Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Electrical | 130 - 155 °C | 266 - 311 °F | Average value: 145 °C Grade Count:9 |
Overview of materials for Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant". Each property range of values re.. |