Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Electrical | 115 °C | 239 °F | UL 746B |
SABIC Innovative Plastics Lexan® LUX9130T PC COPOLYMER (Asia Pacific) LUX9130T Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm / 5VA rating at 6.0mm and is U.. |
|||
UL RTI, Electrical | 115 °C | 239 °F | UL 746B |
SABIC Innovative Plastics Lexan® 303 PC (Asia Pacific) Clear, high viscosity material designed to service severe environments of HID lighting.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
UL RTI, Electrical | 115 °C | 239 °F | UL 746B |
SABIC Innovative Plastics Lexan® ML3019 PC (Europe-Africa-Middle East) LEXAN ML3019 is a medium viscosity, 10% glass reinforced, flame retardant grade, especially designed for applications like industrial enclosures and fuse boxes requiring a low knock-out strength for.. |
|||
UL RTI, Electrical | 115 °C | 239 °F | |
Industrial Laminates/Norplex MC223 Cotton Fabric Description: Grade MC223 is a medium weave cotton phenolic composite that is specifically formulated to meet MIL-P-18324.Typical applications include pintle and stave-type bearings for rudder shafts.. |
|||
UL RTI, Electrical | 115 °C | 239 °F | |
Industrial Laminates/Norplex MC320LE Cotton Fabric Description: Grade MC320LE is a fine weave bleached cotton phenolic composite that has excellent machining characteristics and low moisture absorption. Applications include marine applications, term.. |
|||
UL RTI, Electrical | 115 °C | 239 °F | 0.118 in; UL 746 |
LyondellBasell Hifaxâ„¢ AA36H Polypropylene Homopolymer Description: Hifaxâ„¢ AA36H conventional melt flow, 1,400 MPa flexural modulus, UL 94 V-2 flame retardant polypropylene homopolymer resin has an excellent combination of properties and processabi.. |
|||
UL RTI, Electrical | 115 °C | 239 °F | 0.118 in; UL 746 |
LyondellBasell Hifaxâ„¢ AA56H Polypropylene Homopolymer Description: Hifaxâ„¢ AA56H medium high melt flow, 1,400 MPa flexural modulus, UL 94 V-2 flame retardant polypropylene homopolymer resin has an excellent combination of properties and processabil.. |
|||
UL RTI, Electrical | 115 °C | 239 °F | UL 746B |
SABIC Innovative Plastics ULTEM ATX100 PEI+PCE Higher impact, high flow Polyetherimide blend. ECO Conforming, UL94 HB Listing. |
|||
UL RTI, Electrical | 115 °C | 239 °F | UL 746B |
SABIC Innovative Plastics ULTEM ATX100 PEI+PCE (Asia Pacific) Higher impact, high flow Polyetherimide blend. ECO Conforming, UL94 HB Listing. |
|||
UL RTI, Electrical | 115 °C | 239 °F | UL 746B |
SABIC Innovative Plastics Ultem ATX100F PEI+PCE Higher impact, high flow Polyetherimide blend. ECO Conforming, UL94 HB Listing. US FDA Food Contact Compliant.This data was supplied by SABIC-IP for the Americas region. |
|||
UL RTI, Electrical | 115 °C | 239 °F | UL 746B |
SABIC Innovative Plastics Ultem ATX100F PEI+PCE (Asia Pacific) Higher impact, high flow Polyetherimide blend. ECO Conforming, UL94 HB Listing. US FDA Food Contact Compliant.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
UL RTI, Electrical | 115 °C | 239 °F | UL 746B |
SABIC Innovative Plastics Ultem ATX100R PEI+PCE Higher impact, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 HB listing.This data was supplied by SABIC-IP for the Americas region. |
|||
UL RTI, Electrical | 115 °C | 239 °F | UL 746B |
SABIC Innovative Plastics Ultem ATX100R PEI+PCE (Asia Pacific) Higher impact, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 HB listing.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
UL RTI, Electrical | 115 °C | 239 °F | UL 746B |
SABIC Innovative Plastics ULTEM ATX200F PEI+PCE High flow Polyetherimide blend. ECO Conforming, UL94 V0 Listing. US FDA Food Contact compliant. |
|||
UL RTI, Electrical | 115 °C | 239 °F | UL 746B |
SABIC Innovative Plastics ULTEM ATX200F PEI+PCE (Asia Pacific) High flow Polyetherimide blend. ECO Conforming, UL94 V0 Listing. US FDA Food Contact compliant. |
|||
UL RTI, Electrical | 115 °C @Thickness 1.47 mm |
239 °F @Thickness 0.0579 in |
UL 746B |
Teijin Panlite® LS-2250 Friction and Abrasion Resistant Polycarbonate Resin It is compounded with fluorine powder to improve friction and abrasion resistance, meeting UL 94 V-2. The friction and abrasion resistance is superior than that of polyamidoacetal, maintaining excel.. |
|||
UL RTI, Electrical | 115 °C | 239 °F | UL 746B |
SABIC Innovative Plastics NORYL LTA1350 PPE+PS Noryl* LTA1350 is an unfilled, injection moldable grade. Designed for improved long term heat aging, this resin also uses non-chlorinated, non-brominated FR additives to achieve a V0 UL94 rating. No.. |
|||
UL RTI, Electrical | 115 °C | 239 °F | UL 746B |
SABIC Innovative Plastics ULTEM ATX200 PEI+PCE High flow Polyetherimide blend. ECO Conforming, UL94 V0 Listing. |
|||
UL RTI, Electrical | 115 °C | 239 °F | UL 746B |
SABIC Innovative Plastics ULTEM ATX200 PEI+PCE (Asia Pacific) High flow Polyetherimide blend. ECO Conforming, UL94 V0 Listing. |
|||
UL RTI, Electrical | 115 °C | 239 °F | 0.030 in; UL 94 |
A. Schulman POLYFLAM™ RPP 1221 Low-Blooming, General Purpose Copolymer Polypropylene DescriptionPolyflam® RPP 1221 is a low-blooming general purpose copolymer polypropylene flame retardant material with a UL-V2 flammability rating and 115°C temperature index at 0.030 in. Informati.. |
|||
UL RTI, Electrical | 115 °C | 239 °F | 0.030 in; UL 94 |
A. Schulman POLYFLAM™ RPP 1221 Low-Blooming, General Purpose Copolymer Polypropylene DescriptionPolyflam® RPP 1221 is a low-blooming general purpose copolymer polypropylene flame retardant material with a UL-V2 flammability rating and 115°C temperature index at 0.030 in. Informati.. |
|||
UL RTI, Electrical | 115 °C | 239 °F | 0.030 in; UL 94 |
A. Schulman POLYFLAM™ RPP 1221 Low-Blooming, General Purpose Copolymer Polypropylene DescriptionPolyflam® RPP 1221 is a low-blooming general purpose copolymer polypropylene flame retardant material with a UL-V2 flammability rating and 115°C temperature index at 0.030 in. Informati.. |
|||
UL RTI, Electrical | 115 °C | 239 °F | 0.030 in; UL 94 |
A. Schulman POLYFLAM™ RPP 1221 Low-Blooming, General Purpose Copolymer Polypropylene DescriptionPolyflam® RPP 1221 is a low-blooming general purpose copolymer polypropylene flame retardant material with a UL-V2 flammability rating and 115°C temperature index at 0.030 in. Informati.. |
|||
UL RTI, Electrical | 115 °C | 239 °F | 0.030 in; UL 94 |
A. Schulman POLYFLAM™ RPP 1221 Low-Blooming, General Purpose Copolymer Polypropylene DescriptionPolyflam® RPP 1221 is a low-blooming general purpose copolymer polypropylene flame retardant material with a UL-V2 flammability rating and 115°C temperature index at 0.030 in. Informati.. |
|||
UL RTI, Electrical | 115 °C | 239 °F | 0.030 in; UL 94 |
A. Schulman POLYFLAM™ RPP 1221 Low-Blooming, General Purpose Copolymer Polypropylene DescriptionPolyflam® RPP 1221 is a low-blooming general purpose copolymer polypropylene flame retardant material with a UL-V2 flammability rating and 115°C temperature index at 0.030 in. Informati.. |