Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Electrical | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics Cycolac® EXABS01 ABS Sheet extrusion ABS with medium impact. |
|||
UL RTI, Electrical | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics Cycolac® FR15U ABS (Asia Pacific) Flame retardant ABS. Excellent indoor UV properties. Excellent moldability. UL94 V-0/5VA rated.ing. |
|||
UL RTI, Electrical | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics Cycolac® FR23 ABS Flame retardant ABS (non-PBBE additives). Good properties/toughness. Excellent moldability. UL94 V-0 rated. |
|||
UL RTI, Electrical | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics Cycolac® MG29 ABS Super high impact ABS. Good low temperature toughness. High gloss. |
|||
UL RTI, Electrical | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics Cycolac® S703T ABS (Europe-Africa-Middle East) CYCOLAC S703T is a super high flow ABS developed for thin wall injection/compression moulding applications.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
UL RTI, Electrical | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® C2800 PC+ABS (Europe-Africa-Middle East) Non-chlorinated and non-brominated flame retardant PC+ABS offering balanced flow and impact properties for various applications. |
|||
UL RTI, Electrical | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® C3650 PC+ABS Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering high impact and excellent extrusion and thermoforming characteristics. Halogen free according .. |
|||
UL RTI, Electrical | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® C3650 PC+ABS (Asia Pacific) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering high impact and excellent extrusion and thermoforming characteristics. Halogen free according .. |
|||
UL RTI, Electrical | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® C4210HF PC+ABS (Europe-Africa-Middle East) CYCOLOY C4210HF is a 10% glass reinforced, non-FR PC+ABS grade with high heat resistance, excellent strength and rigidity with good cosmetic appearance. It combines a good processabity with a low sh.. |
|||
UL RTI, Electrical | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® CM6210 PC+ABS (Europe-Africa-Middle East) Cycoloy* resin CM6210 is a high-modulus flame retardant PC/ABS with non-brominated and non-chlorinated FR system. It can be used for extrusion & thermoforming applications and also for injection mol.. |
|||
UL RTI, Electrical | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® CU1650 PC+ABS (Europe-Africa-Middle East) UV stabilized, non-FR PC/ABS of excellent flow and impact performanceThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
UL RTI, Electrical | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® FXC630ME PC+ABS Color package may affect performance. PC+ABS, ECO-conforming flame retardant with metallic or pearlescent appearance. |
|||
UL RTI, Electrical | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® FXC630ME PC+ABS (Asia Pacific) PC+ABS, ECO-conforming flame retardant with metallic or pearlescent appearance. |
|||
UL RTI, Electrical | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® FXC630ME PC+ABS (Europe-Africa-Middle East) PC+ABS, of non-chlorinated & non brominated flame retardant with metallic or pearlescent appearance. MAGIX color package may affect performance.This data was supplied by SABIC-IP for the Europe-Afri.. |
|||
UL RTI, Electrical | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® FXC630SK PC+ABS (Asia Pacific) PC+ABS, ECO-conforming flame retardant with diamond sparkle appearance. |
|||
UL RTI, Electrical | 60.0 °C | 140 °F | |
PTS PCA-2008 Flame Retardant PC/ABS Alloy Information provided by Polymer Technology and Services, LLC (PTS). |
|||
UL RTI, Electrical | 60.0 °C | 140 °F | |
PTS PCA-2201NHV Non Bromine, Non Chlorine Flame Retardant Polycarbonate/ABS Alloy, UV Stabilized Information provided by Polymer Technology and Services, LLC (PTS). |
|||
UL RTI, Electrical | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® C1110 PC+ABS (Asia Pacific) High impact and ductility at 73F (23C) and -20F (-29C). |
|||
UL RTI, Electrical | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® C2805 PC+ABS LNP* Lubricomp* Cycoloy* C2805 compound is a PTFE reinforced PC+ABS, wear resistant, flame retardant compound for moving components in business equipment. Medium heat performance |
|||
UL RTI, Electrical | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® C6840 PC+ABS (Europe-Africa-Middle East) Cycoloy* C6840 resin is an injection moldable, flame retardant PC/ABS blend. It contains non-chlorinated & non-brominated flame retardant systems intended to meet governmental regulations and variou.. |
|||
UL RTI, Electrical | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® CU1650 PC+ABS UV stabilized, non-FR PC/ABS of excellent flow and impact performance |
|||
UL RTI, Electrical | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics LNP LUBRICOMP Cycoloy_C2801 PC+ABS (Europe-Africa-Middle East) LNP* Lubricomp* Cycoloy_C2801 compound is a 5% PTFE reinforced PC+ABS wear resistant flame retardant resin for moving components in business equipment. Medium heat performance |
|||
UL RTI, Electrical | 60.0 - 65.0 °C | 140 - 149 °F | Average value: 62.5 °C Grade Count:8 |
Overview of materials for Nylon 6, 20% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are includ.. |
|||
UL RTI, Electrical | 60.0 °C @Thickness 1.50 mm |
140 °F @Thickness 0.0591 in |
UL746B |
Ineos ABS Lustran® LK197 ABS, Extrusion Grade Lustran® ABS LK197 resin is a high-gloss, medium-impact extrusion grade of ABS (Acrylonitrile Butadiene Styrene). It provides a superior balance between rigidity and impact strength, as well as e.. |
|||
UL RTI, Electrical | 60.0 °C @Thickness >=1.70 mm |
140 °F @Thickness >=0.0669 in |
|
LG Chemical LUPOY GP5056F PC/ABS+GF5%, Flame Retardance Description: Injection Molding, PC/ABS+GF5%, Flame Retardance, General PurposeApplication: IT/OA (Housing)CAS: 103598-77-2, 9003-56-9, 68928-70-1, 1309-64-4 and 65997-17-3Information provided by LG .. |
|||
UL RTI, Electrical | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics LNP THERMOCOMP Cycoloy_C7210A PC+ABS LNP* Thermocomp* Cycoloy_C7210A isa a talc-filled PC+ABS, nonhalogenated FR for thinwall molding applications. Very good modulus-ductility balance. |
|||
UL RTI, Electrical | 60.0 °C @Thickness 1.50 mm |
140 °F @Thickness 0.0591 in |
|
Covestro Bayblend® T 84 Polycarbonate/ABS Blend Easier flowing than BAYBLEND T 85 MN.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |
|||
UL RTI, Electrical | 60.0 °C | 140 °F | |
Covestro Bayblend® T 65 Polycarbonate/ABS Blend High impact and notched impact strength, little risk of brittle fracture, high dimensional accuracy.Applications: Interior automotive components.Information provided by Bayer.As of 1 September 2015,.. |
|||
UL RTI, Electrical | 60.0 °C | 140 °F | UL 746B |
SABIC Innovative Plastics Cycolac® EX39 ABS Highest impact extrusion ABS for sheet and blow molding applications. |
|||
UL RTI, Electrical | 60.0 °C | 140 °F | UL 746B |
LG Chemical XR404T ABS, Heat Resistance Feature: Injection Molding, Heat Resistance, Curl FitApplication: Automotives Interior Housing (P/W Switch Housing Etc)CAS No. 25120-20-1, 9003-56-9, and 9001-96-2Information provided by LG Chemical.. |