Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 127 - 250 °C | 260 - 482 °F | Average value: 167 °C Grade Count:12 |
Overview of materials for Polyphenylene Ether, 10% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 10% Glass Filled". Specific grades with glass content between 5% and 14% are includ.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 140 - 250 °C | 284 - 482 °F | Average value: 218 °C Grade Count:17 |
Overview of materials for Nylon 66, 20% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are inclu.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 220 - 250 °C | 428 - 482 °F | Average value: 238 °C Grade Count:21 |
Overview of materials for Polyethylene Terephthalate (PET), 20% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 20% Glass Reinforced". Specific grades with glass content between 15% .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 232 - 250 °C | 450 - 482 °F | Average value: 245 °C Grade Count:13 |
Overview of materials for Polyethylene Terephthalate (PET), 40% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 40% Glass Reinforced". Specific grades with glass content between 35% .. |