Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 52.0 - 61.0 °C | 126 - 142 °F | ASTM D648 |
DSM Somos® 9120 Epoxy Photopolymer
(Unverified Data**) DescriptionDSM Somos® 9120 is a liquid photopolymer that produces robust, functional and accurate parts using stereolithography machines. The material offers superior chemical resistance, a wide p.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 52.0 - 61.0 °C | 126 - 142 °F | ASTM D648-07 |
DSM Somos® 9120 The need for movable parts is a constant when it comes to prototyping. Being able to ensure the proper fit for parts within a component can save both time and money. Somos® 9120 creates semi-transp.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 59.0 - 61.0 °C | 138 - 142 °F | Thermal Postcure; ASTM D648-98c |
DSM Somos® WaterClear® Ultra 10122 Optically Clear, Colorless, Rigid, Stereolithography Resin DescriptionDSM Somos® WaterClear Ultra 10122 is a next generation optically clear resin with ABS like properties and good temperature resistance. It produces colorless, functional, accurate parts .. |