Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical with Impact | 180 °C @Thickness 1.57 mm |
356 °F @Thickness 0.0618 in |
|
Solvay Specialty Polymers Veradel® A-100, A-200, A-300 Polyethersulfone
(discontinued **) For superior long-term performance at high temperatures in severe service environments. It offers especially good toughness, hydrolytic stability, chemical resistance, plus FDA and USDA compliance.N.. |
|||
UL RTI, Mechanical with Impact | 180 °C | 356 °F | UL 746B |
Victrex® PEEK 150G / 151G Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, depth filtered granules for injection moulding, easy flow, FDA food contact c.. |
|||
UL RTI, Mechanical with Impact | 180 °C | 356 °F | UL 746B |
Victrex® PEEK 450FC30 General Purpose Product Description: High performance thermoplastic material, 30% reinforced with carbon fibre / graphite / PTFE PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and ext.. |
|||
UL RTI, Mechanical with Impact | 180 °C | 356 °F | UL 746B |
Victrex® PEEK 450G General Purpose Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, standard flow, FDA food contac.. |
|||
UL RTI, Mechanical with Impact | 180 °C | 356 °F | UL 746B |
SABIC Innovative Plastics ULTEM 3452 PEI 45% Glass fiber and mineral filled, enhanced flow Polyetherimide (Tg 217C) with enhanced dimensional stability. ECO Conforming, UL94 V0 and 5VA listing in recognized colors. |
|||
UL RTI, Mechanical with Impact | 180 °C | 356 °F | UL 746B |
SABIC Innovative Plastics ULTEM 3452 PEI (Asia Pacific) 45% Glass fiber and mineral filled, enhanced flow Polyetherimide (Tg 217C) with enhanced dimensional stability. ECO Conforming, UL94 V0 and 5VA listing in recognized colors. |
|||
UL RTI, Mechanical with Impact | 180 °C | 356 °F | UL 746B |
Victrex® PEEK 150FC30 Easy Flow Product Description: High performance thermoplastic material, 30% reinforced with carbon fibre / graphite / PTFE PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding, easy .. |
|||
UL RTI, Mechanical with Impact | 180 °C | 356 °F | |
Victrex® PEEK 381G Medium Viscosity Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, depth filtered granules for specialty extrusion processes, standard flow, FD.. |
|||
UL RTI, Mechanical with Impact | 180 °C | 356 °F | UL 746B |
Victrex® PEEK 450G903 Black Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, FDA food contac.. |