Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 204 - 224 °C | 400 - 435 °F | Average value: 212 °C Grade Count:15 |
Overview of materials for Polyetherimide (PEI), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, Carbon Fiber Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 207 - 224 °C | 405 - 435 °F | Average value: 220 °C Grade Count:32 |
Overview of materials for Nylon 610, Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610, Glass Reinforced". Each property range of values reported is minimum and maximum values of ap.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 210 - 224 °C | 410 - 435 °F | Average value: 217 °C Grade Count:10 |
Overview of materials for Polyethersulfone (PES), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 20% Glass Fiber Filled". Each property range of values reported is minimum and m.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 182 - 224 °C | 360 - 435 °F | Average value: 211 °C Grade Count:7 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled". Each property range of values reported is .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 182 - 224 °C | 360 - 435 °F | Average value: 202 °C Grade Count:7 |
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Carbon Fiber Filled". Each property range of values reported is minimu.. |