Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Electrical | 65.0 °C | 149 °F | UL 746B |
SABIC Innovative Plastics Cycolac® GPM5500S ABS (Europe-Africa-Middle East) CYCOLAC GPM5500S is a multi purpose injection moulding grade, equal to GPM5500 but equiped with anti static agents, providing a favourable balance of engineering properties. CYCOLAC GPM5500S has a w.. |
|||
UL RTI, Electrical | 65.0 °C | 149 °F | UL 746B |
SABIC Innovative Plastics Cycolac® GPM5500U ABS (Europe-Africa-Middle East) CYCOLAC GPM5500U is a UV stabilized multi purpose injection moulding grade, providing a favourable balance of engineering properties. CYCOLAC GPM5500U has a wide processing window. It is recommended.. |
|||
UL RTI, Electrical | 65.0 - 140 °C | 149 - 284 °F | Average value: 108 °C Grade Count:11 |
Overview of materials for Nylon 6, 30% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are includ.. |
|||
UL RTI, Electrical | 65.0 °C @Thickness >=0.750 mm |
149 °F @Thickness >=0.0295 in |
|
LG Chemical LUMID GP2500A(W) PA6+GF50%, General Purpose Feature: Injection Molding, PA6+GF50%, General PurposeApplication: Automotive (Gear Shift Housing)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
UL RTI, Electrical | 65.0 °C @Thickness >=1.50 mm |
149 °F @Thickness >=0.0591 in |
|
LG Chemical LUPOL LW4302 PP+GF/MF30% Description: Injection Molding, PP+GF/MF30%, Low WarpageApplication: Electrical, Electronic and Automotive Parts CAS: 9003-07-0, 14807-96-6 and 165997-17-3Information provided by LG Chemical |
|||
UL RTI, Electrical | 65.0 °C | 149 °F | UL 746B |
SABIC Innovative Plastics NORYL RN0401 PPE+PS (Asia Pacific) RN0401 is an unfilled Post Consumer Recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 20% PCR styrenic series resin content. Available in black only. |
|||
UL RTI, Electrical | 65.0 °C | 149 °F | UL 746B |
SABIC Innovative Plastics NORYL RN0401 PPE+PS (Europe-Africa-Middle East) Noryl RN0401 resin is an unfilled Post Consumer Recycle (PCR) based injection moldable modified polyphenylene ether blend comprising at least 20% PCR content. Available in black only. |
|||
UL RTI, Electrical | 65.0 °C | 149 °F | UL 746B |
SABIC Innovative Plastics NORYL V090 PPE+HIPS (Europe-Africa-Middle East) NORYL V090 is an unfilled, flame retardant material with a Vicat B/120 of 95 °C according ISO 306. NORYL V090 is V0 at 2.0 mm and V1 at 1.6 mm according UL94 and halogen free according VDE/DIN 47.. |
|||
UL RTI, Electrical | 65.0 °C | 149 °F | UL 746B |
SABIC Innovative Plastics NORYL V095 PPE+PS (Europe-Africa-Middle East) Noryl* V095 resin is a modified PPE-PS blend that exhibits an excellent balance of non chlorinate, non brominate flame retardance, medium heat/high flow and low specific gravity for light weight par.. |
|||
UL RTI, Electrical | 65.0 °C | 149 °F | UL 746B |
SABIC Innovative Plastics LNP Thermocomp RF006XXP PA 66 (Europe-Africa-Middle East) 30% glass fibre reinforced Polyamide 66 injection moulding resin.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
UL RTI, Electrical | 65.0 °C | 149 °F | UL 746B |
SABIC Innovative Plastics NORYL GFN1720 PPE+HIPS (Europe-Africa-Middle East) Noryl* GFN1720 is a 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Noryl .. |
|||
UL RTI, Electrical | 65.0 °C | 149 °F | UL 746B |
SABIC Innovative Plastics NORYL NH5110E PPE+PS (Europe-Africa-Middle East) NORYL NH5110E is a flame retardant, non halogenated, impact modified extrusion grade. Developed for low beard-growth, with a Vicat B/120 of 138 Deg C, according to ISO 306 and a UL-94 rating of V1@ .. |
|||
UL RTI, Electrical | 65.0 °C | 149 °F | UL 746B |
SABIC Innovative Plastics NORYL ENV131 PPE+HIPS (Europe-Africa-Middle East) Noryl* ENV131 is an unfilled modified polyphenylene ether resin developed for extrusion process. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V1 rating .. |
|||
UL RTI, Electrical | 65.0 °C | 149 °F | UL 746B |
SABIC Innovative Plastics NORYL FP6130 PPE+PS (Asia Pacific) Noryl* FP6130 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR a.. |
|||
UL RTI, Electrical | 65.0 °C | 149 °F | UL 746B |
SABIC Innovative Plastics NORYL GFN1720 PPE+HIPS (Asia Pacific) Noryl* GFN1720 is a 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Noryl .. |
|||
UL RTI, Electrical | 65.0 °C @Thickness 0.780 mm |
149 °F @Thickness 0.0307 in |
UL 746 |
A. Schulman POLYFLAM™ FPP 1006 Talc Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1006 is a 20% talc filled homopolymer polypropylene compound.Information provided by A. Schulman. |
|||
UL RTI, Electrical | 65.0 °C @Thickness 0.780 mm |
149 °F @Thickness 0.0307 in |
UL 746 |
A. Schulman POLYFLAM™ FPP 1006 Talc Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1006 is a 20% talc filled homopolymer polypropylene compound.Information provided by A. Schulman. |
|||
UL RTI, Electrical | 65.0 °C | 149 °F | |
Eurostar Staramide BG7HU PA6, 35% Glass Fiber Filled, Heat and UV Stabilized, Injection Molded Staramide BG7H is a Heat and UV Stabilized, 35% Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
UL RTI, Electrical | 65.0 °C | 149 °F | |
Eurostar Staramide RF006SXP PA66, 30% Glass Fiber Filled, Injection Molded Staramide RF006SXP is a 30% Glass Fiber Reinforced Polyamide 66 Injection Molding Resin (also known as RF1006HS)Information provided by Eurostar. |
|||
UL RTI, Electrical | 65.0 °C | 149 °F | |
Eurostar Starflam AFR200B PA66, Flame Retardant, Injection Molding Staramide AFR200B is an Unfilled, Flame Retardant Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
UL RTI, Electrical | 65.0 °C | 149 °F | |
Eurostar Starflam AFR682A1 PA66, Mineral Reinforced, Flame Retardant, Injection Molding Starflam AFR682A1 is a Flame Retardant, Mineral Filled Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
UL RTI, Electrical | 65.0 °C | 149 °F | |
Eurostar Starflam BFR460A PA6, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam BFR460A is a Flame Retardant, Glass Fiber Reinforced Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
UL RTI, Electrical | 65.0 °C | 149 °F | |
Eurostar Staramide R1000HI620 PA66, Impact Modified, Injection Molded Staramide R1000HI620 is an Impact Modified Polyamide 66 Injection Molding Resin (also known as R1000HI010)Information provided by Eurostar. |
|||
UL RTI, Electrical | 65.0 °C | 149 °F | |
Arkema Group Rilsan® BZM 8 NOIR TL Nylon 11, 8% Glass Fiber Filled (Conditioned) Designation ISO 1874-PA11,MHL,18-020,GF8Rigid grade with glass fiber (8%) filler for injection molding. Available color: black. Light and heat stabilized.Rigidity. Outstanding compromise between goo.. |
|||
UL RTI, Electrical | 65.0 °C @Thickness 1.50 mm |
149 °F @Thickness 0.0591 in |
746B |
BASF Ultramid® A3HG6 HR BK 23591 30% Glass Filled PA66 (Dry) Description: 30% glass-fiber reinforced injection-molding grade with enhanced hydrolysis resistance, e.g., for applications in vehicle cooling systems.Information provided by BASF |
|||
UL RTI, Electrical | 65.0 - 130 °C | 149 - 266 °F | Average value: 122 °C Grade Count:3 |
Overview of materials for Nylon 66, Nucleated This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Nucleated". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
UL RTI, Electrical | 65.0 °C @Thickness 1.50 mm |
149 °F @Thickness 0.0591 in |
746B |
BASF Ultramid® BU50I PA6 (Dry) Description: Ultramid Ultratough Nylon BU50I is an unreinforced PA6, impact modified injection molding product that maintains its impact strength and ductility to -40 deg F (-40 deg C). The extreme .. |
|||
UL RTI, Electrical | 65.0 °C | 149 °F | UL 746B |
SABIC Innovative Plastics Noryl FXN2090H PPE+HIPS (Asia Pacific) Noryl* FXN2090H resin is an unfilled, injection moldable grade. Designed for exceptionally high gloss and improved pencil hardness vs. standard Noryl grades, FXN2090H resin uses non-halogenated FR a.. |
|||
UL RTI, Electrical | 65.0 °C | 149 °F | UL 746B |
SABIC Innovative Plastics NORYL PX2060 PPE+PS (Asia Pacific) Noryl* PX2060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR .. |
|||
UL RTI, Electrical | 65.0 °C | 149 °F | UL 746B |
SABIC Innovative Plastics NORYL RN0612 PPE+HIPS (Europe-Africa-Middle East) Noryl RN0612 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 30% PCR styrenic series resin content. Designed for good dimen.. |