Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 150 - 160 °C | 302 - 320 °F | Average value: 156 °C Grade Count:8 |
Overview of materials for Acetal Copolymer, Steel Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Steel Filled". Each property range of values reported is minimum and maximum values of.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 128 - 160 °C | 262 - 320 °F | Average value: 136 °C Grade Count:13 |
Overview of materials for Polycarbonate, Gamma Radiation Resistant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Gamma Radiation Resistant". Each property range of values reported is minimum and maximum.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 130 - 160 °C | 266 - 320 °F | Average value: 140 °C Grade Count:6 |
Overview of materials for Nylon 12, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Flame Retardant". Each property range of values reported is minimum and maximum values of appr.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 95.0 - 160 °C | 203 - 320 °F | Average value: 138 °C Grade Count:17 |
Overview of materials for Acetal Copolymer, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Impact Modified". Each property range of values reported is minimum and maximum values.. |