Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Electrical | 95.0 °C @Thickness >=1.50 mm |
203 °F @Thickness >=0.0591 in |
|
LG Chemical LUPOY GN5007FL PC/ABS, Halogen Free Flame Retardant, Heat Resistance Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, Heat Resistance, High FlowApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2, 9003-56-9 and 181028.. |
|||
UL RTI, Electrical | 95.0 °C | 203 °F | UL 746B |
SABIC Innovative Plastics NORYL SE0 PPE+HIPS (Europe-Africa-Middle East) NORYL SE0 is an unfilled, flame retardant material with a Vicat B/120 of 130C according ISO 306. NORYL SE0 is V0 at 1.6 mm according UL94 and halogen free according VDE/DIN 472 part 815. |
|||
UL RTI, Electrical | 95.0 °C | 203 °F | UL 746B |
SABIC Innovative Plastics NORYL SE100 PPE+HIPS (Europe-Africa-Middle East) NORYL® SE100 is an unfilled, flame retardant material with a Vicat B/120 of 120°C. It has a UL-94 flammability rating V1 @ 1.47 mm, and is halogen free according to VDE/DIN 472 part 815. |
|||
UL RTI, Electrical | 95.0 °C | 203 °F | UL 746B |
SABIC Innovative Plastics NORYL SE100HX PPE+PS Improved productivity and reliability. Nonchlorinated, nonbrominated FR. |
|||
UL RTI, Electrical | 95.0 °C | 203 °F | UL 746B |
SABIC Innovative Plastics NORYL SE100X PPE+PS PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0/V1 rated. RTI Elec/Imp/Str 95/80/95. Good flow. Suitable for E/E market indoor/outdoor applications. |
|||
UL RTI, Electrical | 95.0 °C | 203 °F | UL 746B |
SABIC Innovative Plastics NORYL SE100X PPE+PS (Asia Pacific) Nonbrominated, nonchlorinated FR resin. Improved productivity and reliability. 199F HDT. |
|||
UL RTI, Electrical | 95.0 °C | 203 °F | UL 746B |
SABIC Innovative Plastics NORYL SE90 PPE+HIPS (Europe-Africa-Middle East) NORYL SE90 is an unfilled, flame retardant material with a Vicat B/120 of 110°C according ISO 306. NORYL SE90 is V1 at 1.6 mm according UL94 and halogen free according VDE/DIN 472 part 815. |
|||
UL RTI, Electrical | 95.0 °C | 203 °F | UL 746B |
SABIC Innovative Plastics Prevex BJAX PPE+PS Foamable resin. All properties at 10% density reduction; 0.250" thick specimens; improved productivity.This data was supplied by SABIC-IP for the Americas region. |
|||
UL RTI, Electrical | 95.0 °C | 203 °F | UL 746B |
SABIC Innovative Plastics PREVEX VGAX PPE+PS Improved productivity and reliability. Nonchlorinated, nonbrominated flame retardant. 180F HDT. |
|||
UL RTI, Electrical | 95.0 °C | 203 °F | |
Samsung Cheil Industries Infino® GC-1015 PC/ABS, FR Information provided by Samsung Cheil Industries. |
|||
UL RTI, Electrical | 95.0 °C | 203 °F | |
Samsung Cheil Industries Infino® GC-1015 PC/ABS, FR Information provided by Samsung Cheil Industries. |
|||
UL RTI, Electrical | 95.0 °C | 203 °F | UL 746B |
SABIC Innovative Plastics NORYL N190 PPE+HIPS (Europe-Africa-Middle East) NORYL N190 is an unfilled, flame retardant material with a Vicat B/120 of 105°C according ISO 306. NORYL N190 is V0 at 1.52 mm and 5VA at 3.12 mm according UL94 and halogen free according VDE/DIN.. |
|||
UL RTI, Electrical | 95.0 °C | 203 °F | UL 746B |
SABIC Innovative Plastics Noryl N190HX PPE+PS High gloss. 182F (83C) HDT. UL94 V-0/5VA rated.This data was supplied by SABIC-IP for the Americas region. |
|||
UL RTI, Electrical | 95.0 °C | 203 °F | UL 746B |
SABIC Innovative Plastics NORYL N190X PPE+PS PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0/5VA rated. RTI Elec/Imp/Str 95/80/95. Dielectric strength. Suitable for E/E market applications. |
|||
UL RTI, Electrical | 95.0 °C | 203 °F | UL 746B |
SABIC Innovative Plastics NORYL N225X PPE+PS PPE+PS blend. Unfilled. Halogen-Free FR performance. UL94 V0/5VA. UL746C F1. Dielectric Strength. Suitable for E/E market indoor/outdoor applications. |
|||
UL RTI, Electrical | 95.0 °C | 203 °F | UL 746B |
SABIC Innovative Plastics NORYL PX1007 PPE+PS Noryl* PX1007 is an unfilled non-chlorinated, non-brominated flame retardant PPE/HIPS grade. |
|||
UL RTI, Electrical | 95.0 °C | 203 °F | UL 746B |
SABIC Innovative Plastics NORYL BN31 PPE+PS Blowmoldable. Excellent processability and flammability. Good heat resistance. Low temperature impact strength. Dimensional stability. |
|||
UL RTI, Electrical | 95.0 °C | 203 °F | UL 746B |
SABIC Innovative Plastics NORYL PX1007 PPE+HIPS (Europe-Africa-Middle East) NORYL* PX1007 is an unfilled non-chlorinated, non-brominated flame retardant PPE/HIPS grade, targeted for flat panel TV enclosures. It has a Vicat B/120 temperature of 96 degC and UL-94 V0 @ 1.5mm .. |
|||
UL RTI, Electrical | 95.0 °C | 203 °F | |
Covestro Bayblend® FR 110 Polycarbonate/ABS Blend Flame retardant grade with antimony, chlorine and bromine free, flame retardant package, good light stability.Applications: Housings for business machines.Information provided by Bayer.As of 1 Septe.. |
|||
UL RTI, Electrical | 95.0 °C | 203 °F | UL-746B |
Axiall SP-6655 Rigid PVC, Molding Georgia Gulf SP-6655 is a high flow rigid PVC compound designed for electrical and custom molding applications. This compound features excellent physical properties, good melt flow, and exceptional.. |
|||
UL RTI, Electrical | 95.0 °C | 203 °F | UL-746B |
Axiall Suprel® SVA 9412 Rigid PVC, Molding Georgia Gulf Suprel® SVA 9412 injection molding alloy features excellent impact resistance, excellent processing characteristics and comprehensive UL listings. The UL listings of Suprel 9412 inclu.. |
|||
UL RTI, Electrical | 95.0 °C | 203 °F | UL-746B |
Axiall 2651 Rigid PVC, Molding Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
UL RTI, Electrical | 95.0 °C | 203 °F | UL 746B |
SABIC Innovative Plastics NORYL PX1005X PPE+PS PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0/5VA rated. UL746C F1. Excelent dielectric strength. Suitable for E/E market in indoor/outdoor applications. |
|||
UL RTI, Electrical | 95.0 °C | 203 °F | |
Covestro Bayblend® FR 2010 Polycarbonate/ABS Blend
(discontinued **) Easy-flowing FR grade. Flame retardant grade with antimony, chlorine and bromine free, flame retardant package, optimized processability.Applications: Housings for office equipment, electrical engin.. |
|||
UL RTI, Electrical | 95.0 °C | 203 °F | UL-746B |
Axiall SP-6235 Rigid PVC, Molding Georgia Gulf SP-6235 is a high flow rigid PVC compound designed for electrical and custom molding applications. This compound features excellent physical properties, high melt flow and exceptionall.. |
|||
UL RTI, Electrical | 95.0 °C | 203 °F | UL 746B |
SABIC Innovative Plastics Noryl EN212 PPE+PS Extrusion grade. 212F (100C) DTUL. UL94 V-1 rated.This data was supplied by SABIC-IP for the Americas region. |