| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 131 - 152 °C | 268 - 306 °F | Average value: 145 °C Grade Count:74 |
| Overview of materials for Polycarbonate, 20% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 20% Glass Filled". Specific grades with glass content between 15% and 24% are included. E.. |
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 138 - 152 °C | 280 - 305 °F | Average value: 142 °C Grade Count:7 |
| Overview of materials for Polycarbonate, Foam Grade, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Foam Grade, Glass Filled". Each property range of values reported is minimum and maximum .. |
|||
| Deflection Temperature at 0.46 MPa (66 psi) | 101 - 152 °C | 214 - 305 °F | Average value: 143 °C Grade Count:51 |
| Overview of materials for Polycarbonate, Carbon Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximum v.. |
|||