Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Electrical | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics Lexan® FL920 PC (Asia Pacific) Various weight reductions at .250"" (6.35 mm) wall, 20% GR. Excellent flex mod, high tensile strength/heat resistance. V-0/5V at .250"" (6.35mm). |
|||
UL RTI, Electrical | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics Lexan® FL930 PC (Asia Pacific) Various weight reductions at 0.250"" (6.35 mm) wall, 30% GR. Superior flex strength/modulus, good tensile strength. V-0/5VA at 0.250"" (6.35 mm). |
|||
UL RTI, Electrical | 110 °C | 230 °F | UL746B |
Idemitsu Kosan Xarec® WA 212 SPS, 30% Glass Filled Crystalline Polymer, Glass Filled, Impact Modified. Used in Automotive and Industrial applications. |
|||
UL RTI, Electrical | 110 °C | 230 °F | UL746B |
Idemitsu Kosan Xarec® WA 212LG SPS, 30% Glass Filled |
|||
UL RTI, Electrical | 110 °C @Thickness 1.50 mm |
230 °F @Thickness 0.0591 in |
UL 746B |
Aardvark Polymers AARTEL® 2000 Rotational Molding Resin Aartel® 2000 POM is a premium homopolymer acetal for rotational molding applications. Aartel® 2000 offers high performance properties and is a high flow, fast cycling polymer.Information prov.. |
|||
UL RTI, Electrical | 110 °C | 230 °F | |
Ineos ABS TRIAX® 1120 ABS/Nylon Blend, Injection Grade, Dry as Molded Injection molding grade with good flow and stress corrosion cracking resistance, good chemical resistance (fuel, cleaning agents), high impact and notched impact strength, good acoustical damping be.. |
|||
UL RTI, Electrical | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics NORYL PX9406 PPE+PS (Asia Pacific) Nonbrominated, nonchlorinated, flame retarded. Improved productivity and reliability. 252F HDT. UL94 V-0 rated. Electrical applications. |
|||
UL RTI, Electrical | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics NORYL PX9406P PPE NORYL* PX9406P resin is an FR (non-halogenated) grade potentially suitable for a variety of electronics applications. RTI (impact) = 105 C. F1 listed in BK color. |
|||
UL RTI, Electrical | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics NORYL SE1GFN1 PPE+HIPS (Europe-Africa-Middle East) Noryl* SE1GFN1 is a 10% glass reinforced, injection moldable modified polyphenylene ether resin. Designed for improved dimensional stability and good flow , this resin also uses non-chlorinated, non.. |
|||
UL RTI, Electrical | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics NORYL SE1GFN1 PPE+PS (Asia Pacific) 10% GR. UL94 V-1 rated. Halogen free flame retardant. Typical applications are TV chassis, deflection yokes and connectors. |
|||
UL RTI, Electrical | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics NORYL SE1GFN2 PPE+HIPS (Europe-Africa-Middle East) Noryl* SE1GFN2 is a 20% glass reinforced, injection moldable modified polyphenylene ether resin. Designed for improved dimensional stability and good flow , this resin also uses non-chlorinated, non.. |
|||
UL RTI, Electrical | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics NORYL SE1GFN3 PPE+HIPS (Europe-Africa-Middle East) Noryl* SE1GFN3 is a 30% glass reinforced, injection moldable modified polyphenylene ether resin. Designed for improved dimensional stability and good flow , this resin also uses non-chlorinated, non.. |
|||
UL RTI, Electrical | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics NORYL SE1X PPE+PS (Asia Pacific) PPO+PS. Improved productivity and reliability. Nonchlorinated, nonbrominated flame retardant. 244F HDT. |
|||
UL RTI, Electrical | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics NORYL V0150B PPE+HIPS Noryl* V0150B is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm a.. |
|||
UL RTI, Electrical | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics NORYL V0150B PPE+HIPS (Europe-Africa-Middle East) Noryl* V0150B is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm a.. |
|||
UL RTI, Electrical | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics Noryl V0150BT PPE+HIPS (Asia Pacific) Noryl* V0150BT is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm .. |
|||
UL RTI, Electrical | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics Noryl V0150BT PPE+HIPS (Europe-Africa-Middle East) Noryl* V0150BT is an unfilled, injection moldable modified polyphenylene ether resin.. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 1.5 mm .. |
|||
UL RTI, Electrical | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics Valox® 865 PBT+PET 30% GR PBTP, UL94 V-0 rated. Non-blooming flame retardant. Improved surface appearance. Same application areas as for VALOX 855. |
|||
UL RTI, Electrical | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics Valox® 865 PBT+PET (Asia Pacific) 30% GR PBTP, UL94 V-0 rated. Non-blooming flame retardant. Improved surface appearance. Same application areas as for VALOX 855. |
|||
UL RTI, Electrical | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics NORYL NH5020 PPE+PS Noryl* NH5020 Resin is an unreinforced blend of Polyphenylene Ether(PPE) + Polystyrenre resin. The material offers a good balance of heat, flow, hydrolytic stability, and non-halogenated flame reta.. |
|||
UL RTI, Electrical | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics NORYL NH5020 PPE+PS (Asia Pacific) Noryl* NH5020 Resin is an unreinforced blend of Polyphenylene Ether(PPE) + Polystyrenre resin. The material offers a good balance of heat, flow, hydrolytic stability, and non-halogenated flame reta.. |
|||
UL RTI, Electrical | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics NORYL NH5120 PPE+PS Noryl* NH5120 Resin is an unreinforced blend of Polyphenylene Ether(PPE) + Polystyrenre resin. The material offers a good balance of heat, flow, hydrolytic stability, and non-halogenated V1 flame re.. |
|||
UL RTI, Electrical | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics NORYL NH6020 PPE+HIPS Noryl NH6020 resin is an unfilled, injection moldable modified polyphenylene ether resin. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 0.8 .. |
|||
UL RTI, Electrical | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics NORYL NH6020 PPE+HIPS (Europe-Africa-Middle East) Noryl* NH6020 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 0.8 mm an.. |
|||
UL RTI, Electrical | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics NORYL NH7114 PPE+HIPS Noryl* NH7114 resin is a 20% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve UL94 flame ratings while offering an exceptional balance of streng.. |
|||
UL RTI, Electrical | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics NORYL NH7114 PPE+HIPS (Europe-Africa-Middle East) Noryl* NH7114 resin is a 20% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve UL94 flame ratings while offering an exceptional balance of streng.. |
|||
UL RTI, Electrical | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics NORYL NH8006 PPE+HIPS (Europe-Africa-Middle East) Noryl* NH8006 resin is a 30% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve a UL94 V0 flame rating (color specific) while offering an exceptio.. |
|||
UL RTI, Electrical | 110 °C | 230 °F | UL 746B |
SABIC Innovative Plastics NORYL N1250 PPE+HIPS (Asia Pacific) Noryl* N1250 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and good flow , this resin also uses non-chlorinated, non-brominated FR ad.. |
|||
UL RTI, Electrical | 110 °C | 230 °F | |
Aclo Accuguard Polypropylene HP1369V2CSL Homopolymer Flame Retardant Copper Stabilized |