Thermal Properties Metric English Comments
UL RTI, Electrical 50.0 - 85.0 °C
122 - 185 °F
Average value: 62.0 °C Grade Count:20
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded". Each property range of values reported i..