Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical with Impact | 50.0 °C | 122 °F | UL 746 |
PolyOne Geon™ Vinyl Rigid Molding M5730 Natural Polyvinyl Chloride, Rigid (PVC, Rigid) NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. The weathering performance of.. |
|||
UL RTI, Mechanical with Impact | 50.0 °C | 122 °F | UL 746 |
PolyOne Geon™ Vinyl Rigid Molding M5731 Polyvinyl Chloride, Rigid (PVC, Rigid) NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. Dark colored compounds do not.. |
|||
UL RTI, Mechanical with Impact | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics Lexan® EXL1444 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1444 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade suitable for FDA compliant applications. This resin offers extreme low temperature (-.. |
|||
UL RTI, Mechanical with Impact | 50.0 °C | 122 °F | UL 746 |
PolyOne Geon™ 81510 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
UL RTI, Mechanical with Impact | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics Lexan® EXL9132 PC Copolymer (Asia Pacific) Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temperature ductility, UV stabilized. Non-chlorinated, non-brominated flame retardant product. UL rated V0/5VA. |
|||
UL RTI, Mechanical with Impact | 50.0 - 60.0 °C | 122 - 140 °F | Average value: 52.7 °C Grade Count:7 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded". Each property range of values reported is m.. |
|||
UL RTI, Mechanical with Impact | 50.0 °C @Thickness >=1.50 mm |
122 °F @Thickness >=0.0591 in |
|
LG Chemical LUPOS GP2205 SAN+GF20%, General Purpose Feature: Injection Molding, SAN+GF20%, General PurposeApplication: Electric & Electronic (Housing, Components)CAS No. 9003-54-7 and 65997-17-3Information provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 50.0 °C @Thickness >=1.50 mm |
122 °F @Thickness >=0.0591 in |
UL 746B |
LG Chemical TR300 MABS, Flame Retardant, Transparency Feature: Injection Molding, Flame Retardant, TransparencyApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9010-94-0 and 25713-60-4Information provided by LG Ch.. |
|||
UL RTI, Mechanical with Impact | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics NORYL SPN420 PPE+PS Superior Productivity plus heat and impact resistance. Excellent processability. |
|||
UL RTI, Mechanical with Impact | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics NORYL V01525 PPE+HIPS (Asia Pacific) Noryl* V01525 is a 15% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
UL RTI, Mechanical with Impact | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics NORYL V02570 PPE+HIPS Noryl* V02570 is a 25% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
UL RTI, Mechanical with Impact | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics NORYL V03550 PPE+HIPS Noryl* V03550 is a 35% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
UL RTI, Mechanical with Impact | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics NORYL V03550 PPE+HIPS (Asia Pacific) Noryl* V03550 is a 35% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
UL RTI, Mechanical with Impact | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics LNP LUBRICOMP Noryl_NF1520 PPE+HIPS (Europe-Africa-Middle East) LNP* Lubricomp* Noryl_NF1520 compound is a 20% glass reinforced, 15% PTFE. Wear resistant; 211F HDT @ 264 psi. |
|||
UL RTI, Mechanical with Impact | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics LNP LUBRICOMP Noryl_NF1520 PPE+PS LNP* Lubricomp* Noryl_NF1520 compound is a 20% glass reinforced, 15% PTFE. Wear resistant; 211F HDT @ 264 psi. |
|||
UL RTI, Mechanical with Impact | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics Prevex VFAX PPE+PS High impact strength. 180F (82C) HDT. Improved productivity/reliability.This data was supplied by SABIC-IP for the Americas region. |
|||
UL RTI, Mechanical with Impact | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics LNP STAT-KON Noryl_HMC1010 PPE+PS LNP* Stat-kon* Noryl_HMC1010 compound is a 10% Carbon fiber reinforced. Static dissipative. Nonbrominated, nonchlor- nated flame retardant system. UL94 V-1 rated. |
|||
UL RTI, Mechanical with Impact | 50.0 °C @Thickness 1.50 mm |
122 °F @Thickness 0.0591 in |
UL 746 |
Teknor Apex APEX® 6500-90 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
UL RTI, Mechanical with Impact | 50.0 °C @Thickness 1.50 mm |
122 °F @Thickness 0.0591 in |
UL 746 |
Teknor Apex APEX® 7500-80 Polyvinyl Chloride, Flexible Notes: 105°C General Purpose; RoHS Compliant Features: High Heat Resistance Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL.. |
|||
UL RTI, Mechanical with Impact | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics NORYL GTX GTX810 PPE+PS+PA 10% Glass Reinforced PPE+PA Alloy. |
|||
UL RTI, Mechanical with Impact | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics NORYL GTX GTX910 PPE+PS+PA Unfilled grade for automotive on-line painted components. Dimensional stability. Excellent chemical resistance. Class A surface appearance. |
|||
UL RTI, Mechanical with Impact | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics LNP THERMOCOMP Noryl_HM3020 PPE+HIPS (Europe-Africa-Middle East) LNP* Thermocomp* Noryl_HM3020 compound is a 30% Glass/Mineral filled, high modulus grade. DTUL 248F (120C). UL94 V-1/5VA rated in black and gray. |
|||
UL RTI, Mechanical with Impact | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics LNP THERMOCOMP Noryl_HM3020 PPE+PS LNP* Thermocomp* Noryl_HM3020 compound is a 30% Glass/Mineral filled, high modulus grade. DTUL 248F (120C). UL94 V-1/5VA rated in black and gray. |
|||
UL RTI, Mechanical with Impact | 50.0 °C @Thickness 1.50 mm |
122 °F @Thickness 0.0591 in |
UL 746 |
Teknor Apex APEX® 6500-85 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
UL RTI, Mechanical with Impact | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics NORYL ENV105 PPE+HIPS (Europe-Africa-Middle East) NORYL ENV105 is an impact modified extrusion grade with a Vicat B/120 of 115C according ISO 306. |
|||
UL RTI, Mechanical with Impact | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics NORYL GTX GTX810 PPE+PS+PA (Asia Pacific) GR 10%. Increased stiffness of 200000 psi (3000 MPa) flexural modulus. Excellent chemical and high heat resistance. Application: lighting. |
|||
UL RTI, Mechanical with Impact | 50.0 °C @Thickness 1.50 mm |
122 °F @Thickness 0.0591 in |
UL 746 |
Teknor Apex APEX® 7500-85 Polyvinyl Chloride, Flexible Notes: 105°C General Purpose; RoHS Compliant Features: High Heat Resistance Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL Q.. |
|||
UL RTI, Mechanical with Impact | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics LNP STAT-KON Noryl_FMC1010 PPE+PS LNP* Stat-kon* Noryl_FMC1010 compound is a 10% carbon fiber, static dissipative, foamable resin Nonchlorinated, nonbrominated. UL94 V1 rated. Property values at 20% WR, 0.250"" wall. |
|||
UL RTI, Mechanical with Impact | 50.0 °C @Thickness 0.700 - 6.00 mm |
122 °F @Thickness 0.0276 - 0.236 in |
|
Kleerdex Kydex® 107 Acrylic/PVC Thermoplastic Sheet
(discontinued **) High performance sheet for NSFApplications: Ice makers, vending machines, beverage dispensers, and other equipment requiring NSF approval, as a replacement for stainless steel parts where cost, weig.. |
|||
UL RTI, Mechanical with Impact | 50.0 °C | 122 °F | UL 746B |
SABIC Innovative Plastics GELOY XP4025 ASA+PC Available in a wide range of colors and is recommended for unpainted exterior applications. |