, flame retardant material with a Vicat B/120 of 95 °C according ISO 306. NORYL V090 is V0 at 2.0 mm and V1 at 1.6 mm according UL94 and halogen free according VDE/DIN 47.. |
|||
UL RTI, Mechanical with Impact | 65.0 °C | 149 °F | UL 746B |
SABIC Innovative Plastics LNP STAT-KON PFD04S PA 6 (Europe-Africa-Middle East) LNP* Statkon* PFD04S is a compound based on PA 6 resin containing Glass Fiber, Carbon Powder. Added features include: Electrically Conductive, Heat Stabilized. |
|||
UL RTI, Mechanical with Impact | 65.0 °C | 149 °F | UL 746B |
SABIC Innovative Plastics Noryl N750T PPE+HIPS ECO-FLO(tm). ECO conforming, nonhalogenated flame retardant PPE+PS. High flow. Electrical, TV and Business equipment applications.This data was supplied by SABIC-IP for the Americas region. |
|||
UL RTI, Mechanical with Impact | 65.0 °C | 149 °F | UL 746B |
SABIC Innovative Plastics NORYL PCN2910 PPE+PS (Asia Pacific) 35% Glass/Mica filled. High modulus and tight tolerance molding for the chassis market. |
|||
UL RTI, Mechanical with Impact | 65.0 °C | 149 °F | UL 746B |
SABIC Innovative Plastics LNP Thermocomp R1000HI620 PA 66 (Europe-Africa-Middle East) Impact modified Polyamide 66 injection moulding resin.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
UL RTI, Mechanical with Impact | 65.0 °C | 149 °F | UL 746B |
SABIC Innovative Plastics Noryl FXN2090H PPE+HIPS Noryl* FXN2090H resin is an unfilled, injection moldable grade. Designed for exceptionally high gloss and improved pencil hardness vs. standard Noryl grades, FXN2090H resin uses non-halogenated FR a.. |
|||
UL RTI, Mechanical with Impact | 65.0 °C | 149 °F | UL 746B |
SABIC Innovative Plastics Noryl FXN2090H PPE+HIPS (Europe-Africa-Middle East) Noryl* FXN2090H resin is an unfilled, injection moldable grade. Designed for exceptionally high gloss and improved pencil hardness vs. standard Noryl grades, FXN2090H resin uses non-halogenated FR a.. |
|||
UL RTI, Mechanical with Impact | 65.0 °C | 149 °F | UL 746B |
SABIC Innovative Plastics NORYL GFN1720 PPE+HIPS (Asia Pacific) Noryl* GFN1720 is a 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Noryl .. |
|||
UL RTI, Mechanical with Impact | 65.0 °C | 149 °F | UL 746B |
SABIC Innovative Plastics NORYL N1150 PPE+PS (Europe-Africa-Middle East) Noryl* N1150 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and good flow, this resin also uses non-chlorinated, non-brominated FR add.. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 0.780 mm |
149 °F @Thickness 0.0307 in |
UL 746 |
A. Schulman POLYFLAM™ FPP 1006 Talc Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1006 is a 20% talc filled homopolymer polypropylene compound.Information provided by A. Schulman. |
|||
UL RTI, Mechanical with Impact | 65.0 °C | 149 °F | |
Eurostar Staramide A28N PA66, Nucleated, Injection Molding Staramide A28K is an Unreinforced and Heat Stabilized, Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
UL RTI, Mechanical with Impact | 65.0 °C | 149 °F | |
Eurostar Staramide B40 PA6, Extrusion Staramide B40 is High Viscosity, Unreinforced Polyamide 6, Extrusion ResinInformation provided by Eurostar. |
|||
UL RTI, Mechanical with Impact | 65.0 °C | 149 °F | |
Eurostar Staramide BG7H PA6, 35% Glass Fiber Filled, Heat Stabilized, Injection Molded Staramide BG7H is a Heat Stabilized, 35% Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
UL RTI, Mechanical with Impact | 65.0 °C | 149 °F | |
Eurostar Staramide RF006SXP PA66, 30% Glass Fiber Filled, Injection Molded Staramide RF006SXP is a 30% Glass Fiber Reinforced Polyamide 66 Injection Molding Resin (also known as RF1006HS)Information provided by Eurostar. |
|||
UL RTI, Mechanical with Impact | 65.0 °C | 149 °F | |
Eurostar Starflam BFR460B1 PA6, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam BFR460B1 is a Flame Retardant, Glass Fiber Reinforced Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 0.750 mm |
149 °F @Thickness 0.0295 in |
DAM; UL 746B |
DuPont Performance Polymers Minlon® FE6190 BK086 Nylon 66 Minlon® FE6190 BK086 is a 36% mineral/glass reinforced, heat stabilized, black polyamide resin for injection molding.Information provided by DuPont Performance Polymers |
|||
UL RTI, Mechanical with Impact | 65.0 °C | 149 °F | |
Eurostar Staramide RF006XXP PA66, 30% Glass Fiber Filled, Injection Molded Staramide RF006XXP is a 30% Glass Fiber Reinforced Polyamide 66 Injection Molding Resin (also known as RF1006)Information provided by Eurostar. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness 1.50 mm |
149 °F @Thickness 0.0591 in |
746B |
BASF Nypel® 2314 HS BK6 PA6 (Dry) Description: Nypel® 2314 HS BK6 is a black pigmented, low viscosity, heat stabilized, semi crystalline, injection molding compound based on recycled PA6 feedstocks. It also offers the following: go.. |
|||
UL RTI, Mechanical with Impact | 65.0 °C | 149 °F | UL 746B |
SABIC Innovative Plastics NORYL FP5140HF PPE+PS Noryl*FP5140HF is an unfilled, injection moldable modified polyphenylene ether resin with an ISO306 Vicat B/120 of 100 deg C. Designed for good dimensional stability and high flow, this resin also u.. |
|||
UL RTI, Mechanical with Impact | 65.0 °C | 149 °F | UL 746B |
SABIC Innovative Plastics Noryl FXN2090H PPE+HIPS (Asia Pacific) Noryl* FXN2090H resin is an unfilled, injection moldable grade. Designed for exceptionally high gloss and improved pencil hardness vs. standard Noryl grades, FXN2090H resin uses non-halogenated FR a.. |
|||
UL RTI, Mechanical with Impact | 65.0 °C | 149 °F | UL 746B |
SABIC Innovative Plastics NORYL RN0612 PPE+HIPS (Europe-Africa-Middle East) Noryl RN0612 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 30% PCR styrenic series resin content. Designed for good dimen.. |
|||
UL RTI, Mechanical with Impact | 65.0 °C @Thickness >=1.50 mm |
149 °F @Thickness >=0.0591 in |
|
LG Chemical LUPOL GP3100 PP+MF10% Description: Injection Molding, PP+MF30%, General PurposeApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 65.0 - 120 °C | 149 - 248 °F | Average value: 76.0 °C Grade Count:9 |
Overview of materials for Polypropylene, Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Mineral Reinforced". Each property range of values reported is minimum and maximum values.. |