Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics Cycolac® EXABS01 ABS Sheet extrusion ABS with medium impact. |
|||
UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics Cycolac® FR15U ABS (Asia Pacific) Flame retardant ABS. Excellent indoor UV properties. Excellent moldability. UL94 V-0/5VA rated.ing. |
|||
UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics Cycolac® FR30U ABS (Asia Pacific) Flame retardant ABS. Good indoor UV properties. Excellent moldability with no bloom. V-1/V-0/5VB rated. |
|||
UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics Cycolac® MG29 ABS Super high impact ABS. Good low temperature toughness. High gloss. |
|||
UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics Cycolac® MG29 ABS (Asia Pacific) Super high impact ABS. Good low temperature toughness. High gloss. |
|||
UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics Cycolac® MG47 ABS (Europe-Africa-Middle East) Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. |
|||
UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics Cycolac® MG47F ABS (Asia Pacific) Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. FDA compliant. |
|||
UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics Cycolac® MG47F ABS (Europe-Africa-Middle East) Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. FDA compliant. |
|||
UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics Cycolac® X17 ABS Automotive: Very high heat resistance with high strength and modulus. UL94 HB rated.This data was supplied by SABIC-IP for the Americas region. |
|||
UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® C2800 PC+ABS (Europe-Africa-Middle East) Non-chlorinated and non-brominated flame retardant PC+ABS offering balanced flow and impact properties for various applications. |
|||
UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® CX1440 PC+ABS CYCOLOY CX1440 is a general purpose PC+ABS blend specially developped for thin wall applications requiring weld line strength and high flow with a good balance of properties |
|||
UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® CX7010 PC+ABS (Asia Pacific) Cycoloy* CX7010 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0. Excellent flow combined with good balance of pro.. |
|||
UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® CY6120 PC+ABS Non-chlorinated and non-brominated flame retardant PC/ABS featuring good flow and impact properties. UL-94 V0 listed at 1.2mm intended for various thin wall applications. |
|||
UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® FXC630ME PC+ABS Color package may affect performance. PC+ABS, ECO-conforming flame retardant with metallic or pearlescent appearance. |
|||
UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics Lexan® JK2000 PC+ABS (Asia Pacific) Lexan* JK2000 compound is a glass reinforced, non-Br and non-Cl FR polycarbonate blends designed for thinwall molding applications. |
|||
UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics LNP COLORCOMP A1000H ABS LNP* COLORCOMP* A1000H is an unfilled compound based on ABS. Added feature of this grade is: Healthcare. |
|||
UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics Cycolac® DL100 ABS (Europe-Africa-Middle East) CYCOLAC DL100 is a high heat, high impact, low emissions ABS/PC blend. |
|||
UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics Cycolac® EX58 ABS High impact ABS for sheet extrusion and blow molding applications. |
|||
UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® C1000HF PC+ABS (Europe-Africa-Middle East) CYCOLOY C1000HF is a general purpose PC+ABS blend specially developed for thin wall applications requiring a high flow with a good balance of properties. It is suitable for applications in the autom.. |
|||
UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® CY5100 PC+ABS (Asia Pacific) CY5100 is a Flame retardant PC blend using non-brominated and non-chlorinated flame retardant systems, offering excellent flow / impact balance for large size applications |
|||
UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | Average value: 60.0 °C Grade Count:10 |
Overview of materials for Polycarbonate/ABS Alloy, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Glass Fiber Filled". Each property range of values reported is minimum and maxi.. |
|||
UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics LNP LUBRICOMP Cycoloy_C2801 PC+ABS (Europe-Africa-Middle East) LNP* Lubricomp* Cycoloy_C2801 compound is a 5% PTFE reinforced PC+ABS wear resistant flame retardant resin for moving components in business equipment. Medium heat performance |
|||
UL RTI, Mechanical with Impact | 60.0 °C @Thickness >=1.70 mm |
140 °F @Thickness >=0.0669 in |
|
LG Chemical LUPOY GP5056F PC/ABS+GF5%, Flame Retardance Description: Injection Molding, PC/ABS+GF5%, Flame Retardance, General PurposeApplication: IT/OA (Housing)CAS: 103598-77-2, 9003-56-9, 68928-70-1, 1309-64-4 and 65997-17-3Information provided by LG .. |
|||
UL RTI, Mechanical with Impact | 60.0 °C @Thickness >=0.750 mm |
140 °F @Thickness >=0.0295 in |
|
LG Chemical LUPOY HP5004 PC/ABS, High Impact at Low Temperature Description: Injection Molding, PC/ABS, General Purpose, High Impact at Low Temperature, High Flow, Heat ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 9003-56-9Information provided.. |
|||
UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | |
Ineos ABS TRIAX® 1220 S ABS/Nylon Blend, As Conditioned Extrusion and injection molding grade with good stress corrosion cracking resistance, good chemical resistance (fuel, cleaning agents), high impact and notched impact strength, good acoustical dampi.. |
|||
UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics LNP THERMOCOMP Cycoloy_C7210A PC+ABS LNP* Thermocomp* Cycoloy_C7210A isa a talc-filled PC+ABS, nonhalogenated FR for thinwall molding applications. Very good modulus-ductility balance. |
|||
UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics NORYL GTX GTX810 PPE+PA (Europe-Africa-Middle East) NORYL GTX810 is a 10% glass reinforced grade with excellent chemical resistance in combination with high stiffness and high heat resistance. |
|||
UL RTI, Mechanical with Impact | 60.0 °C @Thickness 1.50 mm |
140 °F @Thickness 0.0591 in |
|
Covestro Bayblend® T 64 Polycarbonate/ABS Blend Easier flowing than BAYBLEND T 65 MN.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |
|||
UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | |
Covestro Bayblend® T 85 Polycarbonate/ABS Blend High impact and notched impact strength, little risk of brittle fracture, high dimensional accuracy.Applications: Automotive components, electrical engineering.Information provided by Bayer.As of 1 .. |
|||
UL RTI, Mechanical with Impact | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics LNP LUBRICOMP Cycoloy_C2801R PC+ABS LNP* Lubricomp* Cycoloy_C2801R compound is a 5% PTFE reinforced PC+ABS wear resistant, flame retardant compound for moving components in business equipment. 30% recycle content. |