Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 149 - 183 °C | 300 - 361 °F | Average value: 165 °C Grade Count:33 |
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% ar.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 160 - 183 °C | 320 - 361 °F | Average value: 164 °C Grade Count:9 |
Overview of materials for Acetal Copolymer + Glass/PTFE This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer + Glass/PTFE". Each property range of values reported is minimum and maximum values of .. |